摘要:
Provided is a ternary inorganic compound crystal having a molecular formula of Ca 8 Al 12 P 2 O 31 , and a preparation method thereof comprising the following steps: weighing calcium salts, aluminum salts and phosphate respectively according to the molar ratio of calcium, aluminum and phosphorus in the molecular formula Ca 8 Al 12 P 2 O 31 ; calcining at 1550∼1570°C, cooling, and grinding to obtain the ternary inorganic compound crystal. Also provided is an application of the ternary inorganic compound in gelling materials and molecular sieves, nonlinear optical crystals, and photochromic materials.
摘要翻译:本发明提供具有分子式为Ca 8 Al 12 P 2 O 31的三元无机化合物晶体及其制备方法,其包括以下步骤:按钙,铝和铝的摩尔比分别称量钙盐,铝盐和磷酸盐 分子式中的磷Ca 8 Al 12 P 2 O 31; 在1550¼1570℃下煅烧,冷却和研磨,得到三元无机化合物晶体。 还提供了三元无机化合物在胶凝材料和分子筛,非线性光学晶体和光致变色材料中的应用。
摘要:
Provided is a ternary inorganic compound crystal having a molecular formula of Ca 8 Al 12 P 2 O 31 , and a preparation method thereof comprising the following steps: weighing calcium salts, aluminum salts and phosphate respectively according to the molar ratio of calcium, aluminum and phosphorus in the molecular formula Ca 8 Al 12 P 2 O 31 ; calcining at 1550ˆ¼1570°C, cooling, and grinding to obtain the ternary inorganic compound crystal. Also provided is an application of the ternary inorganic compound in gelling materials and molecular sieves, nonlinear optical crystals, and photochromic materials.