公开(公告)号:EP2756883A1
公开(公告)日:2014-07-23
申请号:EP12832451.4
申请日:2012-09-11
申请人: Sinochem Lantian Co., Ltd. , Sinochem Modern Environmental Protection Chemicals (Xi'an) Co., Ltd.
发明人: YANG, Gang , XU, Lei , YANG, Huie , JIANG, En , FAN, Jianping , ZHAO, Xintang , ZENG, Changhua , ZHANG, Wenqing , LEI, Yunlong , LI, Zhong , CHEN, Shukang
IPC分类号: B01J27/132 , C07C21/18 , C07C17/35
CPC分类号: C07C17/206 , B01J23/002 , B01J23/26 , B01J27/132 , B01J37/0018 , B01J2523/00 , C07C21/18 , B01J2523/31 , B01J2523/3712 , B01J2523/67 , B01J2523/3706 , B01J2523/3718 , B01J2523/27 , B01J2523/22
摘要: Provided are a fluorination catalyst for preparing 2,3,3,3-tetrafluoropropene and a method using the catalyst for preparing 2,3,3,3-tetrafluoropropene. The catalyst has the following structural formula: Crx(Y,Z) 0.005-o.5 O 0.1-1.0 F 1.0-3.0 , where Y is one or a combination of two or more among Al, Zn, and Mg, and where Z is a rare earth element having an oxygen-storing/releasing function. The catalyst has in preparing 2,3,3,3-tetrafluoropropene the advantages of increased raw material conversion rate, great product selectivity, and extended catalyst service life.
摘要翻译: 提供用于制备2,3,3,3-四氟丙烯的氟化催化剂和使用该催化剂制备2,3,3,3-四氟丙烯的方法。 该催化剂具有以下结构式:其中Y是Al,Zn和Mg中的一种或两种以上的组合,Cr x(Y,Z)为0.005-0.5O 0.1 -1.0 F 1.0-3.0,并且其中 Z是具有储氧/释放功能的稀土元素。 该催化剂具有制备2,3,3,3-四氟丙烯原料转化率高,产物选择性好,催化剂使用寿命长的优点。