Copper-containing aluminium alloy and method of manufacturing products from said alloy
    3.
    发明公开
    Copper-containing aluminium alloy and method of manufacturing products from said alloy 失效
    含铜铝合金及从合金制造产品的方法

    公开(公告)号:EP0031605A3

    公开(公告)日:1981-07-22

    申请号:EP80201130

    申请日:1980-11-27

    IPC分类号: C22C21/16 C22F01/04

    CPC分类号: C22C21/16

    摘要: A 2000 series aluminum alloy characterized by high strength, high fatigue resistance, and high fracture toughness consists essentially of 4.2 to 4.7 percent copper, 1.3 to 1.8 percent magnesium, 0.8 to 1.3 percent manganese, 0.08 to 0.15 percent zirconium, maximums of 0.15 percent iron, 0.12 percent silicon, 0.25 percent zinc, 0.15 percent titanium, 0.10 percent chromium, 0.05 percent of each of any other trace elements present, and a maximum total of such other trace elements of 0.15 percent, the balance of the alloy being aluminum. The foregoing alloy is hot-worked and heat-treated to yield a final wrought product having a highly elongated and substantially unrecrystallized microstructure.

    Method of producing a plate product or an extruded product from an aluminium alloy
    5.
    发明公开
    Method of producing a plate product or an extruded product from an aluminium alloy 失效
    一种用于生产板或由Al基合金的挤出产品的方法。

    公开(公告)号:EP0038605A1

    公开(公告)日:1981-10-28

    申请号:EP81200434.9

    申请日:1981-04-15

    IPC分类号: C22C21/16 C22F1/04

    CPC分类号: C22C21/16

    摘要: A 2000 series aluminum alloy characterized by high strength, very high fatigue resistance, and very high fracture toughness consists essentially of3.8%to 4.4 % copper, 1.2%to 1.8% magnesium, 0.3% to 0.9% manganese, maximums of 0.12% silicon, 0.15% iron, 0.25% zinc, 0.15 % titanium, 0.10% chromium, 0.05%of each of any othertrace elements present, and a maximum total of such other trace elements of 0.15%, the balance of the alloy being aluminum. It is preferred, especially for plate products, that the maximum iron and silicon levels be restricted to 0.12% and 0.10%, respectively. For extruded products, the foregoing alloy is hot worked to yield a wrought product having a substantially unrecrystallized structure. For plate products, the alloy is subjected to room temperature preaging and a cold rolling treatment to provide a reduction in gauge of from 9% to 13%.

    摘要翻译: 由高强度,非常高的抗疲劳性,和非常高的断裂韧性besteht的本质上为3.8%至4.4%的铜为特征的甲2000系列铝合金,1.2%至1.8%的镁,0.3%至0.9%的锰,0.12%的最大值,以硅树脂, 0:15%的铁,0.25%的锌,0.15%至钛,铬0.10%,每个存在的任何其它微量元素的0.05%,最大总寻求的00等微量元素:15%,该合金是铝的平衡。 它是优选的,尤其是爱对于板产品,所做的最大铁和硅的水平被限制在12:分别为10%,12%和12。 对于挤出产品,前述的合金进行热加工,以产生具有基本上未再结晶结构的锻造产品。 对于板的产品,所述合金进行室温预老化和冷轧处理以提供在从9%至13%计的降低。

    Aluminum-lithium alloy
    7.
    发明公开
    Aluminum-lithium alloy 失效
    铝Lithiumlegierung。

    公开(公告)号:EP0214381A1

    公开(公告)日:1987-03-18

    申请号:EP86108331.9

    申请日:1986-06-19

    CPC分类号: C22C21/12

    摘要: An aluminium-lithium alloy exhibiting good fracture toughness and relatively high strength, having a composition of 2.0 to 2.4% Li, 0.3 to 0.9% Mg. 2.1 to 2.9% Cu, 0.08 to 0.15% Zr, up to 0.15% Fe, up to 0.12% Si, up to 0.25% Zn, up to 0.15% Ti, up to 0.1% Cr, balance Al. A preferred composition has 2.2% Li, 0.6% Mg, 2.5% Cu, 0.12% Zr, balance Al.

    摘要翻译: 具有良好的断裂韧性和较高强度的铝锂合金,其组成为2.0-2.4%的Li,0.3-0.9%的Mg。 2.1〜2.9%的Cu,0.08〜0.15%的Zr,Fe:0.15%以下,Si:0.12%以下,Zn:0.15%以下,Cr:0.1%以下,Al平衡。 优选的组合物具有2.2%Li,0.6%Mg,2.5%Cu,0.12%Zr,余量为Al。

    Aluminum-lithium alloy (2)
    10.
    发明公开
    Aluminum-lithium alloy (2) 失效
    铝Lithiumlegierungen。

    公开(公告)号:EP0149194A2

    公开(公告)日:1985-07-24

    申请号:EP84115929.6

    申请日:1984-12-20

    IPC分类号: C22C21/00

    CPC分类号: C22C21/00

    摘要: An aluminum-lithium alloy exhibiting a good blend of fracture toughness and high strength has a nominal composition of 2.45 percent lithium, 1.4 percent copper, and 0.12 percent zirconium with the balance being aluminum and trace elements.

    摘要翻译: 表现出良好的断裂韧性和高强度共混物的铝锂合金的标称组成为2.45%的锂,1.4%的铜和0.12%的锆,余量为铝和微量元素。