CPC分类号: C09C1/42 , B82Y30/00 , C01P2002/72 , C01P2002/88 , C01P2004/03 , C01P2004/13 , C01P2004/16 , C08L25/06 , C08L63/00 , C08L67/02 , C08L69/00
摘要: A process for the preparation of modified nanoclay in one case comprises the steps of providing an organoclay, dispersing the organoclay in a solvent or mixture of solvents and/or surfactant, providing nariotubes or nanowires, dispersing the nanotubes or nanowires in a solvent or mixture of solvents and/or surfactant, and mixing the organoclay suspension with the nanotube and/or nanowire suspension. The organoclays modified with nanowires or nanotubes provide nanoadditives, which have enhanced thermal stability and electrical conductivity properties. The nanoadditive may include an inherently conducting polymer such as polyaniline. Also provided are polmyer composites including the nanoadditive.