A METHOD FOR ESTERIFYING LIGNIN WITH AT LEAST ONE FATTY ACID
    2.
    发明公开
    A METHOD FOR ESTERIFYING LIGNIN WITH AT LEAST ONE FATTY ACID 审中-公开
    方法酯化木质素至少一种脂肪酸

    公开(公告)号:EP2888273A1

    公开(公告)日:2015-07-01

    申请号:EP13759801.7

    申请日:2013-08-22

    IPC分类号: C07G1/00

    CPC分类号: C07G1/00

    摘要: The present invention relates to a method for producing lignin esterified with at least one fatty acid, wherein the method comprises the following steps: (i) reacting acetylated lignin with at least one fatty acid under the influence of heating and distilling at least part of the acetic acid formed during the reaction away from the reaction mixture, wherein per each mole of acetyl groups present in the lignin an excess molar amount of at least one fatty acid is used; and (ii) recovering lignin esterified with at least one fatty acid formed in step (i).

    LIGNIN AND METHOD AND SYSTEM FOR PROCESSING LIGNIN
    3.
    发明公开
    LIGNIN AND METHOD AND SYSTEM FOR PROCESSING LIGNIN 有权
    LIGNIN SOWIE VERFAHREN UND SYSTEM ZUR VERARBEITUNG VON LIGNIN

    公开(公告)号:EP2831088A1

    公开(公告)日:2015-02-04

    申请号:EP13718603.7

    申请日:2013-03-26

    IPC分类号: C07G1/00 C08L97/00

    摘要: The invention relates to a method for processing lignin. The method comprises: feeding lignin material (11) to the system, decreasing particle size of the lignin material (11) in a grinding device (30) in order to manufacture lignin powder having particle size distribution wherein at least 85 wt.% of the lignin agglomerates and particles are less than 300 microns, and increasing dry solids content of the lignin material at least 5 percentage units while decreasing the particle size in the grinding device (30). In addition, the invention relates to a system for processing lignin, a lignin powder, a method for manufacturing a product comprising lignin, a system for manufacturing a product comprising lignin and a product comprising lignin powder.

    摘要翻译: 本发明涉及一种处理木质素的方法。 该方法包括将木质素材料进料给系统,减少研磨装置中的木质素材料的粒度,以制备具有粒度分布的木质素粉末,其中至少85wt。 木质素附聚物和颗粒的%小于300微米,并且增加木质素材料的干固体含量至少5个百分比,同时降低研磨装置中的粒度。 此外,本发明涉及一种用于处理木质素,木质素粉末,用于制造包括木质素的产品的方法,用于制造包括木质素的产品和包含木质素粉末的产品的系统。