摘要:
An exemplary embodiment of the present invention discloses an aluminum-based blank including: a first plated steel plate; a second plated steel plate connected to the first plated steel plate; and a joint connecting the first plated steel plate and the second plated steel plate at a boundary between the first plated steel plate and the second plated steel plate.
摘要:
Disclosed are a steel plate for a line pipe having excellent hydrogen induced crack resistance with a tensile strength of 450 MPa or more, and a preparation method thereof. According to the present invention, the steel plate for a line pipe, having excellent hydrogen induced crack resistance comprises: 0.03ˆ¼0.05 wt% of carbon (C); 0.2-0.3 wt% of silicon (Si); 0.5-1.3 wt% of manganese (Mn); 0.010 wt% or less of phosphorus (P); 0.005 wt% or less of sulfur (S); 0.02-0.05 wt% of aluminum (Al); 0.2-0.5 wt% of nickel (Ni); 0.2-0.3 wt% of chromium (Cr); 0.03-0.05 wt% of niobium (Nb); 0.02-0.05 wt% of vanadium (V); 0.01-0.02 wt% of titanium (Ti); 0.001-0.004 wt% of calcium (Ca); and a balance of iron (Fe) and inevitable impurities, and has a tensile strength of 450 MPa or more.
摘要:
Disclosed is a method for producing a coated steel sheet. A method for producing a coated steel sheet according to the present invention includes the steps of: reheating a steel slab containing 0.15-0.25 wt% of carbon (C), more than 0 wt% but not more than 1.5 wt% of silicon (Si), 1.5-2.5 wt% of manganese (Mn), more than 0 wt% but not more than 1.8 wt% of aluminum (Al), 0.3-1.0 wt% of chromium (Cr), more than 0 wt% but not more than 0.03 wt% of titanium (Ti), more than 0 wt% but not more than 0.03 wt% of niobium (Nb), and the balance of iron (Fe) and unavoidable impurities; hot-rolling, cooling and coiling the steel slab, thereby producing a hot-rolled steel sheet; pickling the hot-rolled steel sheet, followed by cold rolling; annealing the cold-rolled steel sheet at a temperature between 820°C and 870°C, followed by cooling at a finish-cooling temperature between 350°C and 450°C; tempering the cooled steel sheet at a temperature between 450°C and 550°C; and hot-dip galvanizing the tempered steel sheet.
摘要:
Disclosed is an invention relating to a method for producing a molded article. The method for producing the molded article includes the steps of: preparing a first steel plate and a second steel plate; joining the first steel plate and the second steel plate to each other, thereby preparing a joined steel plate; heating the joined steel plate at a temperature between 910°C and 950°C; subjecting the heated joined steel plate to hot-press molding, thereby preparing an intermediate molded article; and cooling the intermediate molded article, wherein the first steep plate has a tensile strength (TS) higher than that of the second steel plate.
摘要:
Disclosed are a steel sheet having excellent and a method for producing the same. The disclosed steel sheet comprises, by weight, 0.005-0.06% carbon (C), 0.2% or less silicon (Si), 1.0-2.0% manganese (Mn), 0.01% or less sulfur (S), 0.2-2.0% aluminum (Al), one or more of chromium (Cr) and molybdenum (Mo) in an amount satisfying 0.3 ≤ [Cr wt%]+0.3[Mo wt%] ≤ 2.0, and 0.008% or less nitrogen (N), with the remainder being iron (Fe) and inevitable impurities, wherein the density of dislocations in the ferrite matrix of the steel sheet is 1x10 13 /m 2 or more.