    Abstract: The invention provides a water resistant molding material that can be stably manufactured while being excellent in water resistance after dried, and a producing method for the water resistant molding material. The water resistant molding material comprises a binder resin containing a polyvinyl alcohol resin, a viscosity control agent, water and a filler, wherein the concentration of acetate ions is adjusted in the range from 500 to 12,000 ppm by blending, for example, an acetate ion controlling agent (such as NH4NO3, NaOH and KCl).

    Molding material and method of producing molding material
    3.
    发明专利
    Molding material and method of producing molding material 有权
    成型材料及其制造方法

    公开(公告)号:JP2008291075A

    公开(公告)日:2008-12-04

    申请号:JP2007136270

    申请日:2007-05-23

    CPC classification number: C08K3/01 C08K2201/019 C08L29/04

    Abstract: PROBLEM TO BE SOLVED: To provide a water-resistant molding material being manufactured stably and excellent in water resistance after drying, and its manufacturing method.
    SOLUTION: The water-resistant molding material or the like contains a binder resin containing a polyvinyl alcohol resin; a viscosity modifier; water; and aggregate. The concentration of acetate ions in the water-resistant molding material is set at a value within the range of 500 to 12,000 ppm by blending, e.g., an acetate ion modifier (NH
    4 NO
    3 , NaOH, and KC1 or the like), etc.
    COPYRIGHT: (C)2009,JPO&INPIT

    Abstract translation: 待解决的问题:提供稳定制造的耐水成型材料和干燥后耐水性优异的制造方法。 防水成型材料等含有含有聚乙烯醇树脂的粘合剂树脂; 粘度调节剂; 水; 并聚合。 将耐水性成型材料中的乙酸根离子的浓度通过配合例如乙酸根离子改性剂(NH 3 SB <3> <3>)而设定在500〜12000ppm的范围内, / SB>,NaOH和KCl等)等。版权所有(C)2009,JPO&INPIT

    軽量造形材料
    4.
    发明专利

    公开(公告)号:JPWO2007055257A1

    公开(公告)日:2009-04-30

    申请号:JP2007544167

    申请日:2006-11-09

    Abstract: 軽量化材の添加量を多くした場合であっても、所定形状を有する絞り口を介して容易に絞りだすことができる程度の流動性と、絞り口の所定形状をそのまま保持することができる程度の保形性に優れ、しかも膨張問題を解消して、優れた保管性が得られるクリーム状の軽量造形材料を提供する。ポリビニルアルコール系樹脂を含むバインダー樹脂と、粘度調整剤と、水と、軽量化材と、を含有する軽量造形材料であって、軽量化材の添加量を、全体量に対して、3〜22重量%の範囲内の値とするとともに、水の添加量を、全体量に対して、65〜92重量%の範囲内の値とし、かつ、水/ポリビニルアルコール系樹脂の配合比率(重量比)を3〜300の範囲内の値とする。