公开(公告)号:JP5369864B2
公开(公告)日:2013-12-18
申请号:JP2009105830
申请日:2009-04-24
申请人: 住友金属鉱山株式会社
摘要: PROBLEM TO BE SOLVED: To provide a nickel powder wherein the content of impurities is low using a method for producing a nickel powder where nickel hydroxide obtained by a wet process is reduced, and to provide a method for producing the same so that the organic matter in a waste liquid is easily recovered. SOLUTION: The nickel powder is obtained by a production method including: a stage (A) where a nickel chloride aqueous solution is neutralized with an alkali aqueous solution so as to produce the precipitates of nickel hydroxide; a stage (B) where the nickel hydroxide is heat-treated in the air so as to produce nickel oxide; a stage (C) where the nickel oxide is reduced in a reducing gas atmosphere so as to obtain the nickel powder; and a stage (D) where the nickel powder after the reduction is cleaned with a tartaric acid aqueous solution at the pH of ≤6.1. COPYRIGHT: (C)2011,JPO&INPIT
-
公开(公告)号:JPWO2017069067A1
公开(公告)日:2017-10-19
申请号:JP2017506959
申请日:2016-10-14
申请人: 住友金属鉱山株式会社
摘要: 湿式法を用いた場合であっても、安価で、かつ高性能なニッケル粉末を得ることができるニッケル粉末の製造方法を提供することを目的とする。少なくとも水溶性ニッケル塩、ニッケルよりも貴な金属の塩、還元剤、水酸化アルカリ、およびアミン化合物と水とを含む反応液中において、還元反応によりニッケル晶析粉を得る晶析工程を有するニッケル粉末の製造方法であって、前記晶析工程で混合させる前記還元剤はヒドラジンであり、前記アミン化合物は、ヒドラジンの自己分解抑制剤であって、分子内に第1級アミノ基を2個以上含有するか、あるいは、分子内に第1級アミノ基を1個、かつ第2級アミノ基を1個以上含有しており、前記反応液中のニッケルのモル数に対する前記アミン化合物のモル数の割合が0.01モル%〜5モル%の範囲であることを特徴とする。
-
公开(公告)号:JPWO2011037150A1
公开(公告)日:2013-02-21
申请号:JP2011533011
申请日:2010-09-22
申请人: 住友金属鉱山株式会社
CPC分类号: C22C19/03 , B22F1/02 , B22F9/12 , B22F2999/00 , B22F2202/13
摘要: 結晶性に優れ、収縮開始温度が高く、高温に至るまで焼結に伴う収縮が抑制されるとともに樹脂バインダの分解温度に影響を及ぼさないニッケル微粉及びその製造方法を提供することを目的とする。平均粒径が0.05〜0.3μm、比表面積径に対する結晶子径が60〜90%、硫黄含有量が0.1〜0.5質量%、及び酸素含有量が0.4〜1.5質量%であり、表面に酸素を含む厚さが2〜15nmの被覆層を有し、該被覆層の最外面がニッケル硫黄化合物及びニッケル酸素化合物を含む混合物で構成されるニッケル微粉とする。さらに、X線光電子分光法分析において、最外面に含有される硫黄化合物における硫化ニッケルの存在比が50%〜100%、ニッケル酸素化合物における水酸化ニッケルの存在比が0〜50%であることが好ましい。
-
-
-
-