1.
公开(公告)号:JP5522197B2
公开(公告)日:2014-06-18
申请号:JP2012114756
申请日:2012-05-18
Applicant: 旭硝子株式会社
IPC: C09J171/02 , C09J7/02 , H01L21/304
CPC classification number: C09J183/08 , C08G65/2609 , C08G65/2663 , C08G65/33351 , C08G65/336 , C08L2205/05 , C09J7/38 , C09J171/02 , C09J2483/00 , H01L21/6835 , H01L2221/6834 , Y10T428/2896
Abstract: To provide an adherence substance which has a low viscosity and good coatability, can be made solvent free, has good adhesion to an adherend and at the same time has excellent removability, can suppress peel electrostatic charge and is excellent in high speed peeling performance. An adherence substance which is obtainable by curing a curable composition comprising a silyl group-containing polymer (S) represented by the following formula (1): in the formula (1), R 1 represents a t-valent residue obtained by removing all hydroxy groups from a compound having t pieces of hydroxy groups in the molecule; R 2 represents a bivalent organic group; R 3 represents a monovalent organic group having from 1 to 20 carbon atoms; X is a hydroxy group or a hydrolyzable group; Y represents a bivalent group represented by the following formula (A) or a bivalent group represented by the following formula (B); a represents an integer of from 1 to 3; r represents an integer of from 1 to 1,000; t represents an integer of from 1 to 8; €ƒ€ƒ€ƒ€ƒ€ƒ€ƒ€ƒ€ƒ-OR 5 -€ƒ€ƒ€ƒ€ƒ€ƒ(B) in the formula (A), R 4 represents an alkylene group having from 2 to 8 carbon atoms; and in the formula (B), R 5 represents an alkylene group having from 2 to 4 carbon atoms.
-
公开(公告)号:JP5446265B2
公开(公告)日:2014-03-19
申请号:JP2008530927
申请日:2007-08-21
Applicant: 旭硝子株式会社
IPC: C08L71/02 , C08G65/336 , C08K5/19 , C08L33/04
CPC classification number: C08K5/19 , C08G18/4812 , C08G18/718 , C08G65/2609 , C08G65/2663 , C08G65/3322 , C08G65/33351 , C08G65/336 , C08G65/337 , C08L43/04 , C08L71/02 , C08L101/10 , C08L2666/14
-
公开(公告)号:JPWO2008062790A1
公开(公告)日:2010-03-04
申请号:JP2008545408
申请日:2007-11-20
Applicant: 旭硝子株式会社
Inventor: 輝彦 安田 , 輝彦 安田 , 佐藤 寿 , 寿 佐藤 , 浩志 和田 , 浩志 和田 , 泰仁 安達 , 泰仁 安達 , 知弘 林 , 知弘 林 , 鈴木 千登志 , 千登志 鈴木
IPC: C08F2/44 , C08F283/06 , C08G18/63
CPC classification number: C08G18/632 , C08G18/4072 , C08G18/482 , C08G18/5021 , C08G18/506 , C08G18/636 , C08G18/638 , C08G18/672 , C08G2101/0025 , C08G2101/005 , C08G2101/0083 , C08L27/18 , C08L75/04 , C08G18/48 , C08L2666/04
Abstract: 硬質ポリウレタンフォーム用ポリオールとの相溶性が高く、貯蔵安定性に優れると共に、硬質ポリウレタンフォームとした際に良好な断熱性能が得られるポリマー分散ポリオールの製造方法を提供する。ポリオール(X)中で重合性不飽和基を有するモノマーを重合させることにより、ポリマー微粒子がポリオール中に分散した硬質ポリウレタンフォーム用のポリマー分散ポリオールを製造する方法において、前記ポリオール(X)は、オキシエチレン基含有量が10質量%以上であるポリエーテルポリオール(Y)を含み、かつ前記重合性不飽和基を有するモノマーは、含フッ素アクリレートまたは含フッ素メタクリレートを含むことを特徴とするポリマー分散ポリオールの製造方法。
-
公开(公告)号:JP5594142B2
公开(公告)日:2014-09-24
申请号:JP2010532930
申请日:2009-10-06
Applicant: 旭硝子株式会社
IPC: C09J7/02 , B32B27/00 , B32B27/36 , C09J183/10 , C09J183/12 , C09J201/10
CPC classification number: C08G18/718 , B32B7/12 , B32B27/36 , B32B2405/00 , B32B2457/14 , C08G18/10 , C08G18/42 , C08G18/44 , C08G18/4825 , C08G18/4866 , C08G18/755 , C08G63/695 , C08G63/91 , C08G64/0266 , C08G64/42 , C08G65/336 , C09J7/22 , C09J7/35 , C09J167/00 , C09J169/00 , C09J171/02 , C09J175/04 , C09J2205/114 , C09J2467/00 , C09J2469/00 , C09J2471/00 , C09J2483/00 , Y10T428/2852 , Y10T428/2896 , C08G18/289
Abstract: To provide an adhesive laminate with which an adhesive deposit does not result even when a polyester-type substrate layer is used. An adhesive laminate comprising a polyester-type substrate layer and an adherence substance layer, wherein one surface of the polyester-type substrate layer is a treated surface subjected to adhesion-facilitating treatment, the adherence substance layer is in contact with the treated surface, and the adherence substance layer is a layer obtained by curing a curable composition containing the following silyl group-containing polymer (S). The silyl group-containing polymer (S) is a silyl group-containing polymer having a polyether chain, a polyester chain and/or a polycarbonate chain in its main chain and having a hydrolyzable silyl group at its molecular terminal.
-
-
6.
公开(公告)号:JP5040995B2
公开(公告)日:2012-10-03
申请号:JP2009509280
申请日:2008-04-02
Applicant: 旭硝子株式会社
IPC: C09J171/02 , C09J7/02 , C09J167/00 , G02B5/30 , H01L21/304
CPC classification number: C09J183/08 , C08G65/2609 , C08G65/2663 , C08G65/33351 , C08G65/336 , C08L2205/05 , C09J7/38 , C09J171/02 , C09J2483/00 , H01L21/6835 , H01L2221/6834 , Y10T428/2896
Abstract: To provide an adherence substance which has a low viscosity and good coatability, can be made solvent free, has good adhesion to an adherend and at the same time has excellent removability, can suppress peel electrostatic charge and is excellent in high speed peeling performance. An adherence substance which is obtainable by curing a curable composition comprising a silyl group-containing polymer (S) represented by the following formula (1): in the formula (1), R 1 represents a t-valent residue obtained by removing all hydroxy groups from a compound having t pieces of hydroxy groups in the molecule; R 2 represents a bivalent organic group; R 3 represents a monovalent organic group having from 1 to 20 carbon atoms; X is a hydroxy group or a hydrolyzable group; Y represents a bivalent group represented by the following formula (A) or a bivalent group represented by the following formula (B); a represents an integer of from 1 to 3; r represents an integer of from 1 to 1,000; t represents an integer of from 1 to 8; €ƒ€ƒ€ƒ€ƒ€ƒ€ƒ€ƒ€ƒ-OR 5 -€ƒ€ƒ€ƒ€ƒ€ƒ(B) in the formula (A), R 4 represents an alkylene group having from 2 to 8 carbon atoms; and in the formula (B), R 5 represents an alkylene group having from 2 to 4 carbon atoms.
-
公开(公告)号:JPWO2008062794A1
公开(公告)日:2010-03-04
申请号:JP2008545412
申请日:2007-11-20
Applicant: 旭硝子株式会社
IPC: C08G18/48
CPC classification number: C08G18/5021 , C08G18/4072 , C08G18/482 , C08G18/632 , C08G18/636 , C08G18/638 , C08G18/672 , C08G2101/0025 , C08G2101/005 , C08G2101/0083 , C08G18/48
Abstract: 低密度であって、寸法安定性が良好な硬質ポリウレタンフォームが得られると共に、使用するポリマー分散ポリオールと硬質ポリウレタンフォーム用ポリオールとの混合物を貯蔵した場合の貯蔵安定性に優れ、故に硬質ポリウレタンフォームを安定に製造できる硬質ポリウレタンフォームの製造方法を提供する。ポリオール成分(Z)とポリイソシアネート成分とを、発泡剤、整泡剤および触媒の存在下で反応させて硬質ポリウレタンフォームを製造する方法において、前記ポリオール成分(Z)は、平均水酸基価が200〜800mgKOH/gであり、かつポリオール(X)中で、含フッ素モノマーとスチレンとを含む重合性不飽和基を有するモノマーを重合させることにより、ポリマー微粒子がポリオール中に分散したポリマー分散ポリオール(A)を含有することを特徴とする硬質ポリウレタンフォームの製造方法。
-
-
公开(公告)号:JPWO2010041667A1
公开(公告)日:2012-03-08
申请号:JP2010532930
申请日:2009-10-06
Applicant: 旭硝子株式会社
IPC: C09J7/02 , B32B27/00 , B32B27/36 , C08G18/40 , C08G18/83 , C09J183/10 , C09J183/12 , C09J201/10
CPC classification number: C08G18/718 , B32B7/12 , B32B27/36 , B32B2405/00 , B32B2457/14 , C08G18/10 , C08G18/42 , C08G18/44 , C08G18/4825 , C08G18/4866 , C08G18/755 , C08G63/695 , C08G63/91 , C08G64/0266 , C08G64/42 , C08G65/336 , C09J7/22 , C09J7/35 , C09J167/00 , C09J169/00 , C09J171/02 , C09J175/04 , C09J2205/114 , C09J2467/00 , C09J2469/00 , C09J2471/00 , C09J2483/00 , Y10T428/2852 , Y10T428/2896 , C08G18/289
Abstract: ポリエステル系の基材層を用いても糊残りが発生しない粘着積層体を提供する。ポリエステル系基材層と粘着体層とを有する粘着積層体であって、ポリエステル系基材層の一面が易接着処理された処理面であり、粘着体層が該処理面に当接しており、粘着体層が下記シリル基含有重合体(S)を含む硬化性組成物を硬化させて得られる層である。なお、シリル基含有重合体(S)は、主鎖に、ポリエーテル鎖、ポリエステル鎖、および/またはポリカーボネート鎖を有し分子末端に加水分解性シリル基を有するシリル基含有重合体である。
-
公开(公告)号:JPWO2008123552A1
公开(公告)日:2010-07-15
申请号:JP2009509280
申请日:2008-04-02
Applicant: 旭硝子株式会社
IPC: C09J201/10 , C09J7/02 , C09J183/12 , G02B5/30
CPC classification number: C09J183/08 , C08G65/2609 , C08G65/2663 , C08G65/33351 , C08G65/336 , C08L2205/05 , C09J7/38 , C09J171/02 , C09J2483/00 , H01L21/6835 , H01L2221/6834 , Y10T428/2896
Abstract: 低粘度で塗工性が良く、無溶剤化が可能であり、かつ被着体への密着性が良好であるとともに再剥離性に優れ、剥離帯電量が抑制され、かつ高速剥離性にも優れる粘着体を提供する。下記一般式(1)で表されるシリル基含有重合体(S)を含む硬化性組成物を硬化させて得られる粘着体。[化1]式(1)中、R1は一分子中にt個の水酸基を有する化合物から全部の水酸基を除いたt価の残基を示し、R2は2価の有機基を示し、R3は炭素数1〜20の1価の有機基を示し、Xは水酸基又は加水分解性基を示し、Yは一般式(A)で表される2価の基または一般式(B)で表される2価の基を示し、aは1〜3の整数を示し、rは1〜1000の整数を示し、tは1〜8の整数を示す。式(A)中、R4は炭素数2〜8のアルキレン基を示す。式(B)中、R5は炭素数2〜4のアルキレン基を示す。
-
-
-
-
-
-
-
-
-