公开(公告)号:KR1020110124826A
公开(公告)日:2011-11-18
申请号:KR1020100044232
申请日:2010-05-12
申请人: 주식회사 크린아리
发明人: 이학섭
CPC分类号: C04B33/04 , A01K63/00 , B28B5/021 , B28C5/0843 , C04B33/131
摘要: PURPOSE: A bottom material for an aquarium based on natural materials and a method for manufacturing the same are provided to deodorize a fish smell of water and to promote the growth of fish and water plants using zeolite, bentonite, and tourmaline. CONSTITUTION: A bottom material for an aquarium based on natural materials includes 45 weight% of zeolite, 40 weight% of bentonite, 3 weight% of tourmaline, and 12 weight% of purified water. The bottom material is formed into granules of 0.5-1mm, granules of 1-3mm, and granules of 3-7mm. A method for manufacturing the bottom material includes the following: The zeolite, the bentonite, the tourmaline, and the purified water are mixed and kneaded in a mixer(S10). The mixture is transferred using a first transferring conveyor(S12). The transferred material is formed into a sphere form. The shaped material is transferred to a plasticizing part using a second transferring conveyor(S30). The transferred material is plasticized at a temperature between 700 and 800 degrees Celsius. The plasticized material is classified.
摘要翻译: 目的:提供一种基于天然材料的水族箱的底部材料及其制造方法,用于对鱼的气味进行除臭并利用沸石,膨润土和电气石促进鱼和水植物的生长。 构成:基于天然材料的水族箱的底部材料包括45重量%的沸石,40重量%的膨润土,3重量%的电气石和12重量%的净化水。 底部材料形成0.5-1mm的颗粒,1-3mm的颗粒,3-7mm的颗粒。 制造底部材料的方法包括以下步骤:在混合器中将沸石,膨润土,电气石和纯净水混合并捏合(S10)。 使用第一转运输送机转移混合物(S12)。 转移的材料形成球形。 成型材料使用第二传送输送机转移到塑化部件(S30)。 转移的材料在700和800摄氏度之间的温度下增塑。 塑化材料分类。
-
公开(公告)号:KR1020110080454A
公开(公告)日:2011-07-13
申请号:KR1020100000693
申请日:2010-01-06
申请人: 주식회사 크린아리
发明人: 이학섭
摘要: PURPOSE: A deodorant composition, a deodorizing agent manufacturing method using the same, and a deodorizing agent manufactured thereby are provided to prevent secondary pollution by using natural materials. CONSTITUTION: A deodorant composition comprises zeolite, bentonite, vegetable fiber, granite soil, and calcium hydroxide. The vegetable fiber is selected from a group comprising cellulose, rice straw, and rice straw ash. A deodorizing agent manufacturing method is constituted as follows. A mixture is formed by mixing zeolite, bentonite, vegetable fiber, granite soil, and calcium hydroxide. The mixture is kneaded. Molding is performed after extruding dough. The molding is cut and rolled. A processed product is dried two times. The product is cultivated is dipped in a microorganism cultivator.
摘要翻译: 目的:提供除臭剂组合物,使用其的除臭剂制造方法和由其制造的除臭剂,以通过使用天然材料来防止二次污染。 构成:除臭剂组合物包括沸石,膨润土,植物纤维,花岗岩土壤和氢氧化钙。 植物纤维选自纤维素,稻草,稻草灰等。 除臭剂制造方法如下构成。 通过混合沸石,膨润土,植物纤维,花岗岩土壤和氢氧化钙形成混合物。 将混合物捏合。 在挤出面团之后进行成型。 将成型品切割并卷起。 将加工产品干燥两次。 将培养的产物浸入微生物培养器中。
-
-
公开(公告)号:KR1020100004100A
公开(公告)日:2010-01-12
申请号:KR1020090129450
申请日:2009-12-23
申请人: 주식회사 크린아리
发明人: 이학섭
CPC分类号: A47G9/1045 , A47G9/00 , A47G9/007 , A47G2009/006 , A47G2200/143 , A61H39/04
摘要: PURPOSE: A functional pillow using natural material is provided, which emits far infrared ray, negative ion, and phytoncide component and can obtain finger-pressure effect. CONSTITUTION: A functional pillow using natural material comprises a lining(10) and an outer cover(20) which have a pocket form; a zipper(30) which is formed in the lining and outer cover for content exchange; and a filler providing cushion and functionality to the pillow. The filler consists of zeolite 30 weight%, bentonite 30 weight%, cypress 15%, tourmaline 10 weight%, pine resin powder 5 weight%, wormwood powder 5%, and vegetable fiber 5%. The outer cover is formed by sewing lots of upper cover and lower covers and side cover.
摘要翻译: 目的:提供使用天然材料的功能枕头,发射远红外线,负离子和植物苷成分,可获得手指压力效果。 构成:使用天然材料的功能枕头包括具有口袋形式的衬里(10)和外盖(20); 拉链(30),其形成在衬里和外盖中用于内容交换; 以及为枕头提供缓冲和功能的填充物。 填料由沸石30重量%,膨润土30重量%,柏树15%,电气石10重量%,松树脂5重量%,蒿木粉5%,植物纤维5%组成。 外盖通过缝合大量上盖和下盖和侧盖而形成。
-
-
-