公开(公告)号:KR1020080080392A
公开(公告)日:2008-09-03
申请号:KR1020087017597
申请日:2006-12-18
申请人: 바스프 에스이
发明人: 헤흘러,클라우스 , 루펠,빌헬름 , 쉰들러,괴츠-페터 , 클란너,카타리나 , 바슬러,한스-위르겐 , 디터레,마르틴 , 클라페르트,카를-하인리히 , 뮐러-엥겔,클라우스요아힘
CPC分类号: C07C5/3335 , B01J8/008 , B01J8/02 , B01J8/18 , B01J19/02 , B01J2219/00033 , B01J2219/0236 , B01J2219/0286 , C07C5/321 , C07C5/333 , C07C5/48 , C07C45/33 , C07C45/35 , C07C51/215 , C07C51/252 , C07C51/43 , C07C67/08 , C22C38/001 , C22C38/005 , C22C38/02 , C22C38/04 , C22C38/34 , C22C38/40 , C23C10/08 , C23C10/50 , Y02P20/52 , Y02T50/67 , C07C11/06 , C07C57/04 , C07C69/54 , C07C11/04 , C07C47/22
摘要: The invention relates to a method for the continuous heterogeneously catalysed partial dehydrogenation of at least one hydrocarbon to be dehydrogenated, in a reactor, the side of the reactor which comes into contact with the reaction gas consisting of a steel material having a particular element composition, and for the partial oxidation of the dehydrogenated hydrocarbon and the reactor itself.
摘要翻译: 本发明涉及在反应器中与待脱氢的至少一种烃的连续非均相催化部分脱氢的方法,该反应器与由具有特定元素组成的钢材组成的反应气体接触, 并且用于脱氢烃和反应器本身的部分氧化。
-
公开(公告)号:KR101438838B1
公开(公告)日:2014-09-05
申请号:KR1020087017597
申请日:2006-12-18
申请人: 바스프 에스이
发明人: 헤흘러,클라우스 , 루펠,빌헬름 , 쉰들러,괴츠-페터 , 클란너,카타리나 , 바슬러,한스-위르겐 , 디터레,마르틴 , 클라페르트,카를-하인리히 , 뮐러-엥겔,클라우스요아힘
CPC分类号: C07C5/3335 , B01J8/008 , B01J8/02 , B01J8/18 , B01J19/02 , B01J2219/00033 , B01J2219/0236 , B01J2219/0286 , C07C5/321 , C07C5/333 , C07C5/48 , C07C45/33 , C07C45/35 , C07C51/215 , C07C51/252 , C07C51/43 , C07C67/08 , C22C38/001 , C22C38/005 , C22C38/02 , C22C38/04 , C22C38/34 , C22C38/40 , C23C10/08 , C23C10/50 , Y02P20/52 , Y02T50/67 , C07C11/06 , C07C57/04 , C07C69/54 , C07C11/04 , C07C47/22
摘要: 본 발명은, 반응 기체와 접촉하는 면 쪽이 특정의 원소 조성을 갖는 스틸 재료로 제작된 반응기에서, 적어도 1종의 탈수소화될 탄화수소의 불균일 촉매작용 연속 부분적 탈수소화를 위한 방법, 및 상기 탈수소화된 탄화수소의 부분적 산화 방법 및 그 반응기 자체에 관한 것이다.
탈수소화, 불균일 촉매, 탄화수소, 프로판, 프로필렌-
公开(公告)号:KR1020060120589A
公开(公告)日:2006-11-27
申请号:KR1020067003456
申请日:2004-07-15
申请人: 바스프 에스이
发明人: 데메터,위르겐 , 죄트예,올리버 , 바슬러,한스-위르겐 , 다이닝거,위르겐 , 클라페르트,칼-하인리히 , 빈터링,헬무트
CPC分类号: C08G69/28 , B01J19/02 , B01J2219/0236 , B01J2219/0286 , B01J2219/029 , C08G69/04
摘要: Disclosed is a method for producing polyamides and the oligomers or mixtures thereof, optionally with additional reaction products, by reacting a reaction mixture containing monomers that comprise CN groups or -CONH2 groups, other optional polyamide-forming monomers and/or oligomers, and water in a device. Said method is characterized in that the surfaces of the device, which enter in contact with the reaction mixture, are entirely or partly made of a material that is selected among a group comprising: a) an austenitic steel containing 15 to 25 percent by weight of chromium, 3 to 35 percent by weight of nickel, 0 to 10 percent by weight of molybdenum, and other optional alloy components, the balance being made up of iron and the percentages by weight being in relation to a); b) a duplex steel containing 20 to 30 percent by weight of chromium, 3 to 10 percent by weight of nickel, 0 to 5 percent by weight of molybdenum, and other optional alloy components, the balance being made up of iron and the percentages by weight being in relation to b); and c) a basic nickel alloy containing 12 to 25 percent by weight of chromium, 12 to 20 percent by weight of molybdenum, and other optional alloy components, the balance being made up of nickel and the percentages being in relation to c). Also disclosed are devices that are used in or intended for such a method.
摘要翻译: 公开了通过使包含CN基团或-CONH 2基团的单体,其它任选的聚酰胺形成单体和/或低聚物的反应混合物和/或其混合物中的水反应来制备聚酰胺及其低聚物或其混合物,任选地具有另外的反应产物的方法 一个装置。 所述方法的特征在于,与反应混合物接触的装置的表面完全或部分地由选自以下的材料制成:a)奥氏体钢,其含有15至25重量%的 铬,3〜35重量%的镍,0〜10重量%的钼和其它任选的合金成分,余量由铁组成,重量百分比相对于a); b)含有20至30重量%的铬,3至10重量%的镍,0至5重量%的钼以及其它任选的合金成分的双相钢,余量由铁组成,其百分比由 重量相对于b); 和c)含有12至25重量%的铬,12至20重量%的钼和其它任选的合金组分的碱性镍合金,余量由镍组成,其百分比相对于c)。 还公开了用于或用于这种方法的装置。
-
-