公开(公告)号:US20230234883A1
公开(公告)日:2023-07-27
申请号:US18192123
申请日:2023-03-29
Applicant: AGC Inc.
Inventor: Yuki AOSHIMA , Takahiro MASHIMO
CPC classification number: C03C17/002 , C03C17/326 , C03C17/3441 , C03C17/3626 , C03C2217/73 , C03C2217/90
Abstract: A glass laminate, in which an inorganic laminated film having a total thickness of 90 to 500 nm is laminated on a surface of a glass plate with an adhesive film including a resin film interposed therebetween, a carbon-containing film thinner than the inorganic laminated film is attached to a surface of the inorganic laminated film, a storage elastic modulus of an outermost surface on the inorganic laminated film side that is measured by a nanoindentation method using a flat punch indenter under conditions of 1 Hz and 28° C. is 50 MPa to 30 GPa, and a loss coefficient of the outermost surface on the inorganic laminated film side that is measured by the nanoindentation method using the flat punch indenter under conditions of 1 Hz and 28° C. is 0.005 to 0.14.
-
2.
公开(公告)号:US20210114924A1
公开(公告)日:2021-04-22
申请号:US17138118
申请日:2020-12-30
Applicant: AGC INC.
Inventor: Misa INAMOTO , Satoru TOMENO , Yuki AOSHIMA
Abstract: The present invention relates to a glass sheet including a first main surface and a second main surface opposing the first main surface, in which the glass sheet has an affected layer directly below the first main surface, in at least a part of the first main surface, an average element length RSm is from 2500 nm to 6000 nm, a root-mean-square height Sq is from 3 nm to 45 nm, and a skewness Ssk is a negative value.
-
3.
公开(公告)号:US20190061314A1
公开(公告)日:2019-02-28
申请号:US16081198
申请日:2017-02-07
Applicant: AGC INC.
Inventor: Yuki AOSHIMA , Hidefumi ODAKA
Abstract: A laminated substrate for an electrochromic dimmer element includes a glass substrate; and a transparent conductive film. The glass substrate includes a silicon oxide, an aluminum oxide, a boron oxide, an alkaline earth metal oxide, and an alkali metal oxide in a total amount of 90 mol % or more, and includes the alkali metal oxide in a total amount of 12 mol % or less.The transparent conductive film includes an indium oxide film containing tin, and a tin oxide film containing at least one of tantalum, antimony and fluorine, in this order from a glass substrate side.The indium oxide film is formed directly on the glass substrate, a refractive index and an extinction coefficient of the indium oxide film at a wavelength of 1.3 μm is less than 0.4, and greater than 0.4, respectively.A film thickness of the tin oxide film is greater than 35 nm.
-
-