ALUMINUM-MAGNESIUM-LITHIUM ALLOYS, AND METHODS FOR PRODUCING THE SAME
    1.
    发明申请
    ALUMINUM-MAGNESIUM-LITHIUM ALLOYS, AND METHODS FOR PRODUCING THE SAME 审中-公开
    铝镁合金及其制造方法

    公开(公告)号:US20150376740A1

    公开(公告)日:2015-12-31

    申请号:US13828571

    申请日:2013-03-14

    Applicant: Alcoa Inc.

    CPC classification number: C22C21/06 C22F1/04 C22F1/047 C22F1/053

    Abstract: New aluminum-magnesium-lithium alloys, and methods for producing the same are disclosed. The alloys generally contain 2.0-3.9 wt. % Mg, 0.1-1.8 wt. % Li, up to 1.5 wt. % Cu, up to 2.0 wt. % Zn, up to 1.0 wt. % Ag, up to 1.5 wt. % Mn, up to 0.5 wt. % Si, up to 0.35 wt. % Fe, 0.05 to 0.50 wt. % of a grain structure control element, up to 0.10 wt. % Ti, and up to 0.10 wt. % of any other element, with the total of these other elements not exceeding 0.35 wt. %, the balance being aluminum.

    Abstract translation: 公开了新的铝 - 镁 - 锂合金及其制备方法。 合金通常含有2.0-3.9重量% %Mg,0.1-1.8wt。 %Li,高达1.5wt。 %Cu,高达2.0wt。 %Zn,至多1.0wt。 %Ag,高达1.5wt。 %Mn,至多0.5wt。 %Si,高达0.35wt。 %Fe,0.05〜0.50wt。 %的晶粒结构控制元件,高达0.10wt。 %Ti,和至多0.10wt。 任何其他元素的百分比,其中这些其他元素的总和不超过0.35重量%。 %,余量为铝。

    NEW 6XXX ALUMINUM ALLOYS AND METHODS OF MAKING THE SAME
    2.
    发明申请
    NEW 6XXX ALUMINUM ALLOYS AND METHODS OF MAKING THE SAME 审中-公开
    新的6XXX铝合金及其制备方法

    公开(公告)号:US20160348225A1

    公开(公告)日:2016-12-01

    申请号:US15165595

    申请日:2016-05-26

    Applicant: Alcoa, Inc.

    Abstract: New 6xxx aluminum alloy sheet products and methods of making the same are disclosed. The new methods may include preparing a 6xxx aluminum alloy sheet product for solution heat treatment, solution heat treating and then quenching the 6xxx aluminum alloy sheet product, and then exposing the 6xxx aluminum alloy sheet product to a treatment temperature of from 30° C. to 60° C. for 0.2 to 300 seconds. After the exposing step, the 6xxx aluminum alloy sheet product may be coiled and then placed in an ambient environment. Due to the post-quench heating and subsequent exposure to ambient, a preselected amount of Newtonian cooling may be induced, thereby creating a unique and consistent microstructure within the 6xxx aluminum alloy sheet products.

    Abstract translation: 公开了新的6xxx铝合金板产品及其制造方法。 新方法可能包括制备6xxx铝合金板材,用于固溶热处理,固溶热处理,然后淬火6xxx铝合金板材产品,然后将6xxx铝合金板材产品的处理温度从30°C暴露于 60℃下0.2至300秒。 在暴露步骤之后,6xxx铝合金板材产品可能被卷起,然后放置在周围环境中。 由于后淬火加热并随后暴露于环境中,可能会引起预选量的牛顿冷却,从而在6xxx铝合金板材产品内形成独特且一致的微观结构。