Abstract:
Thermoplastic molding compositions comprising A) from 10 to 93% by weight of a thermoplastic polyester B) from 1 to 20% by weight of a phosphinic salt C) from 1 to 20% by weight of a nitrogen-containing flame retardant D) from 5 to 50% by weight of a long-fiber reinforcing material with fiber length from 2 to 25 mm and L/D ratio from 500 to 4000 E) from 0 to 50% by weight of other additives, where the total of the percentages by weight of components A) to E) is 100%.
Abstract:
Thermoplastic molding compositions comprising A) from 10 to 93% by weight of a thermoplastic polyester B) from 1 to 20% by weight of a phosphinic salt C) from 1 to 20% by weight of a nitrogen-containing flame retardant D) from 5 to 50% by weight of a long-fiber reinforcing material with fiber length from 2 to 25 mm and L/D ratio from 500 to 4000 E) from 0 to 50% by weight of other additives, where the total of the percentages by weight of components A) to E) is 100%.
Abstract:
1. The invention relates to the use of polyester molding compositions composed of A) from 20 to 97.9% by weight of a thermoplastic polyester B) from 0.1 to 10% by weight of an epoxidized natural oil or fatty acid ester, or mixture of these, where the epoxide equivalent weight of component B) in accordance with DIN EN ISO 3001 is from 100 to 400 g/eq C) from 1 to 20% by weight of a metal salt of a phosphinic acid D) from 1 to 20% by weight of a melamine compound E) from 0 to 60% by weight of other additional substances, where the total of the percentages by weight of components A) to E) is 100%, for the production of stress-cracking-resistant and halogen-free flame-retardant polyester molding compositions.
Abstract:
1. The invention relates to the use of polyester molding compositions composed of A) from 20 to 97.9% by weight of a thermoplastic polyester B) from 0.1 to 10% by weight of an epoxidized natural oil or fatty acid ester, or mixture of these, where the epoxide equivalent weight of component B) in accordance with DIN EN ISO 3001 is from 100 to 400 g/eq C) from 1 to 20% by weight of a metal salt of a phosphinic acid D) from 1 to 20% by weight of a melamine compound E) from 0 to 60% by weight of other additional substances, where the total of the percentages by weight of components A) to E) is 100%, for the production of stress-cracking-resistant and halogen-free flame-retardant polyester molding compositions.
Abstract translation:1.本发明涉及聚酯成型组合物的使用,该组合物由以重量计0.1至10%重量的环氧化天然油或脂肪酸酯或其混合物的A)20至97.9%重量的热塑性聚酯B) ,其中根据DIN EN ISO 3001的组分B)的环氧当量为100至400g /当量C)1至20重量%的次膦酸金属盐D)1至20重量% 三聚氰胺化合物E)的重量为0至60重量%的其它另外的物质,其中组分A)至E)的重量百分比的总和为100%,用于生产耐应力开裂和卤素 - 自由阻燃聚酯成型组合物。