公开(公告)号:US20090136726A1
公开(公告)日:2009-05-28
申请号:US12223958
申请日:2007-01-15
申请人: Hitoshi Ishii , Seiichi Ibe , Tadayoshi Itoh , Shigeyoshi Nakaki
发明人: Hitoshi Ishii , Seiichi Ibe , Tadayoshi Itoh , Shigeyoshi Nakaki
IPC分类号: B32B7/02
CPC分类号: B32B27/08 , B32B27/34 , B65D75/002 , Y10T428/1328 , Y10T428/1334 , Y10T428/1352 , Y10T428/139 , Y10T428/1393 , Y10T428/24942 , Y10T428/31725 , Y10T428/31739 , Y10T428/31743 , Y10T428/31746
摘要: A heat shrinkable multilayer film comprising an outer surface layer (a) formed of a thermoplastic resin, a first intermediate layer (b1) formed of a polyamide resin, a second intermediate layer (b2) formed of a saponified product of an ethylene-vinyl acetate copolymer, and an inner surface layer (c) formed of a polyolefin resin, wherein the shrink of the heat shrinkable multilayer film in water at 90° C. is within a range of from 3 to 45% in each of machine and transverse directions, and the polyamide resin is a mixture of 60 to 90% by weight of an aliphatic polyamide having a melting point of 210° C. or higher and 10 to 40% by weight of an aromatic polyamide comprising isophthalic acid and terephthalic acid as main components.
摘要翻译: 一种热收缩性多层膜,其包含由热塑性树脂形成的外表面层(a),由聚酰胺树脂形成的第一中间层(b1),由乙烯 - 乙酸乙烯酯的皂化物形成的第二中间层(b2) 共聚物和由聚烯烃树脂形成的内表面层(c),其中在90℃的水中的热收缩多层膜的收缩在机器横向方向上在3〜45%的范围内, 聚酰胺树脂为60〜90重量%的熔点为210℃以上的脂肪族聚酰胺和10〜40重量%的以间苯二甲酸和对苯二甲酸为主要成分的芳香族聚酰胺的混合物。
-
2.
公开(公告)号:US07993713B2
公开(公告)日:2011-08-09
申请号:US12223958
申请日:2007-01-15
申请人: Hitoshi Ishii , Seiichi Ibe , Tadayoshi Itoh , Shigeyoshi Nakaki
发明人: Hitoshi Ishii , Seiichi Ibe , Tadayoshi Itoh , Shigeyoshi Nakaki
CPC分类号: B32B27/08 , B32B27/34 , B65D75/002 , Y10T428/1328 , Y10T428/1334 , Y10T428/1352 , Y10T428/139 , Y10T428/1393 , Y10T428/24942 , Y10T428/31725 , Y10T428/31739 , Y10T428/31743 , Y10T428/31746
摘要: A heat shrinkable multilayer film comprising an outer surface layer (a) formed of a thermoplastic resin, a first intermediate layer (b1) formed of a polyamide resin, a second intermediate layer (b2) formed of a saponified product of an ethylene-vinyl acetate copolymer, and an inner surface layer (c) formed of a polyolefin resin, whereinthe shrink of the heat shrinkable multilayer film in water at 90° C. is within a range of from 3 to 45% in each of machine and transverse directions, andthe polyamide resin is a mixture of 60 to 90% by weight of an aliphatic polyamide having a melting point of 210° C. or higher and 10 to 40% by weight of an aromatic polyamide comprising isophthalic acid and terephthalic acid as main components.
摘要翻译: 一种热收缩性多层膜,其包含由热塑性树脂形成的外表面层(a),由聚酰胺树脂形成的第一中间层(b1),由乙烯 - 乙酸乙烯酯的皂化物形成的第二中间层(b2) 共聚物和由聚烯烃树脂形成的内表面层(c),其中在90℃的水中的热收缩多层膜的收缩在机器横向方向上在3〜45%的范围内, 聚酰胺树脂为60〜90重量%的熔点为210℃以上的脂肪族聚酰胺和10〜40重量%的以间苯二甲酸和对苯二甲酸为主要成分的芳香族聚酰胺的混合物。
-