摘要:
A method for producing a toner, containing: dispersing, in an aqueous medium, an oil phase which contains an organic solvent, and a binder resin component contained in the organic solvent, where the binder resin component contains a crystalline polyester resin and an amorphous polyester resin; and removing the organic solvent from the dispersion to obtain the toner, in which the dispersing further contains heating and dissolving the crystalline polyester and the amorphous polyester in the organic solvent to obtain a solution, cooling the solution so as to recrystallize the crystalline polyester resin, and mechanically pulverizing the recrystallized crystalline polyester resin so as to obtain a crystalline polyester dispersion.
摘要:
A toner, comprising a colorant, a crystalline polyester resin, and an amorphous polyester resin, in which the crystalline polyester resin satisfies the following relations: 60≦(T2-cp)
摘要:
To provide a toner, which contains a binder resin, a colorant, and a releasing agent, wherein the binder resin contains a low molecular weight resin component, where the low molecular weight resin component has a resin softening coefficient (A), represented by the following formula (1), satisfying A>0.165, and has storage elastic modulus (dyne/cm2) G′(Tfb) satisfying G′(Tfb)≦1×104 where Tfb is a flow onset temperature (° C.) of the low molecular weight resin component as measured by a capillary rheometer: A=|[(r1)−ln G′(r2)]/(T1−T2)| Formula (1) (where T1 is temperature (° C.) at which storage elastic modulus G′(r1) is 1×105 (dyne/cm2) and T2 is temperature (° C.) at which storage elastic modulus G′(r2) is 1×103 (dyne/cm2) as measured by means of a viscoelasticity measuring device with measuring frequency of 1 Hz, and measuring distortion of 1 deg; and | | represents an absolute value.).
摘要翻译:为了提供含有粘合剂树脂,着色剂和脱模剂的调色剂,其中粘合剂树脂含有低分子量树脂组分,其中低分子量树脂组分具有树脂软化系数(A),由 (1)满足A> 0.165,并且具有满足G'(Tfb)≦̸ 1×104的储能弹性模量(dyne / cm 2)G'(Tfb),其中Tfb是流动起始温度(℃) 通过毛细管流变仪测量的低分子量树脂组分:A = | [(r1)-ln G'(r2)] /(T1-T2)| 储存弹性模量G'(r1)为1×10 5(达因/ cm 2)且T2为储存弹性模量G'(℃)的温度(℃)的式(1)(其中,T1为温度(℃) r2)是通过测量频率为1Hz的粘弹性测量装置测量的1×10 3(dyne / cm 2),测量失真度为1度,| |表示绝对值。
摘要:
To provide a toner, which contains a binder resin, a colorant, and a releasing agent, wherein the binder resin contains a low molecular weight resin component, where the low molecular weight resin component has a resin softening coefficient (A), represented by the following formula (1), satisfying A>0.165, and has storage elastic modulus (dyne/cm2) G′(Tfb) satisfying G′(Tfb)≦1×104 where Tfb is a flow onset temperature (° C.) of the low molecular weight resin component as measured by a capillary rheometer: A=|[ln G′(r1)−ln G′(r2)]/(T1−T2)| Formula (1) (where T1 is temperature (° C.) at which storage elastic modulus G′(r1) is 1×105 (dyne/cm2) and T2 is temperature (° C.) at which storage elastic modulus G′(r2) is 1×103 (dyne/cm2) as measured by means of a viscoelasticity measuring device with measuring frequency of 1 Hz, and measuring distortion of 1 deg; and ∥ represents an absolute value.)
摘要翻译:为了提供含有粘合剂树脂,着色剂和脱模剂的调色剂,其中粘合剂树脂含有低分子量树脂组分,其中低分子量树脂组分具有树脂软化系数(A),由 (1)满足A> 0.165,并且具有满足G'(Tfb)≦̸ 1×104的储能弹性模量(dyne / cm 2)G'(Tfb),其中Tfb是流动起始温度(℃) 通过毛细管流变仪测量的低分子量树脂组分:A = | [ln G'(r1)-ln G'(r2)] /(T1-T2)| 储存弹性模量G'(r1)为1×10 5(达因/ cm 2)且T2为储存弹性模量G'(℃)的温度(℃)的式(1)(其中,T1为温度(℃) r2)是通过测量频率为1Hz的粘弹性测量装置测量的1×103(dyne / cm 2),测量失真度为1度,∥表示绝对值。
摘要:
A toner including a binder resin comprising a modified polyester having an ester bond and a chemical bond other than the ester bond, and a crystalline polyester; and a release agent comprising a microcrystalline wax comprising a hydrocarbon having 20 to 80 carbon atoms which comprises 55 to 70% by weight of a linear hydrocarbon. The microcrystalline wax has an acid value of from 0.1 to 20 mgKOH/g and a melting point of from 65 to 90° C. The melting point is a temperature at which a local maximum endothermic peak is observed in a differential thermal curve measured by differential scanning calorimetry (DSC). The release agent is dispersed in the toner with a dispersion diameter of from 0.06 to 1.50 μm.
摘要:
A toner which contains: toner base particles having Dv of 4.0-6.0 μm; and two or more additives on surfaces of the toner base particles, where the additives contains Additives A and B, wherein the toner base particles are obtained by the method containing: dispersing, in an aqueous medium, an oil phase in which at least one of a crystalline polyester resin and a non-crystalline polyester resin is contained in an organic solvent, to prepare a dispersion liquid; and removing the organic solvent from the dispersion liquid, and wherein the Additive A has the largest average primary particle diameter in the additives and has CA of 5-10% where the CA is determined by the formula A, and the Additive B has the smallest average primary particle diameter in the additives and has CB of 45-100% where the CB is determined by the formula B.
摘要:
A toner including a binder resin which contains a crystalline polyester resin and a non-crystalline polyester resin, wherein the crystalline polyester resin has at least two diffraction peaks in a range of 20°
摘要:
A toner including a binder resin, a coloring agent, and a releasing agent, the toner formed by dispersing a toner liquid material which is prepared by dispersing the binder resin, the prepolymer, an elongation agent and/or a cross-linking agent for the prepolymer, the coloring agent, and the releasing agent in an organic solvent, dispersing the toner liquid material in an aqueous medium to obtain a liquid dispersion in at least one of cross linking reaction and elongation reaction, and removing the organic solvent from the liquid dispersion, and the toner satisfying the following relationship: 1.35
摘要:
The present invention provides a method for producing a toner, the method including: preparing a wax dispersion liquid by cooling a wax solution, in which a wax is heated and dissolved or dispersed in an organic solvent, in a container so that a standard deviation σ of a temperature distribution between a center portion of the container and an inner wall of the container is 0.5 or less and the cooling rate is 2.0° C./min or more, to precipitate wax particles in the wax solution; forming toner base precursor particles by adding an aqueous phase containing resin fine particles into an oil phase containing at least the wax dispersion liquid, a colorant and a binder resin and mixing the oil phase and the aqueous phase with each other; and preparing toner base particles by removing the solvent from the toner base precursor particles.
摘要:
A toner including a binder resin which contains a crystalline polyester resin and a non-crystalline polyester resin, wherein the crystalline polyester resin has at least two diffraction peaks in a range of 20°