摘要:
In a welded structure and welded pipe, having members joined to each other by welding wherein, at least one of the members is formed of Fe—Ni-base low thermal expansion coefficient alloy, there is provided a welded structure and welded pipe having a weld metal free from cracking and achieving an excellent toughness and stress corrosion cracking resistance. Further, a welding material is provided which can form such a weld metal and is excellent in workability and weldability in fabrication. The weld metal comprises, on the weight % basis, Ni: 30 to 45%, Co: 0 to 10%, C: 0.03 to 0.5%, Mn: 0.7% or less, either one of or the total of Nb and Zr: 0.05 to 4%, and rare earth element: 0 to 0.5%, with impurities being P: 0.02% or less, Al: 0.01% or less, and oxygen: 0.01% or less, wherein each of Si and S satisfies the following formulas {circle around (1)} and {circle around (2)}, where each element symbol in the following formulas {circle around (1)} and {circle around (2)} indicates the content (weight %) of each element. Si≦0.1(Nb+Zr)+0.05% {circle around (1)} S≦0.0015(Nb+Zr)+0.0055% {circle around (2)}
摘要翻译:在焊接结构和焊接管中,具有通过焊接彼此接合的构件,其中至少一个构件由Fe-Ni基低热膨胀系数合金形成,提供焊接结构和焊接管,其具有焊接 金属无裂纹,具有优异的韧性和应力腐蚀开裂性。 此外,提供了可以形成这种焊接金属的焊接材料,并且加工性和制造中的可焊接性优异。 焊接金属以重量%计含有:Ni:30〜45%,Co:0〜10%,C:0.03〜0.5%,Mn:0.7%以下,Nb和Zr: 0.05〜4%,稀土元素:0〜0.5%,杂质为P:0.02%以下,Al:0.01%以下,氧:0.01%以下,Si和S分别满足下式 {round around(1和{circle around(2,where each element symbol in the following formula {circle around(1 and {circle around(2表示每个元素的含量(重量%))。