Polyolefin
    2.
    发明申请

    公开(公告)号:US20210395411A1

    公开(公告)日:2021-12-23

    申请号:US17282524

    申请日:2019-12-20

    Applicant: LG Chem, Ltd.

    Abstract: The present invention relates to polyolefin. More specifically, the present invention relates to polyolefin having excellent dart drop impact strength, and exhibiting improved transparency, and such polyolefin has a density of 0.915 g/cm3 to 0.930 g/cm3 measured according to ASTM D1505; a nd has an ethylene sequence inhomogeneity(I) calculated by the following Equation 1 of 1.25 to 1.40, when analyzed by SSA(Successive Self-nucleation and Annealing): Inhomogeneity (I)=Lw/Ln   [Equation 1] in the Equation 1, Lw is weighted average(unit: nm) of ESL(Ethylene sequence length), and Ln is arithmetic m ean(unit: nm) of ESL(Ethylene sequence length).

    Polyolefin
    3.
    发明授权

    公开(公告)号:US11542351B2

    公开(公告)日:2023-01-03

    申请号:US17268146

    申请日:2019-12-20

    Applicant: LG Chem, Ltd.

    Abstract: The present invention relates to polyolefin. More specifically, the present invention relates to polyolefin having excellent dart drop impact strength, and exhibiting improved transparency, and such polyolefin has a density of 0.915 g/cm3 to 0.930 g/cm3 measured according to ASTM D1505; and satisfies the following requirements (provided that S1+S2+S3=1), when measuring the relative content of peak area according to melting temperature (Tm) using SSA (Successive Self-nucleation and Annealing) analysis: the content(S1) of peak area at Tm less than 100° C. is 0.33 to 0.35; the content(S2) of peak area at Tm of 100° C. or more and 120° C. or less is 0.52 to 0.56; and the content(S3) of peak area at Tm greater than 120° C. is 0.10 to 0.14.

    Polyolefin
    4.
    发明申请

    公开(公告)号:US20210371558A1

    公开(公告)日:2021-12-02

    申请号:US17278005

    申请日:2019-12-20

    Applicant: LG Chem, Ltd.

    Abstract: The present invention relates to polyolefin. More specifically, the present invention relate s to polyolefin having excellent dart drop impact strength, and exhibiting improved transparency and satisfying one of the following 1)˜4): 1) when density is 0.9165 g/cm3 or more and less than 0.9175 g/cm3, the content of SCB (Short Chain Branch) is 9.5 to 10.5 wt %, 2) when density is 0.9175 g/cm3 or more and less than 0.9185 g/cm3, the content of SCB (Short Chain Branch) is 9.0 to 10.0 wt %, 3) when density is 0.9185 g/cm3 or more and less than 0.9195 g/cm3, the content of SCB (Short Chain Branch) is 8.5 to 9.5 wt %, 4) when density is 0.9195 g/cm3 or more and less than 0.9205 g/cm3, the content of SCB (Short Chain Branch) is 7.5 to 8.5 wt %, wherein the density is measured according to ASTM D1505.

    Polyolefin
    5.
    发明申请

    公开(公告)号:US20210332169A1

    公开(公告)日:2021-10-28

    申请号:US17268146

    申请日:2019-12-20

    Applicant: LG Chem, Ltd.

    Abstract: The present invention relates to polyolefin. More specifically, the present invention relates to polyolefin having excellent dart drop impact strength, and exhibiting improved transparency, and such polyolefin has a density of 0.915 g/cm3 to 0.930 g/cm3 measured according to ASTM D1505; and satisfies the following requirements (provided that S1+S2+S3=1), when measuring the relative content of peak area according to melting temperature (Tm) using SSA (Successive Self-nucleation and Annealing) analysis: the content(S1) of peak area at Tm less than 100° C. is 0.33 to 0.35; the content(S2) of peak area at Tm of 100° C. or more and 120° C. or less is 0.52 to 0.56; and the content(S3) of peak area at Tm greater than 120° C. is 0.10 to 0.14.

    Polyolefin
    6.
    发明授权

    公开(公告)号:US12221498B2

    公开(公告)日:2025-02-11

    申请号:US17282524

    申请日:2019-12-20

    Applicant: LG Chem, Ltd.

    Abstract: The present invention relates to polyolefin. More specifically, the present invention relates to polyolefin having excellent dart drop impact strength, and exhibiting improved transparency, and such polyolefin has a density of 0.915 g/cm3 to 0.930 g/cm3 measured according to ASTM D1505; and has an ethylene sequence inhomogeneity (I) calculated by the following Equation 1 of 1.25 to 1.40, when analyzed by SSA (Successive Self-nucleation and Annealing): Inhomogeneity (I)=Lw/Ln  [Equation 1] in the Equation 1, Lw is weighted average (unit: nm) of ESL (Ethylene sequence length), and Ln is arithmetic mean (unit: nm) of ESL (Ethylene sequence length).

    Polyolefin
    7.
    发明授权

    公开(公告)号:US11987655B2

    公开(公告)日:2024-05-21

    申请号:US17278005

    申请日:2019-12-20

    Applicant: LG Chem, Ltd.

    CPC classification number: C08F210/16 C08F2500/10

    Abstract: The present invention relates to polyolefin. More specifically, the present invention relate s to polyolefin having excellent dart drop impact strength, and exhibiting improved transparency and satisfying one of the following 1)˜4):



    1) when density is 0.9165 g/cm3 or more and less than 0.9175 g/cm3, the content of SCB (Short Chain Branch) is 9.5 to 10.5 wt %,
    2) when density is 0.9175 g/cm3 or more and less than 0.9185 g/cm3, the content of SCB (Short Chain Branch) is 9.0 to 10.0 wt %,
    3) when density is 0.9185 g/cm3 or more and less than 0.9195 g/cm3, the content of SCB (Short Chain Branch) is 8.5 to 9.5 wt %,
    4) when density is 0.9195 g/cm3 or more and less than 0.9205 g/cm3, the content of SCB (Short Chain Branch) is 7.5 to 8.5 wt %,
    wherein the density is measured according to ASTM D1505.

    Polyethylene and Preparation Method Thereof
    8.
    发明公开

    公开(公告)号:US20240026041A1

    公开(公告)日:2024-01-25

    申请号:US18036091

    申请日:2021-11-29

    Applicant: LG Chem, Ltd.

    CPC classification number: C08F10/02

    Abstract: Provided are a polyethylene having excellent processability and capable of reducing an injection molding defect rate, and a method of preparing the same. The polyethylene has an integral value in the region where the Log Mw is 5.5 or more in a GPC curve, wherein the x-axis is log Mw and the y-axis is dw/dlogMw, of 9% or less of the total integral value: and has a ratio (Tc10/Tc40) of a crystallization temperature (Tc10) measured at a cooling rate of 10° C./min to a crystallization temperature (Tc40) measured at a cooling rate of 40° C./min of less than 1.04.