公开(公告)号:US06428932B1
公开(公告)日:2002-08-06
申请号:US09574957
申请日:2000-05-19
申请人: Mitsuo Shinoda , Keiichi Kagawa , Seiji Fuchino , Kouji Morita , Yoshiaki Tanino , Makoto Matsuo , Akira Oyama
发明人: Mitsuo Shinoda , Keiichi Kagawa , Seiji Fuchino , Kouji Morita , Yoshiaki Tanino , Makoto Matsuo , Akira Oyama
IPC分类号: H01M424
CPC分类号: C22C1/04 , B22F2998/00 , H01M4/02 , H01M4/04 , H01M4/0483 , H01M4/244 , H01M4/42 , H01M2004/028 , B22F9/082
摘要: Zinc alloy powder for alkaline batteries containing Bi at a rate of 0.01-0.1% by weight, In at a rate of 0.01-0.1% by weight, Mg at a rate of 0.0005-0.03 % by weight and unavoidable impurities, such as Pb, Cd and Cu, capable of improving high-rate performance and being suitable for using as a cathode active substance for alkaline batteries is provided.
摘要翻译: 含有0.01-0.1重量%Bi的碱性电池的锌合金粉末In以0.01-0.1重量%的比例,以0.0005-0.03重量%的Mg和不可避免的杂质如Pb, 提供能够提高高速率性能并适合用作碱性电池的阴极活性物质的Cd和Cu。
-
公开(公告)号:US06746509B2
公开(公告)日:2004-06-08
申请号:US10238858
申请日:2002-09-11
IPC分类号: B22F908
CPC分类号: B22F9/082 , B22F2009/088 , B22F2009/0892 , B22F2999/00 , H01M4/02 , H01M4/42 , H01M10/24 , B22F2201/02 , B22F2201/11
摘要: A process of producing a zinc or zinc alloy powder (4) for batteries which comprises dropping molten zinc or a molten zinc alloy to form a molten metal droplets stream (1) and striking an atomizing medium jet (3) emitted from a nozzle (2) against the molten metal stream (1) at right angles to atomize the molten zinc or the molten zinc alloy, wherein two or more the nozzles are arranged in parallel to each other, the orifice of each of the nozzles has a V-shaped, U-shaped, X-shaped or arc-shaped cross-section, the atomizing medium is air or an inert gas, two or more the molten metal streams have at least two different flow rates selected from a range 0.04 to 0.25 kg/sec, and two or more the atomizing medium jets have at least two different atomizing pressures selected from a range 4 to 9 kg/cm2.
摘要翻译: 一种生产用于电池的锌或锌合金粉末(4)的方法,包括滴加熔融锌或熔融锌合金以形成熔融金属液滴流(1)并且撞击从喷嘴(2)发射的雾化介质射流 )对熔融金属流(1)成直角,以雾化熔融锌或熔融锌合金,其中两个或更多个喷嘴彼此平行地布置,每个喷嘴的孔具有V形, U形,X形或弧形横截面,雾化介质是空气或惰性气体,两个或更多个熔融金属流具有选自0.04至0.25kg / sec的至少两种不同流速, 并且两个或更多个雾化介质射流具有选自4至9kg / cm 2的至少两种不同的雾化压力。
-