公开(公告)号:US20210025021A1
公开(公告)日:2021-01-28
申请号:US16981435
申请日:2019-03-26
Applicant: NIPPON STEEL CORPORATION
Inventor: Hiroki KAMITANI , Takanori TANAKA , Atsushi SOMA , Keiichi KONDO , Hideki MITSUNARI , Seiya OKADA , Takuya MATSUMOTO , Shinji YOSHIDA , Yuji ARAI
Abstract: A seamless steel pipe heat-treatment-finishing-treatment continuous facility includes: a heat treatment apparatus; a steel pipe inspection apparatus which performs a test for a surface defect and/or an inner defect of the seamless steel pipe, the steel pipe inspection apparatus being disposed downstream of the heat treatment apparatus; a main transfer mechanism which forms a main transfer path MT for transferring the seamless steel pipe, discharged from the heat treatment apparatus, to the steel pipe inspection apparatus disposed downstream of the heat treatment apparatus; and a first forced steel pipe-temperature reduction apparatus which forcibly reduces a temperature of the seamless steel pipe on the main transfer path MT, the first forced steel pipe-temperature reduction apparatus being disposed on the main transfer path MT at a position downstream of the heat treatment apparatus and upstream of the steel pipe inspection apparatus.
-
公开(公告)号:US20210017635A1
公开(公告)日:2021-01-21
申请号:US16980671
申请日:2019-03-25
Applicant: NIPPON STEEL CORPORATION
Inventor: Hiroki KAMITANI , Atsushi SOMA , Shinji YOSHIDA , Yuji ARAI , Seiya OKADA
IPC: C22C38/54 , C22C38/52 , C22C38/50 , C22C38/48 , C22C38/46 , C22C38/42 , C22C38/22 , C22C38/06 , C22C38/04 , C22C38/02 , C22C38/00
Abstract: The steel material according to the present disclosure contains a chemical composition consisting of, in mass %, C: 0.20 to 0.50%, Si: 0.05 to 0.50%, Mn: 0.05 to 1.00%, P: 0.030% or less, S: 0.0100% or less, Al: 0.005 to 0.100%, Cr: 0.10 to 1.50%, Mo: 0.25 to 1.50%, Ti: 0.002 to 0.050%, N: 0.0100% or less and O: 0.0100% or less, with the balance being Fe and impurities. The steel material contains an amount of dissolved C within a range of 0.010 to 0.050 mass %. The steel material also has a yield strength within a range of 655 to less than 862 MPa, and a yield ratio of the steel material is 85% or more.
-
公开(公告)号:US20210180149A1
公开(公告)日:2021-06-17
申请号:US17044601
申请日:2019-03-22
Applicant: NIPPON STEEL CORPORATION
Inventor: Yuji ARAI , Shinji YOSHIDA , Atsushi SOMA , Hiroki KAMITANI
IPC: C21D9/08 , C22C38/54 , C22C38/50 , C22C38/48 , C22C38/46 , C22C38/44 , C22C38/42 , C22C38/30 , C22C38/06 , C22C38/04 , C22C38/02 , C22C38/00 , C21D8/10 , C21D6/00
Abstract: The steel pipe according to the present disclosure contains a chemical composition consisting of, in mass %, C: 0.25 to 0.50%, Si: 0.05 to 0.50%, Mn: 0.05 to 1.00%, P: 0.025% or less, S: 0.0050% or less, Al: 0.005 to 0.100%, Cr: 0.30 to 1.50%, Mo: 0.25 to 3.00%, Ti: 0.002 to 0.050%, N: 0.0010 to 0.0100% and O: 0.0030% or less, with the balance being Fe and impurities. The steel pipe contains an amount of dissolved C within a range of 0.010 to 0.050 mass %. The tensile yield strength in the axial direction and the circumferential direction is 862 to 965 MPa, and the yield ratio in the axial direction is 90% or more. The tensile yield strength in the circumferential direction is 30 to 80 MPa higher than the compressive yield strength in the circumferential direction.
-
公开(公告)号:US20210032734A1
公开(公告)日:2021-02-04
申请号:US17043306
申请日:2019-03-22
Applicant: NIPPON STEEL CORPORATION
Inventor: Yuji ARAI , Shinji YOSHIDA , Atsushi SOMA , Hiroki KAMITANI
IPC: C22C38/54 , C21D8/10 , C21D9/08 , C22C38/42 , C22C38/44 , C22C38/50 , C22C38/46 , C22C38/48 , C22C38/52 , C22C38/00 , C22C38/06 , C22C38/02 , C22C38/04
Abstract: The steel pipe according to the present disclosure contains a chemical composition consisting of, in mass %, C: more than 0.50 to 0.65%, Si: 0.05 to 0.50%, Mn: 0.05 to 1.00%, P: 0.025% or less, S: 0.0050% or less, Al: 0.005 to 0.100%, Cr: 0.30 to 1.50%, Mo: 0.25 to 3.00%, Ti: 0.002 to 0.050%, N: 0.0010 to 0.0100% and O: 0.0030% or less, with the balance being Fe and impurities. The steel pipe contains an amount of dissolved C within a range of 0.010 to 0.060 mass %. The tensile yield strength in the axial direction and the circumferential direction is 862 to 1069 MPa, and the yield ratio in the axial direction is 90% or more. The tensile yield strength in the circumferential direction is 30 to 80 MPa higher than the compressive yield strength in the circumferential direction.
-
公开(公告)号:US20220098712A1
公开(公告)日:2022-03-31
申请号:US17422870
申请日:2020-02-13
Applicant: NIPPON STEEL CORPORATION
Inventor: Hiroki KAMITANI , Yohei OTOME , Atsushi SOMA , Taro OE , Nobuaki KOMATSUBARA , Shinji YOSHIDA , Yuji ARAI
IPC: C22C38/54 , C22C38/50 , C22C38/48 , C22C38/46 , C22C38/44 , C22C38/30 , C22C38/20 , C22C38/06 , C22C38/04 , C22C38/02 , C22C38/00
Abstract: A steel material according to the present disclosure has a chemical composition consisting of, in mass %: C: 0.20 to 0.45%, Si: 0.05 to 1.00%, Mn: 0.01 to 1.00%, P: 0.030% or less, S: 0.0050% or less, Al: 0.005 to 0.100%, Cr: 0.60 to 1.50%, Mo: more than 1.00 to 2.00%, Ti: 0.002 to 0.020%, V: 0.05 to 0.30%, Nb: 0.005 to 0.100%, B: 0.0005 to 0.0040%, N: 0.0100% or less, O: less than 0.0020%, and the balance being Fe and impurities, and satisfying Formula (1) described in the specification. A grain diameter of a prior-austenite grain is 11.0 μm or less, and an average area of precipitate which is precipitated in a prior-austenite grain boundary is 10.0×10−3 μm2 or less. A yield strength is 758 to 862 MPa.
-
公开(公告)号:US20210317553A1
公开(公告)日:2021-10-14
申请号:US17259651
申请日:2019-09-26
Applicant: NIPPON STEEL CORPORATION
Inventor: Hiroki KAMITANI , Nobuaki KOMATSUBARA , Seiya OKADA , Atsushi SOMA , Yuji ARAI , Shinji YOSHIDA
Abstract: The seamless steel pipe according to the present disclosure has a chemical composition consisting of, in mass %, C: 0.15 to 0.45%, Si: 0.05 to 1.00%, Mn: 0.01 to 1.00%, P: 0.030% or less, S: 0.0050% or less, Al: 0.005 to 0.070%, Cr: 0.30 to 1.50%, Mo: 0.25 to 2.00%, Ti: 0.002 to 0.020%, Nb: 0.002 to 0.100%, B: 0.0005 to 0.0040%, rare earth metal: 0.0001 to 0.0015%, Ca: 0.0001 to 0.0100%, N: 0.0100% or less and O: 0.0020% or less, with the balance being Fe and impurities, and satisfying Formula (1) described in the description. A predicted maximum major axis of inclusions is 150 μm or less, the predicted maximum major axis being predicted by means of extreme value statistical processing. The yield strength is within a range of 758 to 862 MPa.
-
公开(公告)号:US20210198775A1
公开(公告)日:2021-07-01
申请号:US17044616
申请日:2019-03-22
Applicant: NIPPON STEEL CORPORATION
Inventor: Hiroki KAMITANI , Atsushi SOMA , Keiichi KONDO , Shinji YOSHIDA , Yuji ARAI
Abstract: The steel material according to the present disclosure contains a chemical composition consisting of, in mass %, C: 0.20 to 0.50%, Si: 0.05 to 0.50%, Mn: 0.05 to 1.00%, P: 0.030% or less, S: less than 0.0050%, Al: 0.005 to 0.050%, Cr: 0.10 to 1.50%, Mo: 0.25 to 1.80%, Ti: 0.002 to 0.050%, Nb: 0.002 to 0.100%, B: 0.0001 to 0.0050%, N: 0.0070% or less and O: less than 0.0050% with the balance being Fe and impurities. A yield strength is within a range of 655 to 1069 MPa, and a yield ratio is 85% or more. A proportion of KAM values of 1° or less is 30 area % or more.
-
公开(公告)号:US20210047714A1
公开(公告)日:2021-02-18
申请号:US17043096
申请日:2019-03-22
Applicant: NIPPON STEEL CORPORATION
Inventor: Shinji YOSHIDA , Yuji ARAI , Atsushi SOMA , Hiroki KAMITANI
IPC: C22C38/32 , C22C38/20 , C22C38/30 , C22C38/28 , C22C38/26 , C22C38/22 , C22C38/06 , C22C38/04 , C22C38/02 , C22C38/00 , C22C38/24 , C21D9/46 , C21D8/02 , C21D6/00 , C21D1/18
Abstract: The steel material according to the present disclosure contains a chemical composition consisting of, in mass %, C: more than 0.50 to 0.80%, Si: 0.05 to 1.00%, Mn: 0.05 to 1.00%, P: 0.025% or less, S: 0.0100% or less, Al: 0.005 to 0.100%, Cr: 0.20 to 1.50%, Mo: 0.25 to 1.50%, Ti: 0.002 to 0.050%, B: 0.0001 to 0.0050%, N: 0.0100% or less and O: 0.0100% or less, with the balance being Fe and impurities. The steel material contains an amount of dissolved C within a range of 0.010 to 0.060 mass %. The steel material also has a yield strength within a range of 862 to less than 965 MPa, and a yield ratio of the steel material is 90% or more.
-
公开(公告)号:US20210010099A1
公开(公告)日:2021-01-14
申请号:US16977881
申请日:2019-03-22
Applicant: NIPPON STEEL CORPORATION
Inventor: Shinji YOSHIDA , Yuji ARAI , Atsushi SOMA , Hiroki KAMITANI
IPC: C21D9/46 , C22C38/50 , C22C38/44 , C22C38/54 , C22C38/30 , C22C38/26 , C22C38/24 , C22C38/20 , C22C38/06 , C22C38/04 , C22C38/02 , C22C38/00 , C21D8/02 , C21D6/00
Abstract: The steel material according to the present disclosure contains a chemical composition consisting of, in mass %, C: 0.20 to 0.50%, Si: 0.05 to 1.00%, Mn: 0.05 to 1.00%, P: 0.025% or less, S: 0.0100% or less, Al: 0.005 to 0.100%, Cr: 0.20 to 1.50%, Mo: 0.25 to 1.50%, Ti: 0.002 to 0.050%, B: 0.0001 to 0.0050%, N: 0.0100% or less and O: 0.0100% or less, with the balance being Fe and impurities. The steel material contains an amount of dissolved C within a range of 0.010 to 0.050 mass %. The steel material also has a yield strength within a range of 965 to 1069 MPa, and a yield ratio of the steel material is 90% or more.
-
-
-
-
-
-
-
-