公开(公告)号:US20220098712A1
公开(公告)日:2022-03-31
申请号:US17422870
申请日:2020-02-13
Applicant: NIPPON STEEL CORPORATION
Inventor: Hiroki KAMITANI , Yohei OTOME , Atsushi SOMA , Taro OE , Nobuaki KOMATSUBARA , Shinji YOSHIDA , Yuji ARAI
IPC: C22C38/54 , C22C38/50 , C22C38/48 , C22C38/46 , C22C38/44 , C22C38/30 , C22C38/20 , C22C38/06 , C22C38/04 , C22C38/02 , C22C38/00
Abstract: A steel material according to the present disclosure has a chemical composition consisting of, in mass %: C: 0.20 to 0.45%, Si: 0.05 to 1.00%, Mn: 0.01 to 1.00%, P: 0.030% or less, S: 0.0050% or less, Al: 0.005 to 0.100%, Cr: 0.60 to 1.50%, Mo: more than 1.00 to 2.00%, Ti: 0.002 to 0.020%, V: 0.05 to 0.30%, Nb: 0.005 to 0.100%, B: 0.0005 to 0.0040%, N: 0.0100% or less, O: less than 0.0020%, and the balance being Fe and impurities, and satisfying Formula (1) described in the specification. A grain diameter of a prior-austenite grain is 11.0 μm or less, and an average area of precipitate which is precipitated in a prior-austenite grain boundary is 10.0×10−3 μm2 or less. A yield strength is 758 to 862 MPa.
-
公开(公告)号:US20230203631A1
公开(公告)日:2023-06-29
申请号:US17995368
申请日:2021-04-15
Applicant: NIPPON STEEL CORPORATION
Inventor: Keiichi KONDO , Yuji ARAI , Keiichi NAKAMURA , Taro OE , Takenori KURAMOTO , Yosuke TAKEDA , Hiroki KAMITANI
IPC: C22C38/54 , C22C38/02 , C22C38/04 , C22C38/06 , C22C38/00 , C22C38/42 , C22C38/44 , C22C38/46 , C22C38/48 , C22C38/50 , C21D9/08
CPC classification number: C22C38/54 , C21D9/08 , C22C38/001 , C22C38/02 , C22C38/002 , C22C38/04 , C22C38/005 , C22C38/06 , C22C38/42 , C22C38/44 , C22C38/46 , C22C38/48 , C22C38/50 , C21D2211/001
Abstract: The steel material according to the present disclosure consists of, in mass%, C: 0.15 to 0.45%, Si: 0.05 to 1.00%, Mn: 0.05 to less than 0.80%, P: 0.030% or less, S: 0.0100% or less, Al: 0.100% or less, Cr: 0.30 to 1.50%, Mo: 0.25 to 2.00%, Ti: 0.001 to 0.015%, N: 0.0100% or less, O: 0.0050% or less, V: 0 to 0.05%, Nb: 0 to 0.010%, B: 0 to less than 0.0005%, Ca: 0 to 0.0100%, Mg: 0 to 0.0100%, and rare earth metal: 0 to 0.0100%, with the balance being Fe and impurities. In the steel material, the grain size number of prior-austenite grains is less than 7.0, Formula (1) to Formula (4) described in the specification are satisfied, the yield strength is 896 MPa or more, and the absorbed energy at -10° C. is 95 J or more.
-