Lithium primary cell with a positive electrode including manganese dioxide and a boron compound

    公开(公告)号:US12266827B2

    公开(公告)日:2025-04-01

    申请号:US17261111

    申请日:2019-04-02

    Abstract: A lithium primary cell includes an electrode group and a non-aqueous electrolytic solution. The electrode group includes a positive electrode, a negative electrode, and a separator, in which the positive electrode and the negative electrode are wound with the separator interposed therebetween. In the electrode group, an area where the positive electrode and the negative electrode face each other is 250 cm2 or more and 350 cm2 or less. The positive electrode includes a positive electrode mixture including manganese dioxide and a boron compound. The negative electrode includes lithium metal or a lithium alloy. The non-aqueous electrolytic solution includes ethylene carbonate. A content of the boron compound in the positive electrode is 0.5 parts by mass or more and 2 parts by mass or less in terms of boron with respect to 100 parts by mass of the positive electrode mixture. A content of the ethylene carbonate in the non-aqueous electrolytic solution is 1 part by mass or more and 10 parts by mass or less with respect to 100 parts by mass of the manganese dioxide.

    Positive electrode for alkaline storage batteries and alkaline storage battery

    公开(公告)号:US10128492B2

    公开(公告)日:2018-11-13

    申请号:US15033056

    申请日:2014-12-04

    Abstract: A positive electrode for alkaline storage batteries that enables to improve the active material utilization rate, while suppressing the self-discharge. The positive electrode for alkaline storage batteries includes a support having conductivity, and a positive electrode active material adhering to the support. The positive electrode active material includes particles of a nickel oxide. The particles of the nickel oxide include a first particle group having a particle diameter of 20 μm or more, and a second particle group having a particle diameter of less than 20 μm. The first particle group includes a first component with cracks, and a second component without cracks. The proportion of the first particle group in the particles of the nickel oxide is 15 vol % or more, and the proportion by number of the first component in the first particle group is 15% or more.

Patent Agency Ranking