摘要:
A paper product having increased thickness, absorbency, and softness without altering product strength wherein a fiber blend is provided being up to 50% softwood fibers and up to 100% Hesperaloe funifera fibers.
摘要:
A substrate treated with a lotion including a skin pH balancing compound and a base lotion. The pH balancing compound is preferably an organic acid, such as an alpha-hydroxy acid, an alpha-dihydroxy acid, or a beta-hydroxyacid, a combination of an organic acid and a salt of an organic acid, or a buffer combination, such as combinations of citric acid and disodium phosphate, or disodium citrate and sodium hydroxide. The preferred lotion has the effect of maintaining the skin acid mantle while making the treated substrate, preferably tissue, towel or napkin, optionally wet-strengthened, wipe or nonwoven material, feel smooth, lubricious and nongreasy. The skin care benefits of the lotionized substrate are expressed whether the product is used dry or prewetted with water.
摘要:
A one-ply paper tissue product and a method of making a one-ply paper product combining high strength and softness along with low sidedness. The paper tissue product exhibits a sidedness parameter of less than 0.3 preferably, less than 0.225, a tensile modulus of no more than 32 grams/percent strain, a GM MMD of no more than about 0.225, and a cross directional strength of at least 200 grams per 3 inches. In stratification tissues, these properties are obtained by control of stratification, particularly, chemical stratification and stratification of furnish when appropriate. The tissue has a sidedness parameter value of less than 0.3, preferably, about 0.15 to about less than 0.225. In homogenous tissue, these properties are obtained by adding a strength enhancing agent to separate furnish sources prior to the funish sources being combined, and further, optionally adding the softener to the nascent web.
摘要:
The present invention relates to a soft, thick, single-ply tissue having a serpentine configuration and to a process for the manufacture of such tissue product having a basis weight of at least about 15 lbs./3,000 square foot ream and having low sidedness, said tissue exhibiting: a specific total tensile strength of between 40 and 75 grams per 3 inches per pound per 3000 square feet ream, a cross direction specific wet tensile strength of between 2.75 and 7.5 grams per 3 inches per pound per 3000 square feet ream, the ratio of MD tensile to CD tensile of between 1.25 and 2.75, a specific geometric mean tensile stiffness of between 0.5 and 1.2 grams per inch per percent strain per pound per 3000 square feet ream, a friction deviation of less than 0.225, and a sidedness parameter of less than 0.275.
摘要:
A tissue paper of improved softness, strength and absorbency; and a manufacturing process for such a tissue paper where the generation of foam is reduced, or eliminated altogether. These are obtained using a tissue paper softener system comprising a substantially equimolar, ion-paired mixture of an anionic surfactant and a cationic quaternary ammonium compound, wherein the softener system is formulated such that the charge density of the anionic surfactant/cationic quaternary ammonium compound mixture will be about neutral.
摘要:
The present invention relates to a soft, thick, single-ply tissue and to a process for the manufacture of such tissue product having a basis weight of at least about 15 lbs./3,000 square foot ream and having low sidedness, said tissue exhibiting:a specific total tensile strength of between 40 and 75 grams per 3 inches per pound per 3000 square feet ream, a cross direction specific wet tensile strength of between 2.75 and 7.5 grams per 3 inches per pound per 3000 square feet ream, the ratio of MD tensile to CD tensile of between 1.25 and 2.75, a specific geometric mean tensile stiffness of between 0.5 and 1.2 grams per inch per percent strain per pound per 3000 square feet ream, a friction deviation of less than 0.225, and a sidedness parameter of less than 0.275.
摘要:
A substrate treated with a lotion including an emollient and a retention/release agent, wherein the lotion has at least one of: (a) a .DELTA.H above about 37.degree. C. of above about 10 calories/gram (and optionally, a .DELTA.H below about 37.degree. C. of above about 15 calories/gram), a total heat of melting of above about 25 calories/gram, preferably above about 30 calories/gram, and an onset of melting temperature of at least about 30.degree. C., preferably from about 30.degree. C. to about 45.degree. C.; and (b) a .DELTA.H above about 30.degree. C. of above about 15 calories/gram (and optionally, a .DELTA.H below about 30.degree. C. of above about 10 calories/gram), a total heat of melting of above about 25 calories/gram, preferably above about 30 calories/gram, and an onset of melting temperature of at least about 30.degree. C., preferably from about 30.degree. C. to about 45.degree. C. is disclosed. Preferably the lotion includes an aromatic ester or fatty alcohol ester of a non-fatty organic acid emollient or mixture thereof and a retention/release agent, and optionally, surfactant, and/or medicinal agent. The lotion has the effect of making the treated substrate, preferably tissue, towel or napkin, optionally wet-strengthened, wipe or nonwoven material, feel smooth, lubricious and nongreasy. The skin care benefits of the lotionized substrate are expressed whether the product is used dry or prewetted with water.
摘要:
A one-ply paper tissue product and a method of making a one-ply paper product combining high strength and softness along with low sidedness. The paper tissue product exhibits a sidedness parameter of less than 0.3 preferably, less than 0.225, a tensile modulus of no more than 32 grams/percent strain, a GM MMD of no more than about 0.225, and a cross directional strength of at least 200 grams per 3 inches. In stratification tissues, these properties are obtained by control of stratification, particularly, chemical stratification and stratification of furnish when appropriate. The tissue has a sidedness parameter value of less than 0.3, preferably, about 0.15 to about less than 0.225. In homogenous tissue, these properties are obtained by adding a strength enhancing agent to separate furnish sources prior to the funish sources being combined, and further, optionally adding the softener to the nascent web.
摘要:
The present invention relates to a soft, thick, single-ply tissue and to a process for the manufacture of such tissue product having a basis weight of at least about 15 lbs./3,000 square foot ream and having low sidedness, said tissue exhibiting:a specific total tensile strength of between 40 and 75 grams per 3 inches per pound per 3000 square feet ream, a cross direction specific wet tensile strength of between 2.75 and 7.5 grams per 3 inches per pound per 3000 square feet ream, the ratio of MD tensile to CD tensile of between 1.25 and 2.75, a specific geometric mean tensile stiffness of between 0.5 and 1.2 grams per inch per percent strain per pound per 3000 square feet ream, a friction deviation of less than 0.225, and a sidedness parameter of less than 0.275.
摘要:
The present invention relates to a soft, thick, single-ply tissue having a serpentine configuration and to a process for the manufacture of such tissue product having a basis weight of at least about 15 lbs. per 3000 square foot ream and having low sidedness, said tissue exhibiting: a specific total tensile strength of between 40 and 200 grams per 3 inches per pound per 3000 square foot ream, a cross direction specific wet tensile strength of between 2.75 and 20.0 grams per 3 inches per pound per 3000 square foot ream, the ratio of MD tensile to CD tensile of between 1.25 and 2.75, a specific geometric mean tensile stiffness of between 0.5 and 3.2 grams per inch per percent strain per pound per 3000 square foot ream, a friction deviation of less than 0.250, and a sidedness parameter of less than 0.30.