HETEROPHASIC PROPYLENE COPOLYMER
    1.
    发明申请

    公开(公告)号:US20200062942A1

    公开(公告)日:2020-02-27

    申请号:US16467717

    申请日:2017-12-12

    Abstract: The invention relates to a process for the preparation of a final heterophasic propylene copolymer (A) having a final melt flow rate in the range from 65 to 110 dg/min, comprising visbreaking an intermediate heterophasic propylene copolymer (A′) having an intermediate melt flow rate, which intermediate melt flow rate is lower than the final melt flow rate, to obtain the final heterophasic propylene copolymer,wherein the intermediate heterophasic propylene copolymer (A′) consists of (a) a propylene-based matrix, (b) a dispersed ethylene-α-olefin copolymer, wherein the sum of the total amount of propylene-based matrix and total amount of the dispersed ethylene-α-olefin copolymer in the intermediate heterophasic propylene copolymer is 100 wt % based on the intermediate heterophasic propylene copolymer.

    Composition comprising heterophasic propylene copolymer

    公开(公告)号:US11603453B2

    公开(公告)日:2023-03-14

    申请号:US16467708

    申请日:2017-12-12

    Abstract: The invention relates to a composition comprising a heterophasic propylene copolymer (A), glass fibers (B) and an ethylene-α-olefin copolymer (C), wherein the α-olefin is chosen from the group of α-olefins having 3 to 12 carbon atoms. The heterophasic propylene copolymer (A) consists of (a) a propylene-based matrix, consisting of a propylene homopolymer and/or a propylene-α-olefin copolymer consisting of at least 85 wt % of propylene and at most 15 wt % of α-olefin, and (b) a dispersed ethylene-α-olefin copolymer, wherein the heterophasic propylene copolymer has a flexural modulus of less than 1000 MPa, wherein the dispersed ethylene α-olefin copolymer (b) has an average rubber particle size d50 of at most 1.15 μm as determined by scanning electron microscopy, and wherein the total amount of (b) the dispersed ethylene-α-olefin copolymer in the heterophasic propylene copolymer (A) and the ethylene-α-olefin copolymer (C) is 30 to 60 wt % based on the total composition.

    Heterophasic propylene copolymer
    6.
    发明授权

    公开(公告)号:US11149139B2

    公开(公告)日:2021-10-19

    申请号:US16467717

    申请日:2017-12-12

    Abstract: The invention relates to a process for the preparation of a final heterophasic propylene copolymer (A) having a final melt flow rate in the range from 65 to 110 dg/min, comprising visbreaking an intermediate heterophasic propylene copolymer (A′) having an intermediate melt flow rate, which intermediate melt flow rate is lower than the final melt flow rate, to obtain the final heterophasic propylene copolymer,
    wherein the intermediate heterophasic propylene copolymer (A′) consists of
    (a) a propylene-based matrix,
    (b) a dispersed ethylene-α-olefin copolymer,
    wherein the sum of the total amount of propylene-based matrix and total amount of the dispersed ethylene-α-olefin copolymer in the intermediate heterophasic propylene copolymer is 100 wt % based on the intermediate heterophasic propylene copolymer.

    COMPOSITION COMPRISING HETEROPHASIC PROPYLENE COPOLYMER

    公开(公告)号:US20200002518A1

    公开(公告)日:2020-01-02

    申请号:US16467708

    申请日:2017-12-12

    Abstract: The invention relates to a composition comprising a heterophasic propylene copolymer (A), glass fibers (B) and an ethylene-α-olefin copolymer (C), wherein the α-olefin is chosen from the group of α-olefins having 3 to 12 carbon atoms. The heterophasic propylene copolymer (A) consists of (a) a propylene-based matrix, consisting of a propylene homopolymer and/or a propylene-α-olefin copolymer consisting of at least 85 wt % of propylene and at most 15 wt % of α-olefin, and (b) a dispersed ethylene-α-olefin copolymer, wherein the heterophasic propylene copolymer has a flexural modulus of less than 1000 MPa, wherein the dispersed ethylene α-olefin copolymer (b) has an average rubber particle size d50 of at most 1.15 μm as determined by scanning electron microscopy, and wherein the total amount of (b) the dispersed ethylene-α-olefin copolymer in the heterophasic propylene copolymer (A) and the ethylene-α-olefin copolymer (C) is 30 to 60 wt % based on the total composition.

    PROCESS FOR MANUFACTURE OF LOW EMISSION HETEROPHASIC POLYPROPYLENE

    公开(公告)号:US20190330386A1

    公开(公告)日:2019-10-31

    申请号:US16468091

    申请日:2017-12-12

    Abstract: The invention relates to a process for the preparation of a heterophasic propylene copolymer consisting of a propylene-based matrix and a dispersed ethylene-α-olefin copolymer, comprising the steps of a) preparing the propylene-based matrix from propylene and optionally a C2 or C4-C12 α-olefin by contacting at least propylene and optionally C2 or C4-C12 α-olefin with a catalyst in a first gas-phase reactor at a temperature T1 and a pressure P1, b) subsequently preparing the dispersed ethylene-α-olefin copolymer from ethylene and a C3-C12 α-olefin by contacting the ethylene and the C3-C12 α-olefin with a catalyst in a second gas-phase reactor at a temperature T2 and a pressure P2, wherein T1−T2 is in the range from 6 to 25° C., wherein T1>T2, wherein P1 and P2 are in the range from 22 to 30 bar to prepare a heterophasic propylene copolymer (A′).