Abstract:
A sintered body for use as a liquid reservoir in an electronic cigarette, medication administering devices, in thermally heated evaporators for fragrant substances is provided. The sintered body is made of open-pore sintered glass and has a porosity of greater than 50 vol %. The average pore size is in a range from 1 to 450 μm. The glass of the sintered body has a transition temperature Tg of at least 450° C.
Abstract:
A sintered body for use as a liquid reservoir in an electronic cigarette, medication administering devices, in thermally heated evaporators for fragrant substances is provided. The sintered body is made of open-pore sintered glass and has a porosity of greater than 50 vol %. The average pore size is in a range from 1 to 450 μm. The glass of the sintered body has a transition temperature Tg of at least 450° C.
Abstract:
Methods for producing glass articles from glass melts are provided that include continuously introducing the glass melt into a stirrer vessel, stirring the glass melt in the stirrer vessel by at least one blade stirrer, continuously discharging the glass melt from the stirrer vessel, and shaping the glass melt to obtain the glass article. In some embodiments, the stirring is sufficient to draw the glass melt located at a surface of the stirrer vessel into the stirrer vessel so that a formation of a surface layer of the glass melt with a different composition from the composition of the glass melt introduced is prevented or at least minimized. In other embodiments, the stirring is sufficient so that the glass melt which is located at a surface in the stirrer vessel is not drawn into the stirrer vessel or is drawn in only insubstantially.