公开(公告)号:US20170072458A1
公开(公告)日:2017-03-16
申请号:US15125491
申请日:2015-03-23
发明人: Akira YOSHIKAWA , Yuui YOKOTA , Muneki NAKAMURA , Kunihiro TANAKA , Tatsuya NAKAZAWA , Koichi SAKAIRI
CPC分类号: B22D11/005 , B22D11/00 , B22D11/001 , B22D11/11 , B22D21/005 , C22C1/02 , C22C5/04 , C22F1/18 , C30B15/08 , C30B29/02 , C30B29/52
摘要: The present invention provides a metal wire rod composed of iridium or an iridium alloy, wherein the number of crystal grains on any cross-section in a longitudinal direction is 2 to 20 per 0.25 mm2, and the Vickers hardness at any part is 200 Hv or more and less than 400 Hv. The iridium wire rod is a material which is produced by a μ-PD method, and has low residual stress and which has a small change in the number of crystal grains and hardness even when heated to a temperature equal to or higher than a recrystallization temperature (1200° C. to 1500° C.). The metal wire rod of the present invention is excellent in oxidative consumption resistance under a high-temperature atmosphere, and mechanical properties.
摘要翻译: 本发明提供一种由铱或铱合金构成的金属线材,其中纵向方向的任何截面上的晶粒数为2〜20 / 0.25mm 2,任何部分的维氏硬度为200Hv或 多于400 Hv。 铱线棒是通过μ-PD法制造的材料,残留应力低,即使在加热到再结晶温度以上的温度下,晶粒数和硬度也有小的变化 (1200℃〜1500℃)。 本发明的金属线棒在高温环境下的耐氧化消耗性优异,机械性能优良。