公开(公告)号:US20190316229A1
公开(公告)日:2019-10-17
申请号:US16471141
申请日:2017-12-05
发明人: Kiyohito ISHIDA , Toshihiro OMORI , Yutaka SATO , Koichi SAKAIRI , Kunihiro TANAKA , Tatsuya NAKAZAWA
摘要: The present invention relates to a Ni-based heat-resistant alloy including Ir: 5.0 mass % or more and 50.0 mass % or less, Al: 1.0 mass % or more and 8.0 mass % or less, W: 5.0 mass % or more and 25.0 mass % or less, and balance Ni, having an L12-structured γ′ phase present in the matrix, and including at least one of Zr: 0.01 mass % or more and 3.0 mase/0 or less and Hf: 0.01 mass % or more and 3.0 mass % or less. This Ni-based heat-resistant alloy has improved toughness over a conventional Ni-based heat-resistant alloy based on a Ni—Ir—Al—W-based alloy, and is also excellent in ambient-temperature strength.
-
公开(公告)号:US20160040276A1
公开(公告)日:2016-02-11
申请号:US14774223
申请日:2014-03-11
发明人: Kiyohito ISHIDA , Toshihiro OMORI , Yutaka SATO , Kunihiro TANAKA , Muneki NAKAMURA , Koichi SAKAIRI
摘要: The present invention is a heat-resistant Ni-base alloy including a Ni—Ir—Al—W alloy having essential additive elements of Ir, Al, and W added to Ni, wherein the heat-resistant Ni-base alloy includes Ir: 5.0 to 50.0 mass %, Al: 1.0 to 8.0 mass %, and W: 5.0 to 20.0 mass %, the balance being Ni, and a γ′ phase having an L12 structure disperses in a matrix as an essential strengthening phase. The heat-resistant material including the Ni-base alloy may contain one or more additive elements selected from B: 0.001 to 0.1 mass %, Co: 5.0 to 20.0 mass %, Cr: 1.0 to 25.0 mass %, Ta: 1.0 to 10.0 mass %, Nb: 1.0 to 5.0 mass %, Ti: 1.0 to 5.0 mass %, V: 1.0 to 5.0 mass %, and Mo: 1.0 to 5.0 mass %, or 0.001 to 0.5 mass % of C.
摘要翻译: 本发明是一种耐Ni基合金,其中Ni-Ir-Al-W合金具有添加到Ni中的Ir,Al和W的重要添加元素,其中耐热Ni基合金包括Ir:5.0 至50.0质量%,Al:1.0〜8.0质量%,W:5.0〜20.0质量%,余量为Ni,具有L12结构的γ'相分散在基质中作为必需的强化相。 包含Ni基合金的耐热材料可以含有选自B:0.001〜0.1质量%,Co:5.0〜20.0质量%,Cr:1.0〜25.0质量%,Ta:1.0〜10.0质量% %,Nb:1.0〜5.0质量%,Ti:1.0〜5.0质量%,V:1.0〜5.0质量%,Mo:1.0〜5.0质量%,或0.001〜0.5质量%。
-
公开(公告)号:US20190338398A1
公开(公告)日:2019-11-07
申请号:US16469083
申请日:2017-12-04
发明人: Kiyohito ISHIDA , Toshihiro OMORI , Yutaka SATO , Koichi SAKAIRI , Kunihiro TANAKA , Tatsuya NAKAZAWA
IPC分类号: C22C19/05
摘要: The present invention relates to a Ni-based heat-resistant alloy including Ir: 5.0 mass % or more and 50.0 mass % or less, Al: 1.0 mass % or more and 8.0 mass % or less, W: 5.0 mass % or more and 25.0 mass % or less, and balance Ni, having an L12-structured γ′ phase present in the matrix, and including at least one of Ru: 0.8 mass % or more and 5.0 mass % or less and Re: 0.8 mass % or more and 5.0 mass % or less. This Ni-based heat-resistant alloy has improved toughness over a conventional Ni-based heat-resistant alloy based on a Ni—Ir—Al—W-based alloy, and is also excellent in ambient-temperature strength.
-
公开(公告)号:US20170072458A1
公开(公告)日:2017-03-16
申请号:US15125491
申请日:2015-03-23
发明人: Akira YOSHIKAWA , Yuui YOKOTA , Muneki NAKAMURA , Kunihiro TANAKA , Tatsuya NAKAZAWA , Koichi SAKAIRI
CPC分类号: B22D11/005 , B22D11/00 , B22D11/001 , B22D11/11 , B22D21/005 , C22C1/02 , C22C5/04 , C22F1/18 , C30B15/08 , C30B29/02 , C30B29/52
摘要: The present invention provides a metal wire rod composed of iridium or an iridium alloy, wherein the number of crystal grains on any cross-section in a longitudinal direction is 2 to 20 per 0.25 mm2, and the Vickers hardness at any part is 200 Hv or more and less than 400 Hv. The iridium wire rod is a material which is produced by a μ-PD method, and has low residual stress and which has a small change in the number of crystal grains and hardness even when heated to a temperature equal to or higher than a recrystallization temperature (1200° C. to 1500° C.). The metal wire rod of the present invention is excellent in oxidative consumption resistance under a high-temperature atmosphere, and mechanical properties.
摘要翻译: 本发明提供一种由铱或铱合金构成的金属线材,其中纵向方向的任何截面上的晶粒数为2〜20 / 0.25mm 2,任何部分的维氏硬度为200Hv或 多于400 Hv。 铱线棒是通过μ-PD法制造的材料,残留应力低,即使在加热到再结晶温度以上的温度下,晶粒数和硬度也有小的变化 (1200℃〜1500℃)。 本发明的金属线棒在高温环境下的耐氧化消耗性优异,机械性能优良。
-
公开(公告)号:US20240321705A1
公开(公告)日:2024-09-26
申请号:US18269456
申请日:2021-12-13
IPC分类号: H01L23/498 , H01L23/00
CPC分类号: H01L23/49827 , H01L23/49811 , H01L23/49866 , H01L24/81 , H01L2224/81201
摘要: The interposer substrate is joined in an overlapping state to one or more members having a connection part at one place or more, and electrically connected to the member. The interposer substrate includes a base material having one or more connection regions corresponding to connection parts of the member to be joined. A plurality of through-holes are formed in the connection region. A segment as one unit for electrical connection is constituted by forming the plurality of through-holes adjacent to each other. One or more segments are formed in the connection region. In the through-hole are formed a through electrode and a bump with a wide width formed at an end of the through electrode. The through electrode and bump are composed of a metal powder sintered body formed by sintering a metal powder including gold or the like having a predetermined purity and average particle size.
-
公开(公告)号:US20170264082A1
公开(公告)日:2017-09-14
申请号:US15504500
申请日:2015-09-11
发明人: Koichi SAKAIRI , Hiroshi MATSUO , Kunihiro TANAKA
CPC分类号: H01T13/39 , B23K11/002 , H01T21/02
摘要: The present invention relates to a tape material for manufacturing an ignition plug electrode, the tape material being a member for forming an electrode chip, in which a base metal layer and a precious metal layer are cladded, on a bonded region set on an electrode base material of an ignition plug, the member is in the form of a long tape in which the base metal layer being in contact with the bonded region is cladded with the precious metal layer being in contact with the base metal layer, the base metal layer has a width substantially equal to one of the longitudinal width, lateral width and diameter of the bonded region. According to the present invention, bonding between a precious metal chip and a substrate can be reliably maintained to prolong the life of an ignition plug. Accordingly, precious metals can be efficiently used to save resources.
-
公开(公告)号:US20170130310A1
公开(公告)日:2017-05-11
申请号:US15127348
申请日:2015-03-23
发明人: Kiyohito ISHIDA , Toshihiro OMORI , Yutaka SATO , Kunihiro TANAKA , Muneki NAKAMURA , Koichi SAKAIRI , Tatsuya NAKAZAWA
CPC分类号: C22F1/10 , C22C19/03 , C22C19/055 , C22C19/056 , C22C30/00
摘要: The present invention relates to a NiIr-base heat-resistant alloy which includes a Ni—Ir—Al—W-base alloy which contains Ir: 5.0 to 50.0 mass %, Al: 1.0 to 8.0 mass %, W: 5.0 to 20.0 mass %, and the balance is Ni, and a γ′ phase having an L12 structure precipitating and dispersing in a matrix as an essential strengthening phase, and a ratio (Y/X) of a peak intensity (Y) of (201) plane of the Ir3W phase observed in the range of 2θ=48° to 50° to a peak intensity (X) of (111) plane of the γ′ phase observed in the range of 2θ=43° to 45° in X-ray diffraction analysis is 0.5 or less. The alloy exhibits good high-temperature property stably.
-
-
-
-
-
-