摘要:
High modulus, high tenacity fibers of poly-p-phenylene terephthalamide (PPD-T) are manufactured comprising a fiber heat treating process for increasing the inherent viscosity and the crystallinity index of the PPD-T. Never-dried fibers swollen with water of controlled acidity are heated beyond dryness in an atmoshphere having a flow of greater than Reynolds Number 10,000 throughout the duration of the heating.
摘要:
High modulus, high tenacity fibers of poly-p-phenylene terephthalamide (PPD-T) are disclosed along with a fiber heat treating process for increasing the inherent viscosity and the crystallinity index of the PPD-T. Never-dried fibers swollen with water of controlled acidity are heated beyond dryness.
摘要:
A method for producing para-aramid pulp includes forming a liquid, actively-polymerizing solution and subjecting the solution to orienting flow which produces an optically anisotropic liquid solution with polymer chains oriented in the direction of the flow. When the solution has a viscosity sufficient to maintain the orientation of the polymer chains, the solution is incubated until it gels. The gel is cut transversely at intervals and para-aramid pulp is isolated from the gel. Para-aramid pulp produced by the process can be used similarly to pulp produced from spun fiber.
摘要:
The present invention provides a process for recovering the chlorine value from a particulate feed stream of metal chlorides wherein the total energy and reactant mass flow are managed to minimize the build up of deposits of solids on the reactor walls and maximize the conversion of the metal chlorides to metal oxides and chlorine.
摘要:
A method for producing para-aramid pulp includes forming a liquid, actively-polymerizing solution and subjecting the solution to orienting flow which produces an optically anisotropic liquid solution with polymer chains oriented in the direction of the flow. When the solution has a viscosity sufficient to maintain the orientation of the polymer chains, the solution is incubated until it gels. The gel is cut transversely at intervals and para-aramid pulp is isolated from the gel. Para-aramid pulp produced by the process can be used similarly to pulp produced from spun fiber.