Low-friction member, image-forming device, and agent for forming low-friction coating film

    公开(公告)号:US10906277B2

    公开(公告)日:2021-02-02

    申请号:US15324571

    申请日:2015-08-07

    Abstract: A problem addressed by the present invention is to provide a low-friction member which does not easily lose low-friction properties thereof even when used for a relatively long period. The low-friction member LS according to the present invention is consisting of at least lubricating materials PL, PS and a polyimide resin MR. The low-friction member has a surface roughness Rsk or 0.500 or more and the surface exposure ratio of the lubricating materials of 15.0% or more. It is particularly preferred that the surface roughness Rsk be in a range of 0.0900 (inclusive) to 0.1400 (inclusive), and the surface exposure ratio of the lubricating materials be 35.0% or more. It is preferred that the lubricating materials be a fluororesin. The low-friction member thus has the property of not losing the low-friction properties thereof easily even when used for a relatively long period.

    Polyimide fiber and method for producing polyimide fiber

    公开(公告)号:US10662555B2

    公开(公告)日:2020-05-26

    申请号:US15425249

    申请日:2017-02-06

    Abstract: The method for producing a polyimide fiber includes a coagulation step of forming a polyimide precursor fiber by extruding a polyimide precursor solution containing a polyimide precursor and a compound having an acid dissociation constant (pKa) of a conjugate acid in water at 25° C. of 6.0 to 10 inclusive and an octanol-water partition coefficient (Log P) at 25° C. of −0.75 to 0.75 inclusive into a poor solvent or nonsolvent for the polyimide precursor; and a heat drawing step of forming the polyimide fiber by drawing the polyimide precursor fiber while heating same. The polyimide fiber of the present disclosure has a physical property such that the coefficient of thermal expansion thereof is in the range of −15 ppm/K to 0 ppm/K inclusive.

Patent Agency Ranking