ETHYLENE-PROPYLENE-DIENE RUBBER FOAMED MATERIAL AND SEALING MATERIAL
    11.
    发明申请
    ETHYLENE-PROPYLENE-DIENE RUBBER FOAMED MATERIAL AND SEALING MATERIAL 审中-公开
    乙烯 - 丙烯 - 丁二烯橡胶泡沫材料和密封材料

    公开(公告)号:US20140287223A1

    公开(公告)日:2014-09-25

    申请号:US14205774

    申请日:2014-03-12

    Abstract: An ethylene-propylene-diene rubber foamed material is obtained by foaming a rubber composition containing an ethylene-propylene-diene rubber. In the ethylene-propylene-diene rubber foamed material, the content ratio of a sulfur atom calculated based on the measurement result of a fluorescent X-ray measurement, based on mass, is 1000 ppm or less, a rate of change of a 50% compressive load value after being heated at 140° C. for 7 days to a 50% compressive load value before being heated is 50% or more and 150% or less, and the 50% compressive load value before being heated is 0.1 N/cm2 or more and 2.0 N/cm2 or less.

    Abstract translation: 通过使含有乙烯 - 丙烯 - 二烯橡胶的橡胶组合物发泡,得到乙烯 - 丙烯 - 二烯橡胶发泡体。 在乙烯 - 丙烯 - 二烯橡胶发泡材料中,基于质量计算的基于荧光X射线测量的测量结果计算的硫原子的含量比为1000ppm或更小,变化率为50% 在加热之前,在140℃下加热7天至50%压缩载荷值的压缩载荷值为50%以上且150%以下,加热前的50%压缩载荷值为0.1N / cm 2 以上且2.0N / cm 2以下。

Patent Agency Ranking