Composition comprising heterophasic propylene copolymer

    公开(公告)号:US10167384B2

    公开(公告)日:2019-01-01

    申请号:US15532172

    申请日:2015-11-26

    Inventor: Marc Herklots

    Abstract: The invention is directed to a composition comprising (A) a heterophasic propylene copolymer, (B) talc and (C) a functionalized polypropylene grafted with an acid or acid anhydride functional group, wherein the heterophasic propylene copolymer consists of (a) a propylene-based matrix, wherein the propylene-based matrix consists of a propylene homopolymer and/or a propylene-α-olefin copolymer consisting of at least 70 wt % of propylene and at most 30 wt % of a-olefin, based on the total weight of the propylene-based matrix and wherein the propylene-based matrix is present in an amount of 90 to 95 wt % based on the total heterophasic propylene copolymer and (b) a dispersed ethylene-α-olefin copolymer, wherein the dispersed ethylene-α-olefin copolymer is present in an amount of 10 to 5 wt % based on the total heterophasic propylene copolymer and wherein the sum of the total amount of propylene-based matrix and total amount of the dispersed ethylene-α-olefin copolymer in the heterophasic propylene copolymer is 100 wt %, wherein the heterophasic propylene copolymer has an MFI of 0.1-0.5 dg/min as determined according to IS01133 at 230° C. and 2.16 kg and wherein the amount of the talc in the composition is 0.025-10 wt % of the total composition and the amount of the functionalized polypropylene is 0.005-2.5 wt % of the total composition.

    COMPOSITION COMPRISING HETEROPHASIC PROPYLENE COPOLYMER

    公开(公告)号:US20180186983A1

    公开(公告)日:2018-07-05

    申请号:US15740112

    申请日:2016-06-23

    Abstract: The invention relates to a composition comprising (A) a heterophasic propylene copolymer and (B) a block copolymer, wherein the heterophasic propylene copolymer consists of (a) a propylene-based matrix, wherein the propylene-based matrix consists of a propylene homopolymer and/or a propylene-α-olefin copolymer consisting of at least 70 wt % of propylene and at most 30 wt % of α-olefin, based on the total weight of the propylene-based matrix and wherein the propylene-based matrix is present in an amount of 60 to 95 wt % based on the total heterophasic propylene copolymer and (b) a dispersed ethylene-α-olefin copolymer, wherein the dispersed ethylene-α-olefin copolymer is present in an amount of 40 to 5 wt % based on the total heterophasic propylene copolymer and wherein the sum of the total amount of propylene-based matrix and total amount of the dispersed ethylene-α-olefin copolymer in the heterophasic propylene copolymer is 100 wt %, and wherein the block copolymer comprises a terminal block comprising styrene or alpha-methylstyrene and wherein the ratio of the melt flow rate of (A) the heterophasic propylene copolymer (MFIheterophasic) and the melt flow rate of (B) the block copolymer (MFIblock) is at most 50, preferably at most 40, at most 30, at most 25 or at most 20, wherein MFIheterophasic and MFIblock are measured in accordance with ISO 1133 using a 2.16 kg weight and at a temperature of 230° C.

Patent Agency Ranking