POLYPROPYLENE COMPOSITION FOR AUTOMOTIVE INTERIOR APPLICATIONS

    公开(公告)号:US20170137617A1

    公开(公告)日:2017-05-18

    申请号:US15310283

    申请日:2015-05-18

    Applicant: BOREALIS AG

    Abstract: Polypropylene composition comprising a heterophasic propylene copolymer and a mineral filler, wherein said heterophasic propylene copolymer has a melting temperature in the range of 140 to 155° C., a xylene cold soluble content in the range of 20 to 35 wt.-% and a comonomer content of the xylene cold soluble fraction in the range of 18 to 95 wt.-%, wherein further the weight ratio between heterophasic propylene copolymer and the mineral filler is in the range of 2/1 to 4/1.

    POLYETHYLENE BLEND FOR A FILM LAYER

    公开(公告)号:US20250129241A1

    公开(公告)日:2025-04-24

    申请号:US18832327

    申请日:2023-01-24

    Applicant: BOREALIS AG

    Abstract: Disclosed is a polyethylene blend of a specific multimodal metallocene catalysed linear low density polyethylene (mLLDPE) and a specific high density polyethylene, produced in a presence of a Ziegler-Natta catalyst (ZN-HDPE), which provides films with well-balanced properties, especially stiffness/impact balance.

    HETEROPHASIC COPOLYMER OBTAINED BY A PROCESS FOR PRODUCING HETEROPHASIC COPOLYMER

    公开(公告)号:US20230002607A1

    公开(公告)日:2023-01-05

    申请号:US17898119

    申请日:2022-08-29

    Applicant: BOREALIS AG

    Abstract: A heterophasic copolymer composition obtained by a process comprising polymerising in multiple steps and multiple polymerisation reactors propylene monomer and a comonomer selected from ethylene, alpha-olefins having 4 to 10 carbon atoms and their mixtures, in the presence of an olefin polymerisation catalyst comprising a solid catalyst component and a co-catalyst, wherein the solid catalyst component comprises titanium, magnesium, halogen and an internal donor of the formula (I): wherein R1 and R2 are the same or different being a linear or branched C1-C12-alkyl group and R is hydrogen or a linear, branched or cyclic C1 to C12-alkyl.

    PROCESS FOR PREPARING A CAP OR CLOSURE

    公开(公告)号:US20220227030A1

    公开(公告)日:2022-07-21

    申请号:US17607059

    申请日:2020-04-28

    Applicant: BOREALIS AG

    Abstract: A process for producing a cap or closure comprising obtaining a polypropylene composition by sequential polymerization comprising the steps: A) polymerizing in a first reactor, preferably a slurry reactor, in the presence of a Ziegler-Natta catalyst monomers comprising propylene and optionally one or more comonomers selected from ethylene and C4-C10 alpha-olefins, to obtain a first propylene polymer fraction having a comonomer content in the range of 0.0 to 1.8 wt %, and a MFR2 in the range of from 12.0 to 40.0 g/10 min, as measured according to ISO 1133 at 230° C. under a load of 2.16 kg; B) polymerizing in a second reactor, preferably a first gas-phase reactor, monomers comprising propylene and one or more comonomers selected from ethylene and C4-C10 alpha-olefins, in the presence of the first propylene polymer fraction, to obtain a second propylene polymer fraction, wherein the polypropylene composition comprising said first and second propylene polymer fractions has an MFR2 in the range of from 12.0 to 60.0 g/10 min, as measured according to ISO 1133 at 230° C. under a load of 2.16 kg, has a comonomer content in the range of from 2.2 to 5.0 wt % and wherein the ratio of the comonomer content of component A) to the comonomer content of the polypropylene composition is 0.35 or less, C) melting, extruding and moulding the polypropylene composition in the presence of at least one nucleating agent to prepare a cap or closure; and D) exposing the cap or closure obtained in step (C) to a cooling rate of 50 K/s or more.

    NUCLEATED PROPYLENE POLYMER COMPOSITION WITH HIGH TOUGHNESS

    公开(公告)号:US20220135714A1

    公开(公告)日:2022-05-05

    申请号:US17429230

    申请日:2020-01-20

    Applicant: BOREALIS AG

    Abstract: The present invention is directed to a propylene polymer composition comprising (a) at least 90 wt. %, based on the weight of the total propylene homopolymer composition, of a propylene homopolymer having (i) a pentad isotacticity (mmmm) of equal or more than 98.0 mol.-%, determined by quantitative 13C NMR spectroscopy, (ii) a relative amount of erythro regio-defects of not more than 0.2 mol.-%, determined by quantitative 13C NMR spectroscopy, as described herein, and (b) a nucleating agent (B) selective for the beta-modification of isotactic polypropylene in an amount of from 0.001 to 1.0 wt. %, based on the weight of the total propylene homopolymer composition, wherein said propylene homopolymer composition has a melt flow rate MFR2 (230° C., 2.16 kg) according to ISO 1133 of 0.1 to 10 g/10 min., a beta-phase content of not less than 80%, measured by wide angle x-ray scattering (WAXS). Further disclosed is a moulded propylene homopolymer product obtainable by compression moulding or extrusion of the propylene homopolymer composition.

    PROPYLENE BUTENE COPOLYMER
    28.
    发明申请

    公开(公告)号:US20210395427A1

    公开(公告)日:2021-12-23

    申请号:US17292066

    申请日:2019-11-14

    Applicant: BOREALIS AG

    Abstract: The invention provides a multimodal propylene butene random copolymer having a melt flow rate (MFR2) of 1.0 to 20.0 g/10 min and a butene content of 5.0 to 20.0 wt %, wherein said copolymer is prepared using a single site catalyst and wherein said copolymer comprises: (i) 30 to 70 wt % of a propylene butene copolymer (A) having an MFR2 of 0.5 to 20.0 g/10 min and a butene content of 2.0 to 10.0 wt %; and (ii) 70 to 30 wt % of a propylene butene copolymer (B) having an MFR2 of 0.5 to 20.0 g/10 min and a butene content of 4.0 to 20.0 wt %; wherein copolymers (A) and (B) are different.

    HETEROPHASIC POLYPROPYLENE COMPOSITION WITH IMPROVED BALANCE OF PROPERTIES

    公开(公告)号:US20210253836A1

    公开(公告)日:2021-08-19

    申请号:US16973673

    申请日:2019-07-10

    Applicant: BOREALIS AG

    Abstract: The present invention is directed to a heterophasic polypropylene composition having an improved balance of desirable properties, i.e. high stiffness, high toughness, and high transparency. The heterophasic polypropylene composition of the present invention comprises 60.0 to 95.0 wt % of a crystalline propylene homopolymer with a melting temperature Tm1 measured by differential scanning calorimetry of higher than 155° C., 5.0 to 20.0 wt % of an elastomeric ethylene-propylene rubber, and at least one polymeric nucleating agent, wherein the crystalline propylene homopolymer (H-PP) and the elastomeric ethylene-propylene rubber (EPR) have been produced in the presence of a single-site catalyst, wherein the heterophasic polypropylene composition is characterized by a soluble fraction determined in 1,2,4-trichlorobenzene at 40° C. in the range of 5.0 to 20.0 wt %, and wherein the soluble fraction has an ethylene in content in the range of 12.0 to 40.0 wt %. The present invention is further directed to a process for the preparation of the heterophasic polypropylene composition comprising polymerizing propylene in at least three polymerization steps in the presence of a single-site catalyst, wherein the at least one polymeric nucleating agent is introduced either as a master batch by a compounding step or via a prepolymerization step prior to the first polymerization step. The present invention is further directed to an article obtained by extrusion of the heterophasic polypropylene composition, and to a packaging article comprising the extruded article. Finally, the present invention is directed to the use of the heterophasic polypropylene composition for the production of extruded articles such as films or sheets.