Abstract:
An object of the present invention is to provide ferrite particles having a high saturation magnetisation, and being excellent in the dispersibility in a resin, a solvent or a resin composition, a resin composition including the ferrite particles, and a resin film composed of the resin composition. The ferrite particles are a single crystalline body having an average particle size of 1 to 2000 nm, and Mn-based ferrite particles having a spherical shape, and have a saturation magnetisation of 45 to 95 Am2/kg. The resin composition includes the ferrite particles as a filler. The resin film is composed of the resin composition.
Abstract:
The object is to provide a composite magnetic powder for noise suppression to give a noise suppressor having ability to suppress the noise in a wide range from a low frequency through a high frequency while suppressing heat generation by reducing a dielectric constant loss on the high frequency side, and in order to attain the object, there is employed a composite magnetic powder for noise suppression in which the surface of a metallic powder is coated with a fine particle having a high dielectric constant and a binder resin or the like. By using this composite magnetic powder for noise suppression, there can be provided a noise suppressor excellent in ability to suppress the noise in a wide frequency region.
Abstract:
A porous ferrite core material for an electrophotographic developer wherein the apparent density thereof is 1.5 to 1.9 g/cm3, the shape factor SF-2 thereof is 101 to 110 and the magnetization as measured with a VSM at 1K·1000/4π·A/m is 40 to 60 Am2/kg, a resin-coated ferrite carrier for an electrophotographic developer obtained by coating the surface of the porous ferrite core material with a resin, and an electrophotographic developer using the ferrite carrier.
Abstract:
Provided are a ferrite powder capable of maintaining a high withstand voltage even when used in a resin composition having high magnetic properties and electrical resistivity and a high filling ratio, and a method for producing the same. A ferrite powder composed of spherical ferrite particles, wherein the ferrite powder contains iron (Fe): 55.0-70.0 mass % and manganese (Mn): 3.5-18.5 mass %, the ferrite powder containing more than 0.0 mass % to 7.5 mass % α-Fe2O3, and the ferrite powder has a volume average particle size (D50) of 15.0 μm or less.
Abstract:
Provided is an iron oxide powder for a brake friction material which can be suitably used in a brake friction material that is less likely to cause problems regarding brake squealing and that provides superior braking performance. The iron oxide powder for a brake friction material according to a first embodiment of the present invention is characterized by having a sulfur content of 150 ppm or less as measured by combustion ion chromatography, and a saturation magnetization of 20 emu/g or less. The iron oxide powder for a brake friction material according to a second embodiment of the present invention is characterized by having an average particle size of 1.0 μm or more, a chlorine content of 150 ppm or less as measured by combustion ion chromatography, and a saturation magnetization of 20 emu/g or less.
Abstract:
Provided are: an Mn ferrite powder characterized by including a plurality of ferrite particles, having a volume-average particle diameter of 1-10 μm, and having a 2.106 μm volume-based cumulative distribution (sieved) of 0.1-50.0 vol %; and a resin composition characterized by including said powder and a resin material.
Abstract:
Mn—Zn ferrite particles according to the present invention contain 44-60% by mass of Fe, 10-16% by mass of Mn and 1-11% by mass of Zn. The ferrite particles are single crystal bodies having an average particle diameter of 1-2,000 nm, and have polyhedral particle shapes, while having an average sphericity of 0.85 or more but less than 0.95.
Abstract:
An object of the present invention is to provide a ferrite carrier core material for an electrophotographic developer having desired resistance properties and charging properties with small environmental variation of resistivity and charge amount while maintaining the advantages of ferrite carriers, a ferrite carrier for an electrophotographic developer, an electrophotographic developer using the ferrite carrier, and a method for manufacturing the ferrite carrier core material for an electrophotographic developer. In order to solve the problem, a ferrite carrier core material comprising ferrite particles containing 15 mass % or more and 25 mass % or less of Mn, 0.5 mass % or more and 5.0 mass % or less of Mg, 0.05 mass % or more and 4.0 mass % of Sr, and 45 mass % or more and 55 mass % or less of Fe, with Si localized in the surface thereof is used.
Abstract:
An object of the present invention is to provide a ferrite carrier core material for an electrophotographic developer having desired resistance properties and charging properties with small environmental variation of resistivity and charge amount while maintaining the advantages of ferrite carriers, a ferrite carrier for an electrophotographic developer, an electrophotographic developer using the ferrite carrier, and a method for manufacturing the ferrite carrier core material for an electrophotographic developer. In order to solve the problem, a ferrite carrier core material comprising ferrite particles containing 15 mass % or more and 25 mass % or less of Mn, 0.5 mass % or more and 5.0 mass % or less of Mg, 0.05 mass % or more and 4.0 mass % of Sr, and 45 mass % or more and 55 mass % or less of Fe, with Zr localized in the surface thereof is used.
Abstract:
Ferrite powder of the present invention is ferrite powder detectable with a metal detector, comprising: hard ferrite particles containing Sr of 7.8 mass % or more and 9.0 mass % or less and Fe of 61.0 mass % or more and 65.0 mass % or less, wherein an amount of Na to be measured by ion chromatography is 1 ppm or more and 200 ppm or less. It is preferable that a volume average particle diameter of the particles constituting the ferrite powder is 0.1 μm or more and 100 μm or less. It is preferable that residual magnetization by a VSM measurement when magnetic field of 10 K·1000/4πA/m is applied is 25 A·m2/kg or more and 40 A·m2/kg or less.