摘要:
A toner, including a colorant; a binder resin; a release agent; and a fixing supplemental component, wherein the toner has a storage elastic modulus G′ (Pa) satisfying the following conditions: 5.0×104
摘要:
A toner, comprising a colorant, a crystalline polyester resin, and an amorphous polyester resin, in which the crystalline polyester resin satisfies the following relations: 60≦(T2-cp)
摘要:
A toner including a binder resin comprising a modified polyester having an ester bond and a chemical bond other than the ester bond, and a crystalline polyester; and a release agent comprising a microcrystalline wax comprising a hydrocarbon having 20 to 80 carbon atoms which comprises 55 to 70% by weight of a linear hydrocarbon. The microcrystalline wax has an acid value of from 0.1 to 20 mgKOH/g and a melting point of from 65 to 90° C. The melting point is a temperature at which a local maximum endothermic peak is observed in a differential thermal curve measured by differential scanning calorimetry (DSC). The release agent is dispersed in the toner with a dispersion diameter of from 0.06 to 1.50 μm.
摘要:
Provided is a static charge image developing toner of which flowing start temperatures (Tfb) measured with a flow tester satisfy relational formulae below: Tfb(2-5)=100−[Tfb(5 Kg)/Tfb(2 Kg)]×100 (Formula 1) 2.00≦Tfb(2-5)≦6.50 (Formula 2) where in Formula 1 above, Tfb(2 Kg) and Tfb(5 Kg) represent flowing start temperatures of the static charge image developing toner when 1.5 g of the toner is heated at a temperature raising rate of 3° C./minute and let to flow out from a die having a diameter of 1.0 mm under loads of 2 Kg and 5 Kg respectively.
摘要:
An image forming apparatus including: image bearing member; latent image forming unit; developing unit; transfer unit; fixing unit, wherein toner in the developing unit contains amorphous polymer, crystalline resin and releasing agent, when the toner is measured for G′ at 40° C. to 210° C. with rheometer at 1 Hz and 1 deg, G′(100) is ≦20,000 and G′(150) is ≧500 Pa, and straight line drawn by connecting points of the G′(100) and G′(110) on curve of the G′ has gradient of ≦0.035, the gradient being “a” expressed by: a=|log10G′(100)−log10G′(110)|/10, and the fixing unit includes: heating member containing flexible endless belt; heat source fixed within the flexible endless belt; and press member in contact with the belt to form nip portion, and the fixing unit is configured to heat/press the medium passing through the nip portion to fix the image on the medium.
摘要:
A method of manufacturing toner including melting, mixing, and kneading a releasing agent and a coloring agent with at least part of a polyester binder resin, and suspending and granulating an oil phase comprising the binder resin, the coloring agent, and the releasing agent in an aqueous medium.
摘要:
A toner including at least one polyester resin serving as a binder resin, a colorant, a releasing agent, and a fixing aid, wherein the fixing aid includes a fatty acid amide-based compound, and the fatty acid amide-based compound is at least one of a fatty acid amide compound having a mono- or higher valent amide bond and a fatty acid amide-based compound having a mono- or higher valent amino group or a hydroxyl group.
摘要:
A toner including at least one polyester resin serving as a binder resin, a colorant, a releasing agent, and a fixing aid, wherein the fixing aid includes a fatty acid amide-based compound, and the fatty acid amide-based compound is at least one of a fatty acid amide compound having a mono- or higher valent amide bond and a fatty acid amide-based compound having a mono- or higher valent amino group or a hydroxyl group.
摘要:
A method of manufacturing toner including melting, mixing, and kneading a releasing agent and a coloring agent with at least part of a polyester binder resin, and suspending and granulating an oil phase comprising the binder resin, the coloring agent, and the releasing agent in an aqueous medium.
摘要:
Provided is a resin powder including first particles containing a polyolefin-based resin, wherein surfaces of the first particles are coated with second particles at an average coating ratio of 0.15 or greater, where the average coating ratio is measured with a Material Development Kit (MDK) at a temperature lower than a melting point of the resin powder for producing a three-dimensional object by 15 degrees C.