摘要:
A glass composition which is reduced in the amount of residual bubbles and is produced using smaller amounts of an environmentally unfriendly component such as arsenic oxide and antimony oxide. This glass composition contains, in terms of mass %: 40-70% SiO2; 5-20% B2O3; 10.25% Al2O3; 0-10% MgO; 0-20% CaO; 0-20% SrO; 0-10% BaO; 0-0.5% Li2O; 0-1.0% Na2O; 0-1.5% K2O; and 0-1.5%, excluding 0%, Cl, Li2O+Na2O+K2O exceeding 0.06%. The glass composition can be produced suitably using, for example, a chloride as part of the raw glass materials.
摘要:
A glass flake (10) having improved heat resistance and chemical resistance is formed from a glass base material satisfying, in mass %, 60≦SiO2≦75, 5
摘要:
A glass substrate for a display, which is formed of a glass having a light weight and having high refinability with decreasing environmental burdens, the glass comprising, by mass %, 50 to 70% of SiO2, 5 to 18% of B2O3, 10 to 25% of Al2O3, 0 to 10% of MgO, 0 to 20% of CaO, 0 to 20% of SrO, 0 to 10% of BaO, 5 to 20% of RO (in which R is at least one member selected from the group consisting of Mg, Ca, Sr and Ba), and over 0.20% but not more than 2.0% of R′2O (in which R′ is at least one member selected from the group consisting of Li, Na and K), and containing, by mass %, 0.05 to 1.5% of oxide of metal that changes in valence number in a molten glass, and substantially containing none of As2O3, Sb2O3 and PbO.
摘要翻译:一种显示器用玻璃基板,其由重量轻且具有降低的环境负荷的高可熔性的玻璃形成,所述玻璃以质量%计含有50〜70%的SiO 2,5〜18%的B 2 O 3,10〜 25%的Al 2 O 3,0〜10%的MgO,0〜20%的CaO,0〜20%的SrO,0〜10%的BaO,5〜20%的RO(其中R为选自 由Mg,Ca,Sr和Ba组成的组)和超过0.20%但不超过2.0%的R'2O(其中R'为选自Li,Na和K中的至少一种), 并且以质量%计含有熔融玻璃中价数变化的金属氧化物的0.05〜1.5%,并且基本上不含有As 2 O 3,Sb 2 O 3和PbO。
摘要:
A glass substrate for a display, which is formed of a glass having a light weight and having high refinability with decreasing environmental burdens, the glass comprising, by mass %, 50 to 70% of SiO2, 5 to 18% of B2O3, 10 to 25% of Al2O3, 0 to 10% of MgO, 0 to 20% of CaO, 0 to 20% of SrO, 0 to 10% of BaO, 5 to 20% of RO (in which R is at least one member selected from the group consisting of Mg, Ca, Sr and Ba), and over 0.20% but not more than 2.0% of R′2O (in which R′ is at least one member selected from the group consisting of Li, Na and K), and containing, by mass %, 0.05 to 1.5% of oxide of metal that changes in valence number in a molten glass, and substantially containing none of As2O3, Sb2O3 and PbO.
摘要:
Disclosed is a wireless communication apparatus for receiving a code-spread transmission signal. The wireless communication apparatus includes: an RF section; and a baseband section, wherein, in the baseband section, despreaders of an integral submultiple, which is 1/n1, of the number of chips of a spread code are arranged in parallel, and there is provided a propagation measurement section that measures a propagation channel by using the plurality of despreaders a plurality of times in a time-division manner and performing despread of each period corresponding to a chip rate of the spread code.
摘要:
Disclosed is a glass composition which can be suitably used as a glass filler to be blended into a polycarbonate resin. This glass composition contains, in mass %, 50≦SiO2≦60, 8≦Al2O3≦15, 0≦MgO≦10, 10≦CaO≦30, 0≦Li2O+Na2O+K2O
摘要翻译:公开了一种玻璃组合物,其可以适合用作要掺入聚碳酸酯树脂中的玻璃填料。 该玻璃组合物以质量%计含有50 <= SiO 2 =60,8≤Al2 O 3 =15,0≤MOBO= 10,10 <= CaO <= 30,0 <= Li 2 O + Na 2 O + K 2 O 2和5
摘要:
The present invention provides a glass composition that has good formability and tends not to cause electric-field breakdown when formed into a spacer for an electron beam-excited display. The present invention relates to a glass composition that contains the following components, in terms of mass %: 20≦SiO2
摘要:
The present invention improves a method of forming a surface unevenness using a difference in etching rates, and relaxes limitations on substrates in this method. In a method of the present invention, an uneven surface is formed by a method including applying pressure to a predetermined region in a surface of a thin film formed on a substrate, and etching a region including at least a portion of the predetermined region and at least a portion of the reminder of the surface that excludes the predetermined region. An etching rate difference within the thin film increases freedom in selecting a substrate material.
摘要:
The present invention provides a glass composition in which a smaller amount of arsenic oxide or antimony oxide that has a heavy burden on the environment is used and fewer bubbles remain. This glass composition includes, in terms of mass %: 40 to 70% of SiO2, 5 to 20% of B2O3, 10 to 25% of Al2O3, 0 to 5% of MgO (up to and not including 5%), 0 to 20% of CaO, 0 to 20% of SrO, 0 to 10% of BaO, 0 to 1.5% of Li2O, 0 to 1.5% of Na2O, 0 to 1.5% of K2O, and 0 to 1.5% of Cl. The sum of the contents of Li2O, Na2O, and K2O is 0.05 to 1.5 mass %, and the content of K2O is equal to or larger than that of Na2O.
摘要翻译:本发明提供一种玻璃组合物,其中使用较少量的环境负担较重的氧化亚砷或氧化锑,并且保留较少的气泡。 该玻璃组合物以质量%计含有40〜70%的SiO 2,5〜20%的B 2 O 3 3, 10〜25%的Al 2 O 3 3,0〜5%的MgO(不高于5%),0〜20%的CaO,0〜20 0%的BaO,0〜1.5%的Li 2 O,0〜1.5%的Na 2 O,0〜1.5%的K 2, SUB> 2 O,0〜1.5%的Cl。 Li 2 O,Na 2 O和K 2 O 2的含量之和为0.05〜1.5质量%,含量为 K 2 O等于或大于Na 2 O的O 2。
摘要:
The glass composition of the present invention includes the following components, expressed in mass%: 70% to 88% of SiO2; 6% to 18% of B2O3; 0.5% to 4.5% of Al2O3; 0% to 0.5% of Li2O; 0% to 0.5% of Na2O; 2% to 10% of K2O; and 0% to 2% of MgO+CaO+SrO+BaO, and the glass composition further includes chlorine (Cl). The glass composition of the present invention is used suitably as a glass substrate for an information display device.
摘要翻译:本发明的玻璃组合物包含以质量%表示的以下组分:70%〜88%的SiO 2; 6%至18%的B 2 O 3 3; 0.5%至4.5%的Al 2 O 3 3; 0%至0.5%的Li 2 O; 0%至0.5%的Na 2 O; 2%至10%的K 2 O; 和0〜2%的MgO + CaO + SrO + BaO,玻璃组合物还含有氯(Cl)。 本发明的玻璃组合物适合用作信息显示装置的玻璃基板。