Abstract:
A glass composition of the present invention is an oxide glass, in which the percentages of elements except for oxygen (O) contained therein are as follows, in terms of atom %: the amount of boron (B) exceeds 72% but does not exceed 86%, the total amount of lithium (Li), sodium (Na), and potassium (K) is 8% to 20%, the total amount of magnesium (Mg), calcium (Ca), strontium (Sr), and barium (Ba) is 1% to 8%, the amount of silicon (Si) is from 0% to less than 15%, and the amount of zinc (Zn) is from 0% to less than 2%. This glass composition further may contain molybdenum (Mo) and/or tungsten (W) in the range of more than 0% but not more than 3%.
Abstract:
The present invention aims to drive a PDP at low voltage by providing a material with a high secondary electron emission coefficient under a practical manufacturing condition. In order to achieve the aim, a crystalline oxide selected from the group consisting of CaSnO3, SrSnO3, BaSnO3, and a solid solution of two or more of them, in which an amount of Ca, Sr or Ba in a surface region thereof is reduced, is used as a material for a protective film when a plasma display panel is produced.
Abstract:
A plasma display panel of the present invention includes display electrodes and address electrodes that cross each other. The electrode to be covered with the first dielectric layer contains at least one selected from silver and copper. The first glass contains Bi2O3. The first glass further contains 0 to 4 wt % of MoO3 and 0 to 4 wt % of WO3, and the total of the contents of MoO3 and WO3 that are contained in the first glass is in a range of 0.1 to 8 wt %. The first glass may contain, as components thereof: 0 to 15 wt % SiO2; 10 to 50 wt % B2O3; 15 to 50 wt % ZnO; 0 to 10 wt % Al2O3; 2 to 40 wt % Bi2O3; 0 to 5 wt % MgO; 5 to 38 wt % CaO+SrO+BaO; 0 to 4 wt % MoO3; and 0 to 4 wt % WO3, and the total of the contents of MoO3 and WO3 that are contained in the first glass is in the range of 0.1 to 8 wt %.
Abstract:
A printer includes a first receiving unit that receives a print job containing a printing requirement, where the printing requirement is set as either an indispensable requirement that is indispensable for executing the print job or a desired requirement that is desirable for executing the print job; a second receiving unit that receives, from each of external image forming apparatuses connected to the image forming apparatus via a network, a printability level indicating whether the external image forming apparatus has a printing function satisfying the indispensable requirement or a printing function satisfying the desired requirement; a selecting unit that selects an image forming apparatus that executes the print job from the external image forming apparatuses by checking the printability level; and a print-operation control unit that sends the print job to the selected image forming apparatus and causes the selected image forming apparatus to execute the print job.
Abstract:
A plasma display panel (200) of the present invention includes a first panel (1) and a second panel (8). A discharge space (14) is formed between the first panel (1) and the second panel (8). In the plasma display panel (200), an electron emitting material (20) is disposed to face the discharge space (14). The electron emitting material (20) contains Sn, an alkali metal, O (oxygen), and at least one element selected from the group consisting of Ca, Sr, and Ba.
Abstract:
A head apparatus includes: a head unit where a plurality of magnetic elements, which carry out reproducing and/or recording on data tracks on a magnetic tape, are disposed at equal intervals on a first straight line; a moving mechanism that moves the head unit; and a controller that carries out tracking control to cause the moving mechanism to move the head unit and keep the magnetic elements on the data tracks. The moving mechanism can rotate the head unit so as to increase or decrease an angle between a second straight line along a width of the magnetic tape and the first straight line. During tracking control, the controller causes the moving mechanism to rotate the head unit so as to increase or decrease the angle in accordance with changes in an interval between the data tracks and keep the respective magnetic elements on the respective data tracks.
Abstract:
A burst interval measuring apparatus includes: a detector that outputs detection signals that can to measure a burst interval of servo patterns for a tracking servo; and a measuring unit that measures the burst interval based on the detection signals. The detector is constructed so as to be capable of outputting the detection signals that can measure the burst interval at plural positions that are separated in a width direction of the magnetic tape inside one of the servo patterns. The measuring unit uses measurement values for the burst interval at at least two positions out of the plural positions that have been measured based on the detection signals to specify velocity fluctuations in a movement velocity of the magnetic tape in the length direction and corrects the measurement values based on the velocity fluctuations.
Abstract:
Disclosed is a glass composition composed of an oxide glass wherein the percentages of constitutional elements other than oxygen (O) expressed in atomic % are as follows: boron (B) is not less than 56% and not more than 72%; silicon (Si) is not less than 0% and not more than 15%; Zinc (Zn) is not less than 0% and not more than 18%; potassium (K) is not less than 8% and not more than 20%; and the total of K, sodium (Na) and lithium (Li) is not less than 12% and not more than 20%. This glass composition further may contain at least one of magnesium (Mg), calcium (Ca), strontium (Sr) and barium (Ba) in an amount of more than 0% and not more than 5%, and molybdenum (Mo) and/or tungsten (W) in an amount of more than 0% and not more than 3%.
Abstract:
A glass composition for covering electrodes of the present invention contains: 0 to 15 wt % SiO2; 10 to 50 wt % B2O3; 15 to 50 wt % ZnO; 0 to 10 wt % Al2O3; 2 to 40 wt % Bi2O3; 0 to 5 wt % MgO; 5 to 38 wt % CaO+SrO+BaO; 0 to 0.1 wt % Li2O+Na2O+K2O; 0 to 4 wt % MoO3; and 0 to 4 wt % WO3, and the total of the contents of MoO3 and WO3 is in the range of 0.1 to 8 wt %. The glass composition for covering electrodes of the present invention may contain: 0 to 2 wt % SiO2; 10 to 50 wt % B2O3; 15 to 50 wt % ZnO; 0 to 10 wt % Al2O3; 2 to 40 wt % Bi2O3; 0 to 5 wt % MgO; 5 to 38 wt % CaO+SrO+BaO; 0 to 4 wt % MoO3; and 0 to 4 wt % WO3, and the total of the contents of MoO3 and WO3 may be in the range of 0.1 to 8 wt %.
Abstract translation:本发明的覆盖电极用玻璃组合物含有:0〜15重量%的SiO 2; 10至50重量%B 2 O 3 3; 15〜50wt%的ZnO; 0至10重量%的Al 2 O 3 3; 2至40重量%的Bi 2 O 3 3; 0〜5重量%的MgO; 5〜38重量%CaO + SrO + BaO; 0〜0.1重量%Li 2 O + Na 2 O + K 2 O; 0至4wt%MoO 3 3; 和0至4重量%的WO 3,MoO 3 3和WO 3 3的含量的总和在0.1至8的范围内 重量%。 本发明的覆盖电极用玻璃组合物可以含有0〜2重量%的SiO 2, 10至50重量%B 2 O 3 3; 15〜50wt%的ZnO; 0至10重量%的Al 2 O 3 3; 2至40重量%的Bi 2 O 3 3; 0〜5重量%的MgO; 5〜38重量%CaO + SrO + BaO; 0至4wt%MoO 3 3; 和0〜4重量%的WO 3,MoO 3 3和WO 3的含量的总和可以在0.1〜 8重量%。