Process of burning cattle dung
    31.
    发明授权
    Process of burning cattle dung 失效
    燃烧牛粪的过程

    公开(公告)号:US4747356A

    公开(公告)日:1988-05-31

    申请号:US11559

    申请日:1987-02-04

    摘要: Disclosed is a process for burning cattle dung at a temperature of from 500.degree. to 780.degree. C., preferably from 650.degree. to 780.degree. C., in the presence of one or more aluminum-containing substances selected from the class consisting of bauxite, kaolin and aluminum compound-containing ash from furnaces for firing solid fuels. A major part of the alkalies contained in the cattle dung and a substantial part of the chlorine are retained in combined form in the resulting furnace ash.

    摘要翻译: 公开了一种在一种或多种选自以下的含铝物质存在下,在500至780℃,优选650℃至780℃的温度下燃烧牛粪的方法,该方法包括:铝土矿, 用于燃烧固体燃料的熔炉中的高岭土和含铝化合物的灰分。 牛粪中含有的碱的主要部分和大部分氯在所得的炉灰中以组合的形式保留。