公开(公告)号:US5796019A
公开(公告)日:1998-08-18
申请号:US583516
申请日:1996-01-05
CPC分类号: H01B1/16 , B22F1/0011 , C22C29/12 , C22C32/0021
摘要: A method of manufacturing an electrically conductive cermet that includes less than 35% by volume of a precious metal by mixing a powdered refractory ceramic with the powdered metal, molding the mixture into a green, and sintering the green to create a cermet with a dense ceramic phase and a metallic phase in the form of a coherent network. The object is good electric conductivity at a low metal content. The precious metal powder is selected to shrink less and exhibits less sintering tendency as it forms the metallic phase than does the ceramic powder as it forms the ceramic phase.
摘要翻译: 一种制造导电金属陶瓷的方法,其通过将粉末状耐火陶瓷与粉末状金属混合,将该混合物混合成绿色,并且将该陶瓷烧结成具有致密陶瓷的金属陶瓷,该陶瓷陶瓷包含小于35体积%的贵金属 相位和相干网络形式的金属相位。 该物体在低金属含量下具有良好的导电性。 选择贵金属粉末与其形成陶瓷相时相比陶瓷粉末形成金属相时收缩较少并且表现出较少的烧结倾向。