摘要: Disclosed is an alkali-doped optical fiber perform and method for making the same. A silica glass member, such as a rod or the like is heated in a furnace chamber at a temperature of less than 75° C. below the softening point of the glass rod in an environment containing an alkali metal vapor to form an alkali metal oxide doped glass rod. This method provides a peak concentration in the outer half portion of the silica glass member. The alkali metal oxide doped glass member may be overclad with additional glass to form an optical fiber preform ready for drawing into an optical fiber. Alternatively, the alkali metal oxide doped glass member may be inserted into a porous, glass soot optical fiber preform or inserted into a tube comprising solid glass.
摘要翻译: 公开了一种碱掺杂光纤的制造方法及其制造方法。 在含有碱金属蒸气的环境中,在玻璃棒的软化点以下的温度低于75℃的炉室中加热石英玻璃构件,形成碱金属氧化物 掺杂玻璃棒。 该方法提供石英玻璃构件的外半部分的峰值浓度。 掺杂碱金属氧化物的玻璃构件可以用额外的玻璃包覆以形成准备用于拉入光纤的光纤预制件。 或者,掺杂碱金属氧化物的玻璃构件可以插入到多孔玻璃烟炱光纤预制件中或插入到包含固体玻璃的管中。