    Abstract: Provided are an apparatus for removing phosphorous from wastewater including: a first coagulation sedimentation unit including a first rapid mixing tank, a first flocculation tank and a first sedimentation tank; and a second coagulation sedimentation unit including a second rapid mixing tank, a second flocculation tank and a second sedimentation tank, and a method for removing phosphorous using the same. The first rapid mixing tank stirs wastewater and an inorganic coagulant with low basicity at high speed and the second rapid mixing tank stirs the treated water supplied from the first sedimentation tank and an inorganic coagulant with high basicity at high speed. As a result, removal of phosphorous from the wastewater is maximized and coagulation and sedimentation may be optimized through control of metal content in the inorganic coagulants added to the first rapid mixing tank and the second rapid mixing tank.

    Abstract translation: 提供了一种用于从废水中除去磷的设备,包括:第一凝结沉降单元,包括第一快速混合罐,第一絮凝罐和第一沉淀池; 以及包括第二快速混合槽,第二絮凝槽和第二沉淀池的第二凝结沉降单元,以及使用其形成的除去磷的方法。 第一快速混合槽高速搅拌废水和碱度低的无机凝结剂,第二快速混合槽以高速度搅拌从第一沉淀池供给的处理水和高碱度的无机凝结剂。 结果,从废水中除去磷最多,通过控制添加到第一快速混合罐和第二快速混合罐中的无机凝结剂中的金属含量,可以优化凝结和沉淀。

    Method of preparing a green-ceramic pigment for reduction firing using copper oxide and a green ceramic made thereby
    3.
    发明申请
    Method of preparing a green-ceramic pigment for reduction firing using copper oxide and a green ceramic made thereby 有权
    制备用于使用氧化铜还原焙烧的绿色陶瓷颜料的方法和由此制成的生坯

    公开(公告)号:US20100304031A1

    公开(公告)日:2010-12-02

    申请号:US12456789

    申请日:2009-06-23

    Applicant: Byung-Ha Lee

    Inventor: Byung-Ha Lee

    CPC classification number: C04B35/45 C04B35/457 C04B35/6262 C04B35/64

    Abstract: A method of preparing a green-ceramic pigment for reduction firing using copper oxide that includes mixing tin oxide (SnO2) and copper oxide (CuO); providing a fired product by applying oxidation firing to the mixture at a firing temperature of 1000 to 1300° C.; and grinding the fired product. Aspects also provide a green-ceramic pigment prepared by this method, as well as a method of manufacturing a green ceramic.

    Abstract translation: 一种使用包括混合氧化锡(SnO 2)和氧化铜(CuO))的氧化铜制备用于还原烧制的生陶瓷颜料的方法; 通过在1000〜1300℃的烧成温度下对所述混合物进行氧化烧成来提供烧成品; 并研磨烧制产品。 方面还提供通过该方法制备的绿色陶瓷颜料以及生产陶瓷的方法。

    APPARATUS AND METHOD FOR PHOSPHOROUS REMOVAL FROM WASTE WATER USING DOLOMITE
    4.
    发明申请
    APPARATUS AND METHOD FOR PHOSPHOROUS REMOVAL FROM WASTE WATER USING DOLOMITE 审中-公开
    使用DOLOMITE从废水中去除磷的装置和方法

    公开(公告)号:US20130334143A1

    公开(公告)日:2013-12-19

    申请号:US13593191

    申请日:2012-08-23

    CPC classification number: C02F1/5236 C02F2101/105

    Abstract: The present disclosure provides apparatus and method for phosphorous removal using dolomite by mixing an inorganic coagulant and dolomite together to improve the phosphorous removal efficiency and controlling pH, which has been lowered due to the use of the inorganic coagulant, close to the neutral by means of dolomite to improve the economic feasibility and minimize an additional neutralizing process.

    Abstract translation: 本公开提供了使用白云石通过将无机凝结剂和白云石混合在一起来去除白云石的装置和方法,以提高除磷效率,并且通过使用无机凝结剂将pH降至最接近中性点 白云石,以改善经济可行性,并尽量减少额外的中和过程。

    Method of preparing a green-ceramic pigment for reduction firing using copper oxide and a green ceramic made thereby
    5.
    发明授权
    Method of preparing a green-ceramic pigment for reduction firing using copper oxide and a green ceramic made thereby 有权
    制备用于使用氧化铜还原焙烧的绿色陶瓷颜料的方法和由此制成的生坯

    公开(公告)号:US08334018B2

    公开(公告)日:2012-12-18

    申请号:US12456789

    申请日:2009-06-23

    Applicant: Byung-Ha Lee

    Inventor: Byung-Ha Lee

    CPC classification number: C04B35/45 C04B35/457 C04B35/6262 C04B35/64

    Abstract: A method of preparing a green-ceramic pigment for reduction firing using copper oxide that includes mixing tin oxide (SnO2) and copper oxide (CuO); providing a fired product by applying oxidation firing to the mixture at a firing temperature of 1000 to 1300° C.; and grinding the fired product. Aspects also provide a green-ceramic pigment prepared by this method, as well as a method of manufacturing a green ceramic.

    Abstract translation: 一种使用包括混合氧化锡(SnO 2)和氧化铜(CuO))的氧化铜制备用于还原烧制的生陶瓷颜料的方法; 通过在1000〜1300℃的烧成温度下对所述混合物进行氧化烧成来提供烧成品; 并研磨烧制产品。 方面还提供通过该方法制备的绿色陶瓷颜料以及生产陶瓷的方法。