摘要: A cemented carbide body is 1-30% by mass of binder consisting of Co, Co/Ni, Co/Fe, Co/Ni/Fe or Ni/Fe and a hard material having a hexagonal WC phase and having a face-centered cubic phase of the form (M1, M2, M3)C or (M1, M2, M3)(C, N) or (M1, M2, M3)(O, C, N) where M1=Ti and/or Zr and M2=W and M3 optionally means none or one or a plurality of the elements Ta, Nb, Hf, Cr, Mo or V, wherein the proportion of the face-centered cubic phase based on the total mass is 2% to 97%, preferably 5 to 12% by mass, and the microstructure of the hexagonal phase and of the face-centered cubic phase has a mean grain size of between 0.2 μm and 1 μm, preferably ≦0.9 μm, and the mean grain sizes of the hexagonal phase and of the face-centered cubic phase differ at most by 30%.
摘要翻译: 硬质合金体为由Co,Co / Ni,Co / Fe,Co / Ni / Fe或Ni / Fe组成的粘合剂为1-30质量%,硬质合金具有六方晶相WC并具有面心立方 形式(M1,M2,M3)C或(M1,M2,M3)(C,N)或(M1,M2,M3)(O,C,N)的形式(M1,M2,M3)的相位,其中M1 = Ti和/或Zr和M2 = W和M3可选地意味着不含或一个或多个元素Ta,Nb,Hf,Cr,Mo或V,其中基于总质量的面心立方相的比例为2%至97%,优选 5〜12质量%,六方晶相和面心立方相的微观结构的平均粒径为0.2μm〜1μm,优选为nlE;0.9μm,六方相的平均粒径 和面心立方相最多相差30%。