CPC分类号: C25D5/50 , C25D5/12 , G11B5/858 , H01F41/26 , Y10T428/12611 , Y10T428/1275
摘要: A process for producing magnetic plated media suitable for use in high-performance disk drives is disclosed. A layer of nickel is first provided on a standard aluminum alloy substrate, by electroless deposition, to improve adhesion of subsequent layers. A layer of nickel phosphorous and a magnetic layer of nickel cobalt are then, in turn, electroplated. The plated media disk is then oxidized below a nickel-magnetizing temperature to provide a protective outer surface.A variation of this process is also disclosed. This time a magnetically-shielding copper layer is electroplated over the first nickel layer. The nickel phosphorous and nickel cobalt layers are then electroplated on as before. The plated media can now be oxidized at a temperature higher than the nickel-magnetizing temperature to speed up the process.
摘要翻译: 公开了一种用于生产适用于高性能磁盘驱动器的磁性电镀介质的工艺。 首先通过无电沉积在标准铝合金基底上提供镍层,以改善后续层的粘附性。 然后电镀一层镍磷和一个镍钴磁性层。 然后将镀覆的介质盘氧化成低于镍磁化温度以提供保护性外表面。 还公开了该方法的变体。 这次磁屏蔽铜层电镀在第一镍层上。 镍磷和镍钴层然后如前所述电镀。 电镀介质现在可以在高于镍磁化温度的温度下被氧化,以加速工艺。
-
公开(公告)号:US4581109A
公开(公告)日:1986-04-08
申请号:US560478
申请日:1983-12-12
申请人: Dan Goor , Everett Niles , Robert L. Stone
发明人: Dan Goor , Everett Niles , Robert L. Stone
CPC分类号: G11B5/858 , C25D5/12 , C25D5/50 , H01F41/26 , Y10S205/922
摘要: A process for producing magnetic plated media suitable for use in high-performance disk drives is disclosed. A layer of nickel is first provided on a standard aluminum alloy substrate, by electroless deposition, to improve adhesion of subsequent layers. A layer of nickel phosphorous and a magnetic layer of nickel cobalt are then, in turn, electroplated. The plated media disk is then oxidized below a nickel-magnetizing temperature to provide a protective outer surface.A variation of this process is also disclosed. This time a magnetically-shielding copper layer is electroplated over the first nickel layer. The nickel phosphorous and nickel cobalt layers are then electroplated on as before. The plated media can now be oxidized at a temperature higher than the nickel-magnetizing temperature to speed up the process.
摘要翻译: 公开了一种用于生产适用于高性能磁盘驱动器的磁性电镀介质的工艺。 首先通过无电沉积在标准铝合金基底上提供镍层,以改善后续层的粘附性。 然后电镀一层镍磷和一个镍钴磁性层。 然后将镀覆的介质盘氧化成低于镍磁化温度以提供保护性外表面。 还公开了该方法的变体。 这次磁屏蔽铜层电镀在第一镍层上。 镍磷和镍钴层然后如前所述电镀。 电镀介质现在可以在高于镍磁化温度的温度下被氧化,以加速工艺。
-