Preparation of iron powder
    1.
    发明授权
    Preparation of iron powder 失效
    铁粉的制备

    公开(公告)号:US4652305A

    公开(公告)日:1987-03-24

    申请号:US760043

    申请日:1985-07-29

    IPC分类号: B22F9/30 C22C1/04

    CPC分类号: B22F9/305

    摘要: Iron powder is prepared by thermal decomposition of iron pentacarbonyl in a cavity decomposer, with an average amount of from 4 to 8 kg per m.sup.2 per hour of iron carbonyl striking the heating surface, by a process in which the velocity of the inflowing stream is brought to about 0.2-4 kg per m.sup.2 per second of carbonyl vapor or vapor/inert gas mixture by changing the inlet cross-section.

    摘要翻译: 通过在空腔分解器中热分解五羰基铁制备铁粉,其平均含量为每小时4至8kg每小时的羰基羰基冲击加热表面,通过其中流入流速度的方法 通过改变入口横截面,每秒钟至约0.2-4kg / m 2的羰基蒸汽或蒸气/惰性气体混合物。

    Preparation of iron whiskers
    3.
    发明授权
    Preparation of iron whiskers 失效
    铁制品的制备

    公开(公告)号:US5085690A

    公开(公告)日:1992-02-04

    申请号:US615844

    申请日:1990-11-20

    IPC分类号: B22F1/00 B22F9/30

    CPC分类号: B22F9/305 B22F1/004

    摘要: Iron whiskers are produced by thermal decomposition of iron pentacarbonyl vapor in an indirectly heated empty-space decomposer in which the cross-sectional area for entry of the iron pentacarbonyl into the empty-space decomposer is from 10 to 40% of the cross-sectional area of the empty-space decomposer, the mass flow density of the iron pentacarbonyl vapor, based on the cross-sectional area of the decomposer, is from 0.01 to 0.07 kg per square meter per second, and the temperature in the empty-space decomposer should at no point be below 360.degree. C.

    摘要翻译: 铁晶须是通过在间接加热的空空间分解器中热分解铁五羰基蒸气来制造的,其中五羰基铁进入空间分解器的横截面面积为横截面积的10至40% 的空 - 空分解器,基于分解器的横截面面积的五羰基铁蒸汽的质量流密度为每平方米每秒0.01至0.07kg,空间分解器中的温度应为 在任何时候都不低于360℃