Angular abrasive proppant, process for the preparation thereof and process for hydraulic fracturing of oil and gas wells
    1.
    发明授权
    Angular abrasive proppant, process for the preparation thereof and process for hydraulic fracturing of oil and gas wells 有权
    角磨料支撑剂,其制备方法和油气井水力压裂工艺

    公开(公告)号:US09234127B2

    公开(公告)日:2016-01-12

    申请号:US12047019

    申请日:2008-03-12

    CPC分类号: C09K8/80

    摘要: An angular abrasive proppant comprises angular sintered particles of a material selected from bauxite, clay-minerals, and mixtures thereof, with particle sizes varying from 30 mesh to 150 mesh. A process for the production of an angular abrasive proppant comprising sintered particles of a material selected from bauxite, clay-minerals, and mixtures thereof comprises the steps of drying, grinding, pelletizing, and sintering a bauxite starting material, grinding the sintered pellets, and sizing said particles to a particle size varying from 35 to 150 mesh. A hydraulic fracturing process uses as proppant the angular abrasive proppant as the described above.

    摘要翻译: 角磨料支撑剂包括选自铝土矿,粘土矿物及其混合物的材料的角度烧结颗粒,粒度从30目到150目不等。 一种生产角磨料支撑剂的方法,其包括选自铝土矿,粘土矿物及其混合物的材料的烧结颗粒,包括以下步骤:干燥,研磨,造粒和烧结铝土矿原料,研磨烧结颗粒,以及 将所述颗粒的尺寸调整为从35至150目变化的粒度。 水力压裂方法用作支撑剂,如上所述的角磨料支撑剂。

    ANGULAR ABRASIVE PROPPANT, PROCESS FOR THE PREPARATION THEREOF AND PROCESS FOR HYDRAULIC FRACTURING OF OIL AND GAS WELLS
    3.
    发明申请
    ANGULAR ABRASIVE PROPPANT, PROCESS FOR THE PREPARATION THEREOF AND PROCESS FOR HYDRAULIC FRACTURING OF OIL AND GAS WELLS 有权
    直角磨料专利,其制备方法和油气井液压破碎方法

    公开(公告)号:US20090227480A1

    公开(公告)日:2009-09-10

    申请号:US12047019

    申请日:2008-03-12

    IPC分类号: E21B43/267

    CPC分类号: C09K8/80

    摘要: An angular abrasive proppant comprises angular sintered particles of a material selected from bauxite, clay-minerals, and mixtures thereof, with particle sizes varying from 30 mesh to 150 mesh. A process for the production of an angular abrasive proppant comprising sintered particles of a material selected from bauxite, clay-minerals, and mixtures thereof comprises the steps of drying, grinding, pelletizing, and sintering a bauxite starting material, grinding the sintered pellets, and sizing said particles to a particle size varying from 35 to 150 mesh. A hydraulic fracturing process uses as proppant the angular abrasive proppant as the described above.

    摘要翻译: 角磨料支撑剂包括选自铝土矿,粘土矿物及其混合物的材料的角度烧结颗粒,粒度从30目到150目不等。 一种生产角磨料支撑剂的方法,其包括选自铝土矿,粘土矿物及其混合物的材料的烧结颗粒,包括以下步骤:干燥,研磨,造粒和烧结铝土矿原料,研磨烧结颗粒,以及 将所述颗粒的尺寸调整为从35至150目变化的粒度。 水力压裂方法用作支撑剂,如上所述的角磨料支撑剂。