公开(公告)号:US09656867B2
公开(公告)日:2017-05-23
申请号:US14639988
申请日:2015-03-05
Applicant: Hsing-I Hsiang , Chang-Ting Yang , Jui-Huan Tu , Juu-En Chang
Inventor: Hsing-I Hsiang , Chang-Ting Yang , Jui-Huan Tu , Juu-En Chang
CPC classification number: C01B19/007 , C01P2002/72 , C01P2002/82 , C01P2002/84 , C01P2002/85 , C01P2004/03 , C01P2004/04 , H01L21/02568 , H01L21/02601
Abstract: This present invention relates to a method of synthesizing copper selenide powder by using a hot-injection method wherein a proper amount of a reducing agent is added to a mixed solution made of copper cationic solution and selenium anionic solution, and the mixed solution is maintained at a temperature of 230° C. for 40 minutes to obtain Copper Selenide powder. The Copper selenide powder, which is in the form of CuSe or Cu2-xSe, can be synthesized by adjusting the amount of the reducing agent being added to the mixed solution.
-
公开(公告)号:US20160257567A1
公开(公告)日:2016-09-08
申请号:US14639988
申请日:2015-03-05
Applicant: Hsing-I Hsiang , Chang-Ting Yang , Jui-Huan Tu , Juu-En Chang
Inventor: Hsing-I Hsiang , Chang-Ting Yang , Jui-Huan Tu , Juu-En Chang
IPC: C01B19/00
CPC classification number: C01B19/007 , C01P2002/72 , C01P2002/82 , C01P2002/84 , C01P2002/85 , C01P2004/03 , C01P2004/04 , H01L21/02568 , H01L21/02601
Abstract: This present invention relates to a method of synthesizing copper selenide powder chemical by using a hot-injection method wherein a proper amount of a. reducing agent is added to a mixed solution made of copper cationic solution and selenium anionic solution, and the mixed solution is maintained at a temperature of 230° C. for 40 minutes to obtain Copper Selenide powder. The Copper selenide powder which is in the form of CuSe or Cu2-xSe, can be synthesized by adjusting the amount of the reducing agent being added to the mixed solution.
Abstract translation: 本发明涉及一种通过使用热喷射法合成硒化硒粉末化学品的方法,其中适量的a。 将还原剂加入到由阳离子阳离子溶液和硒阴离子溶液制成的混合溶液中,并将混合溶液保持在230℃的温度下40分钟以获得硒化铜粉末。 可以通过调节添加到混合溶液中的还原剂的量来合成CuSe或Cu2-xSe形式的硒化铜粉末。
-
公开(公告)号:US20100009185A1
公开(公告)日:2010-01-14
申请号:US12218292
申请日:2008-07-14
Applicant: Tsang-Tse Fang , Steve Lien-Chung Hsu , Hsing-I Hsiang , Han-Yang Chung , Ting-I Lu , Chih-Wei Hsu , Chun-Hung Chen , Jung-Kun Chiu , Shang-Hui Shen
Inventor: Tsang-Tse Fang , Steve Lien-Chung Hsu , Hsing-I Hsiang , Han-Yang Chung , Ting-I Lu , Chih-Wei Hsu , Chun-Hung Chen , Jung-Kun Chiu , Shang-Hui Shen
CPC classification number: H01B3/308 , H01B3/10 , Y10T428/2956
Abstract: An enameled wire containing a nano-filler includes a metallic wire and at least one layer of insulating coating. At least one layer of the at least one layer of insulating coating includes a nano-filler. The nano-filler is a modified silicon dioxide slurry comprising silicon dioxide, organic solvent and organic silane coupling agent. The nano-filler comprises silicon dioxide modified with an organic silane coupling agent to improve dispersion of the nano-filler and maintain properties of the insulating coating. In addition, material and manufacturing costs of the enameled wire can be lowered.
Abstract translation: 包含纳米填料的漆包线包括金属线和至少一层绝缘涂层。 至少一层绝缘涂层的至少一层包括纳米填料。 纳米填料是包含二氧化硅,有机溶剂和有机硅烷偶联剂的改性二氧化硅浆液。 纳米填料包括用有机硅烷偶联剂改性的二氧化硅,以改善纳米填料的分散性并保持绝缘涂层的性能。 此外,可以降低漆包线的材料和制造成本。
-
公开(公告)号:US20090136441A1
公开(公告)日:2009-05-28
申请号:US11896734
申请日:2007-09-05
Applicant: Steve Lien-Chung Hsu , Tsang-Tse Fang , Hsing-I Hsiang , Ming-Chung Fang
Inventor: Steve Lien-Chung Hsu , Tsang-Tse Fang , Hsing-I Hsiang , Ming-Chung Fang
IPC: C09D5/16
CPC classification number: C09D5/1687
Abstract: A nano-scaled antifouling paint for boat is fabricated. A few hydrophobic nano-particles are added into the paint to obtain a nanostructure and a low surface energy. Thus, sea creatures are hard to adhere on the boat or are easily removed. Moreover, owing to a low wettability of the paint, a water drag is reduced when the boat sails, and so fuel is saved.
Abstract translation: 制造了纳米级的船用防污漆。 将几种疏水性纳米颗粒加入到涂料中以获得纳米结构和低表面能。 因此,海洋生物难以粘附在船上或容易被移除。 此外,由于油漆的低润湿性,当船帆行驶时,阻水减少,因此节省燃料。
-
-
-