Process for controlling deposit of sticky material
    1.
    发明授权
    Process for controlling deposit of sticky material 有权
    控制粘性材料沉积的工艺

    公开(公告)号:US06171445B2

    公开(公告)日:2001-01-09

    申请号:US09363225

    申请日:1999-07-30

    IPC分类号: D21F132

    CPC分类号: D21H21/02 Y10S162/04

    摘要: Method of inhibiting the deposit of sticky material on a papermill felt used in processing pulp slurry into sheets, comprising applying to the papermill felt at least one cationic polymer and at least one nonionic surfactant having an HLB of about 11 to 14.

    摘要翻译: 用于抑制在用于将纸浆浆料加工成片材的用于造纸毛毡上的粘性材料的沉积的方法,其包括将至少一种阳离子聚合物和至少一种HLB为约11至14的非离子表面活性剂施用到所述造纸机上。

    Process for controlling deposit of sticky material
    2.
    发明授权
    Process for controlling deposit of sticky material 失效
    控制粘性材料沉积的工艺

    公开(公告)号:US06517682B2

    公开(公告)日:2003-02-11

    申请号:US09727011

    申请日:2000-11-30

    IPC分类号: D21F132

    CPC分类号: D21H21/02 Y10S162/04

    摘要: Method of inhibiting the deposit of sticky material on a papermill felt used in processing pulp slurry into sheets, comprising applying to the papermill felt at least one cationic polymer and at least one nonionic surfactant having an HLB of about 11 to 14.

    摘要翻译: 用于抑制在用于将纸浆浆料加工成片材的用于造纸毛毡上的粘性材料的沉积的方法,其包括将至少一种阳离子聚合物和至少一种HLB为约11至14的非离子表面活性剂施加到所述造纸机上。

    Felt conditioner for deinked recycled newsprint papermaking system
    3.
    发明授权
    Felt conditioner for deinked recycled newsprint papermaking system 失效
    脱墨再生新闻纸造纸系统的毡制调理剂

    公开(公告)号:US5575893A

    公开(公告)日:1996-11-19

    申请号:US404771

    申请日:1995-03-15

    摘要: A method for conditioning the felts in a papermaking process utilizing deinked secondary fiber in the furnish by adding a felt conditioner consisting of from 5-33% of a nonionic surfactant, from 5-33% of a dispersant, or blends thereof, with the remainder water; wherein the nonionic surfactant is selected from the group consisting of ethoxylated nonylphenols having moles of ethoxylation of from 7.5 to 30 and an HLB of about 12 to 17.2 and di-alkyl phenol ethoxylates having moles of ethoxylation of from 15 to 24 and an HLB of about 13 to 15.1; and wherein the dispersant is selected from the group consisting of the sodium salt of naphthalene sulfonate formaldehyde-condensate having an average molecular weight of from about 700 to 3500, the potassium salt of polymerized alkyl naphthalene sulfonic acid having an average molecular weight of approximately 1000, or the sodium or ammonium salt of lignosulfonate. Additionally, from 1 to 5% of an alkylether hydroxypropyl sultaine enhances performance.

    摘要翻译: 通过添加由5-33%的非离子表面活性剂组成的毛发调理剂,5-33%的分散剂或其混合物与其余部分组合,在造纸方法中利用脱墨的次级纤维调理造纸方法中的毛毡的方法, 水; 其中所述非离子表面活性剂选自乙氧基化度为7.5-30,乙氧基化度为约12至17.2的乙氧基化壬基酚,乙氧基化度为15-24,摩尔数为15-24的二烷基酚乙氧基化物, 13至15.1; 并且其中所述分散剂选自平均分子量为约700至3500的萘磺酸盐甲醛缩合物的钠盐,聚合烷基萘磺酸的钾盐,其平均分子量为约1000, 或木质素磺酸钠或铵盐。 另外,1至5%的烷基醚羟丙基磺基甜菜碱可提高性能。