Method of producing ceramic matrix composite, and ceramic matrix composite produced by the method for production
    1.
    发明授权
    Method of producing ceramic matrix composite, and ceramic matrix composite produced by the method for production 失效
    生产陶瓷基复合材料的方法,以及生产方法生产的陶瓷基复合材料

    公开(公告)号:US06830724B2

    公开(公告)日:2004-12-14

    申请号:US10219505

    申请日:2002-08-15

    IPC分类号: B22F700

    摘要: A method of producing a ceramic matrix composite is provided, which production method reduces metal residual percentage within matrix with little energy consumption, without requiring special external heating means and special equipment while it is industrially simple and at a low price. It is a method of producing a ceramic matrix composite having the steps of filling mixed powder obtained by mixing metal powder and boron nitride powder into a predetermined container to form a green compact having a porous structure, and infiltrating the above described green compact with molten Al to form a composite material containing metal boride and having aluminum nitride as a matrix. The green compact is formed by compressing the mixed powder whose mixing ratio of metal powder to boron nitride powder is 1:1.8 to 1:2.2 (molar ratio) so that porosity of the green compact is 34 to 42%.

    摘要翻译: 提供了一种陶瓷基复合材料的制造方法,该制造方法在能量消耗少的基质内减少金属残留量,而无需特殊的外部加热装置和专用设备,而且在工业上简单且价格低廉。 一种陶瓷基复合材料的制造方法,其特征在于,具有将金属粉末和氮化硼粉末混合而得到的混合粉末填充到规定的容器中,形成具有多孔结构的生坯的步骤,将熔融的Al 以形成含有金属硼化物并具有氮化铝作为基质的复合材料。 通过压缩金属粉末与氮化硼粉末的混合比为1:1.8〜1:2.2(摩尔比)的混合粉末,使压坯的孔隙率为34〜42%,形成生坯。