公开(公告)号:US4026877A
公开(公告)日:1977-05-31
申请号:US625568
申请日:1975-10-24
Applicant: Kunio Kageyama , Hiroshi Hirakawa , Masatake Ozaki , Iwao Sugiyama , Mitsuharu Iwakura , Yoshiaki Someya
Inventor: Kunio Kageyama , Hiroshi Hirakawa , Masatake Ozaki , Iwao Sugiyama , Mitsuharu Iwakura , Yoshiaki Someya
IPC: C08L23/00 , C08K5/20 , C08K5/21 , C08K5/36 , C08K5/38 , C08K5/45 , C08K5/46 , C08L7/00 , C08L21/00 , C08L33/00 , C08L33/02 , C08L101/00 , C08L9/00 , C09K3/00
CPC classification number: C08K5/21
Abstract: Rubber compositions containing therein as a source of carbon disulfide at least one compound selected from the group consisting of cyclic bis (thiocarbamoyl) mono- or di-sulfides, cyclic bis (thioxanthogenyl) mono- or di-sulfides, and cyclic (thiocarbamoyl-thioxanthogenyl) mono- or di-sulfides and an amine-isocyanate addition compound as a vulcanization accelerator system having excellent scorching stability with rapid vulcanization at usual vulcanization temperatures.
Abstract translation: 其中含有二硫化碳源的至少一种化合物的橡胶组合物选自环状双(硫代氨基甲酰基)单 - 或二 - 硫化物,环状双(硫代异戊烯基)单 - 或二 - 硫化物和环状(硫代氨基甲酰基 - 噻吨基 )单 - 或二 - 硫化物和胺 - 异氰酸酯加成化合物作为硫化促进剂体系,在通常的硫化温度下快速硫化具有优异的烧焦稳定性。
-
公开(公告)号:US4026878A
公开(公告)日:1977-05-31
申请号:US625569
申请日:1975-10-24
Applicant: Kunio Kageyama , Hiroshi Hirakawa , Masatake Ozaki , Iwao Sugiyama , Mitsuharu Iwakura , Yoshiaki Someya
Inventor: Kunio Kageyama , Hiroshi Hirakawa , Masatake Ozaki , Iwao Sugiyama , Mitsuharu Iwakura , Yoshiaki Someya
IPC: C08L23/00 , C08K5/20 , C08K5/21 , C08K5/36 , C08K5/38 , C08K5/45 , C08L7/00 , C08L21/00 , C08L33/00 , C08L33/02 , C08L101/00 , C08L9/00 , C09K3/00
CPC classification number: C08K5/21
Abstract: Rubber compositions containing therein as a source of carbon disulfide a compound selected from the group consisting of cyclic bis (dithiocarbamic acid) metal salts and cyclic or non-cyclic dithiocarbamic-xanthogenic acid metal salts and an amine-isocyanate addition compound as a vulcanization accelerator system having excellent scorching stability with rapid vulcanization at usual vulcanization temperatures.
Abstract translation: 其中含有二硫化碳源的橡胶组合物选自环状双(二硫代氨基甲酸)金属盐和环状或非环状二硫代氨基甲酸 - 黄原酸金属盐和胺 - 异氰酸酯加成化合物作为硫化促进剂体系 具有优异的烧焦稳定性,在通常的硫化温度下快速硫化。
-