Method and apparatus for producing a quartz glass cylinder
    1.
    发明授权
    Method and apparatus for producing a quartz glass cylinder 有权
    用于生产石英玻璃圆筒的方法和设备

    公开(公告)号:US08613207B2

    公开(公告)日:2013-12-24

    申请号:US12737302

    申请日:2009-06-25

    IPC分类号: C03B15/14

    摘要: In a known method for drawing a tubular quartz glass strand, SiO2-containing starting material is fed to a melting crucible, softened therein into a viscous quartz glass mass (27), and said mass is pulled vertically downward as a cylindrical quartz glass strand (5; 33) through a die (4; 34) provided in the bottom region of the melting crucible (1), said die having a gap-shaped outlet (25; 36), which is defined by a bottom opening and a die inside part, and thereafter the quartz glass cylinder is cut to length. In order to provide a method starting from this which facilitates the production of homogeneous quartz glass cylinders, even if the lateral dimensions thereof are in the range of the inside diameters of conventional melting crucibles (1), according to the invention the viscous quartz glass mass is drawn over a flow constriction (12; 32) provided in an upper region of the die (4; 34) and leading downward into the outlet (25; 36) via a flow channel, said region facing the crucible interior, wherein the outlet has an opening width that is larger than the width of the flow constriction (12; 32), and wherein a first minimum circumscribed circle around the flow constriction (12; 32) has a diameter that is a maximum of 30% of the diameter of a second minimum circumscribed circle around the quartz glass strand (5; 33) to be drawn. The invention further relates to a corresponding apparatus.

    摘要翻译: 在已知的用于拉制管状石英玻璃线的方法中,将含SiO 2的起始材料供给到熔化的坩埚中,在其中软化成粘性石英玻璃块(27),并将所述物质作为圆柱形石英玻璃绞线垂直向下拉( 5; 33)通过设置在熔化坩埚(1)的底部区域中的模具(4; 34),所述模具具有间隙形出口(25; 36),其由底部开口和模具内部限定 然后将石英玻璃圆筒切割成长度。 为了提供一种便于生产均质石英玻璃圆筒的方法,即使其横向尺寸在常规熔化坩埚(1)的内径范围内,根据本发明,粘性石英玻璃质量 被设置在模具(4; 34)的上部区域中的流动收缩部(12; 32)上,并经由流动通道向下流入出口(25; 36),所述区域面向坩埚内部,其中出口 具有大于所述流动收缩部(12; 32)的宽度的开口宽度,并且其中所述流动收缩部(12; 32)周围的第一最小限定圆的直径为所述流动收缩部(12; 32)的直径的最大值的30% 围绕要被拉伸的石英玻璃绞线(5; 33)的第二最小外接圆。 本发明还涉及相应的装置。

    Method for coating a component for use in a crucible drawing method for quartz glass, and coated component obtained according to the method
    2.
    发明授权
    Method for coating a component for use in a crucible drawing method for quartz glass, and coated component obtained according to the method 有权
    用于石英玻璃的坩埚拉拔方法中使用的成分的涂布方法以及根据该方法得到的涂布成分

    公开(公告)号:US07955715B2

    公开(公告)日:2011-06-07

    申请号:US11642349

    申请日:2006-12-20

    IPC分类号: B32B15/04 C03B37/00

    摘要: In a known method for coating a crucible for use at a high working temperature in a crucible drawing method for quartz glass, a base body wall of tungsten has applied thereto a protective layer containing a coating metal consisting of the group selected from iridium, rhenium, osmium and ruthenium. Starting therefrom, to provide a method for producing such a component exhibiting high corrosion resistance to the quartz glass melt at low material costs, it is suggested according to the invention that the protective layer should be produced from a layer material which contains tungsten and the coating metal, and in which the amount of the coating metal should be dimensioned such that it exceeds the limit amount of a coating metal-rich phase boundary of a solid mixture phase of tungsten and the coating metal, with the solid mixture phase being thermodynamically stable at the working temperature, by not more than 25 at. % (based on the total amount of tungsten and the coating metal in the layer material).

    摘要翻译: 在用于石英玻璃的坩埚拉拔方法中用于涂覆在高工作温度下使用的坩埚的已知方法中,钨基体壁向其施加保护层,该保护层含有由选自铱,铼, 锇和钌。 从其开始,为了提供一种以低材料成本制造对石英玻璃熔体具有高耐腐蚀性的组分的方法,根据本发明,建议保护层应由含钨的层材料和涂层 金属,并且其中涂层金属的量的尺寸应使其超过钨和涂覆金属的固体混合物相的涂覆金属富集相边界的极限量,其中固体混合物相在热力学上稳定在 工作温度不超过25℃。 %(基于钨层和层材料中涂层金属的总量)。

    METHOD AND APPARATUS FOR PRODUCING A QUARTZ GLASS CYLINDER
    3.
    发明申请
    METHOD AND APPARATUS FOR PRODUCING A QUARTZ GLASS CYLINDER 有权
    用于制造石墨玻璃圆筒的方法和装置

    公开(公告)号:US20110113829A1

    公开(公告)日:2011-05-19

    申请号:US12737302

    申请日:2009-06-25

    IPC分类号: C03B17/04 C03B5/16

    摘要: In a known method for drawing a tubular quartz glass strand, SiO2-containing starting material is fed to a melting crucible, softened therein into a viscous quartz glass mass (27), and said mass is pulled vertically downward as a cylindrical quartz glass strand (5; 33) through a die (4; 34) provided in the bottom region of the melting crucible (1), said die having a gap-shaped outlet (25; 36), which is defined by a bottom opening and a die inside part, and thereafter the quartz glass cylinder is cut to length. In order to provide a method starting from this which facilitates the production of homogeneous quartz glass cylinders, even if the lateral dimensions thereof are in the range of the inside diameters of conventional melting crucibles (1), according to the invention the viscous quartz glass mass is drawn over a flow constriction (12; 32) provided in an upper region of the die (4; 34) and leading downward into the outlet (25; 36) via a flow channel, said region facing the crucible interior, wherein the outlet has an opening width that is larger than the width of the flow constriction (12; 32), and wherein a first minimum circumscribed circle around the flow constriction (12; 32) has a diameter that is a maximum of 30% of the diameter of a second minimum circumscribed circle around the quartz glass strand (5; 33) to be drawn. The invention further relates to a corresponding apparatus.

    摘要翻译: 在已知的用于拉制管状石英玻璃线的方法中,将含SiO 2的起始材料供给到熔化的坩埚中,在其中软化成粘性石英玻璃块(27),并将所述物质作为圆柱形石英玻璃绞线垂直向下拉( 5; 33)通过设置在熔化坩埚(1)的底部区域中的模具(4; 34),所述模具具有间隙形出口(25; 36),其由底部开口和模具内部限定 然后将石英玻璃圆筒切割成长度。 为了提供一种便于生产均质石英玻璃圆筒的方法,即使其横向尺寸在常规熔化坩埚(1)的内径范围内,根据本发明,粘性石英玻璃质量 被设置在模具(4; 34)的上部区域中的流动收缩部(12; 32)上,并经由流动通道向下流入出口(25; 36),所述区域面向坩埚内部,其中出口 具有大于所述流动收缩部(12; 32)的宽度的开口宽度,并且其中所述流动收缩部(12; 32)周围的第一最小限定圆的直径为所述流动收缩部(12; 32)的直径的最大值的30% 围绕要被拉伸的石英玻璃绞线(5; 33)的第二最小外接圆。 本发明还涉及相应的装置。

    Method for coating a component for use in a crucible drawing method for quartz glass, and coated component obtained according to the method
    4.
    发明申请
    Method for coating a component for use in a crucible drawing method for quartz glass, and coated component obtained according to the method 有权
    用于石英玻璃的坩埚拉拔方法中使用的成分的涂布方法以及根据该方法得到的涂布成分

    公开(公告)号:US20070178329A1

    公开(公告)日:2007-08-02

    申请号:US11642349

    申请日:2006-12-20

    IPC分类号: B05D1/36 C23C4/08 F01D5/18

    摘要: In a known method for coating a crucible for use at a high working temperature in a crucible drawing method for quartz glass, a base body wall of tungsten has applied thereto a protective layer containing a coating metal consisting of the group selected from iridium, rhenium, osmium and ruthenium. Starting therefrom, to provide a method for producing such a component exhibiting high corrosion resistance to the quartz glass melt at low material costs, it is suggested according to the invention that the protective layer should be produced from a layer material which contains tungsten and the coating metal, and in which the amount of the coating metal should be dimensioned such that it exceeds the limit amount of a coating metal-rich phase boundary of a solid mixture phase of tungsten and the coating metal, with the solid mixture phase being thermodynamically stable at the working temperature, by not more than 25 at. % (based on the total amount of tungsten and the coating metal in the layer material).

    摘要翻译: 在用于石英玻璃的坩埚拉拔方法中用于涂覆在高工作温度下使用的坩埚的已知方法中,钨基体壁向其施加保护层,该保护层含有由选自铱,铼, 锇和钌。 从其开始,为了提供一种以低材料成本制造对石英玻璃熔体具有高耐腐蚀性的组分的方法,根据本发明,建议保护层应由含钨的层材料和涂层 金属,并且其中涂层金属的量的尺寸应使其超过钨和涂覆金属的固体混合物相的涂覆金属富集相边界的极限量,其中固体混合物相在热力学上稳定在 工作温度不超过25℃。 %(基于钨层和层材料中涂层金属的总量)。

    METHOD AND DEVICE FOR DRAWING A QUARTZ GLASS CYLINDER FROM A MELT CRUCIBLE
    5.
    发明申请
    METHOD AND DEVICE FOR DRAWING A QUARTZ GLASS CYLINDER FROM A MELT CRUCIBLE 审中-公开
    用于从熔体坩埚绘制石英玻璃圆筒的方法和装置

    公开(公告)号:US20120174629A1

    公开(公告)日:2012-07-12

    申请号:US13381050

    申请日:2010-06-15

    IPC分类号: C03B17/04

    CPC分类号: C03B17/04 Y02P40/57

    摘要: The invention relates to a known method for drawing a quartz glass cylinder from a melt crucible comprising an inner crucible chamber extending in the direction of a center crucible axis and bounded by a side wall and a floor, wherein SiO2 granulate is fed into the melt crucible and therein softened into a quartz glass mass, and said mass is drawn vertically downward as a cylindrical quartz glass strand by means of a first draw-off device through a first draw nozzle provided in the floor of the melt crucible, and the quartz glass cylinder is cut off therefrom. In order to disclose a method starting herefrom and allowing the production of homogenous quartz glass cylinder at simultaneously high levels of productivity, the invention proposes that at least one second quartz glass strand is drawn off through at least one further second draw nozzle provided in the floor of the melt crucible, wherein the first draw nozzle and the second draw nozzle are disposed eccentrically to the center crucible axis and at a distance from each other.

    摘要翻译: 本发明涉及一种用于从熔融坩埚中抽取石英玻璃圆筒的公知方法,所述熔融坩埚包括沿中心坩埚轴线方向延伸并由侧壁和底板限定的内坩埚室,其中SiO 2颗粒被送入熔融坩埚 并且在其中软化成石英玻璃物质,并且所述物质通过设置在熔融坩埚的地板中的第一牵引喷嘴借助于第一牵引装置作为圆柱形石英玻璃绳垂直向下拉动,并且石英玻璃圆筒 被切断。 为了公开一种从此开始的方法,并允许以同时高的生产率生产均匀的石英玻璃圆筒,本发明提出,至少一个第二石英玻璃丝线通过设置在地板中的至少一个另外的第二个拉伸喷嘴被抽出 所述第一拉丝喷嘴和所述第二拉伸喷嘴相对于所述中心坩埚轴偏心设置并且彼此间隔一定距离。

    Method and device for drawing a tubular strand of quartz glass
    6.
    发明申请
    Method and device for drawing a tubular strand of quartz glass 审中-公开
    用于绘制石英玻璃管状管的方法和装置

    公开(公告)号:US20090064715A1

    公开(公告)日:2009-03-12

    申请号:US11920370

    申请日:2007-03-07

    IPC分类号: C03B23/047

    CPC分类号: C03B17/04 C03B5/0336

    摘要: In a known method for drawing a tubular quartz glass strand, a crucible is fed with SiO2-containing start material, the start material is softened in the crucible and, as a softened quartz glass mass, is drawn vertically downwards as a tubular quartz glass strand along a drawing axis through an annular gap between an outer member and an inner member, which is arranged in a through hole of the outer member, of a drawing nozzle provided in the bottom area of the crucible. To improve the known method with respect to less inhomogeneity in the drawn-off tubular strand and thereby to permit the manufacture of homogeneous, defect-free hollow cylinders of quartz glass by drawing from the melt, it is suggested according to the invention that the inner member of the drawing nozzle, viewed in the direction of the drawing axis, is held suspended and radially movable inside the through hole of the outer member, and that the annular gap of the drawing nozzle has a longitudinal section “L” in which its cross-sectional nozzle area is reduced in size from the top to the bottom.