Method and installation for the production of steel products having an optimum surface quality
    1.
    发明授权
    Method and installation for the production of steel products having an optimum surface quality 有权
    生产具有最佳表面质量的钢制品的方法和安装

    公开(公告)号:US07998237B2

    公开(公告)日:2011-08-16

    申请号:US10559802

    申请日:2004-05-25

    Abstract: Disclosed are a method and an installation for producing steel products (1) having an optimum surface quality, especially extremely low carbon contents (UCL steel or IF steel), nitrogen contents, total oxygen contents, high-strength or stainless steel qualities. According to the invention, the liquid steel is cast into a thin slab (5a) from a process route (10, 11, 12, or 13) that is selected according to the desired final structure (9) based on an electric-arc furnace (2b), is descaled, cut into billets (15) having a partial length, optionally descaled once again, subjected to final descaling downstream from a holding furnace (16), milled in a finishing mill train (6a), rolled up in a rolling station (20) located downstream from the last finishing mill stand (19) or downstream from a cooling section (21), and the final structure (9) is adjusted in the cooling section (21) according to the desired steel quality by cooling on a run-out roller table (22), whereupon the rolling stock (1a) is completely rolled up in a second rolling station (23).

    Abstract translation: 公开了一种具有最佳表面质量,特别是极低碳含量(UCL钢或IF钢),氮含量,总氧含量,高强度或不锈钢质量的钢产品(1)的制造方法和装置。 根据本发明,液态钢从根据期望的最终结构(9)选择的工艺路线(10,11,12或13)基于电弧炉浇铸成薄板坯(5a) (2b)切割成具有局部长度的坯料(15),再次可选地除锈,在从精轧机(6a)中研磨的保持炉(16)的下游进行最终除垢,在轧制机 位于上一个精轧机架(19)的下游或冷却部分(21)的下游的轧制站(20),并且通过冷却来根据期望的钢质量在冷却部分(21)中调节最终结构(9) 在排出辊台(22)上,在第二轧制站(23)中车辆(1a)完全卷起。

    Method and Installation for the Production of Steel Products Having an Optimum Surface Quality
    4.
    发明申请
    Method and Installation for the Production of Steel Products Having an Optimum Surface Quality 有权
    具有最佳表面质量的钢材生产方法和安装

    公开(公告)号:US20070272054A1

    公开(公告)日:2007-11-29

    申请号:US10559802

    申请日:2004-05-25

    Abstract: Disclosed are a method and an installation for producing steel products (1) having an optimum surface quality, especially extremely low carbon contents (UCL steel or IF steel), nitrogen contents, total oxygen contents, high-strength or stainless steel qualities. According to the invention, the liquid steel is cast into a thin slab (5a) from a process route (10, 11, 12, or 13) that is selected according to the desired final structure (9) based on an electric-arc furnace (2b), is descaled, cut into billets (15) having a partial length, optionally descaled once again, subjected to final descaling downstream from a holding furnace (16), milled in a finishing mill train (6a), rolled up in a rolling station (20) located downstream from the last finishing mill stand (19) or downstream from a cooling section (21), and the final structure (9) is adjusted in the cooling section (21) according to the desired steel quality by cooling on a run-out roller table (22), whereupon the rolling stock (1a) is completely rolled up in a second rolling station (23).

    Abstract translation: 公开了一种具有最佳表面质量,特别是极低碳含量(UCL钢或IF钢),氮含量,总氧含量,高强度或不锈钢质量的钢产品(1)的制造方法和装置。 根据本发明,液态钢从根据期望的最终结构(9)选择的工艺路线(10,11,12或13)铸造成薄板坯(5a),基于电弧 炉(2b)被除鳞,切成具有部分长度的坯料(15),再次可选地除去,在保持炉(16)的下游进行最终除垢,在精轧机(6a)中研磨,轧制 在位于上一个精轧机架(19)下游的轧制工位(20)中或冷却部分(21)的下游,并且根据期望的钢在冷却部分(21)中调节最终结构(9) 在排出辊台(22)上进行冷却的质量,于是在第二轧制站(23)中车辆(1a)被完全卷起。

Patent Agency Ranking